journal article·2025-08Open access

Healable nanoscale deterioration of gold nanothin film

Parivat Phiphatbunyabhorn, Komsun Lapawae, Witchukorn Phuthong, Anusit Kaewprajak, Tanyakorn Muangnapoh, Pisist Kumnorkaew, Kitiphat Sinthiptharakoon, Varong Pavarajarn

Abstract

Metal deterioration in semiconductor devices increases the risk of equipment failures leading to higher operating costs, waste generation, and poor resource utilization. Although the understanding of degradation dynamics and the corresponding molecular products especially at the early stages can improve degradation prevention, the acquisition of such information from real samples is challenging. This is not only because of the ultra-small size of degradation features but also the correlation of measurable data. Herein, nanoscale electrochemical deterioration and healability of ultrathin Au films on an n -type Si substrate are investigated. Considering the possible effect of internal band bending on surface electron mobility and surface reaction, the investigation is performed with different Au thicknesses on n -type and undoped Si substrates with sample storage time varying from 24 h up to 300 h. In conjunction with the structural insight obtained from 4-point probing (4PP) data and X-ray diffraction (XRD) data, the electrochemical dynamics of surface degradation and healing induced by highly localized contact electrification (CE) are described through anionic clusters denoted by atomic force microscope (AFM) force curve mapping data. The finding can contribute to the improvement of surface protection for functional metal films in semiconductor devices and highlights the importance of nanothickness selection.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: ZnO doping and properties · Copper-based nanomaterials and applications · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. High quantum efficiency hot electron electrochemistry10.1021/acs.nanolett.9b02289 ↗
2. Feasible antibacterial nanomaterials: copper oxide nanoparticles synthesized using dandelion leaf extract10.1016/j.inoche.2024.112804 ↗
3. Chemical design of high performance SPR biosensor based on a dielectric nanoparticle assembly supported onto a gold thin film10.1039/D2SD00069E ↗
4. Substrate heat-assisted spray pyrolysis of crack-free ytterbium sesquioxide-Si heterojunction diodes for photo-sensing applications
5. Ultra-fast switching memristors based on two-dimensional materials10.1038/s41467-024-46372-y ↗
6. Augmented photovoltaic performance of Cu/Ce-(Sn:Cd)/n-Si Schottky barrier diode utilizing dual-doped Ce-(Sn:Cd) thin films10.1016/j.optmat.2024.115133 ↗
7. Bifacial perovskite solar cells with gold transparent electrodes grown on molybdenum disulfide surfaces10.1021/acsaem.4c00665 ↗
8. Atmospheric corrosion of materials and their effects on mechanical properties: a brief review10.1016/j.matpr.2020.10.939 ↗
9. Disentangling the role of surface chemical interactions on interfacial charge transport at BiVO4 photoanodes10.1021/acsami.8b11366 ↗
10. A shape-recovery polymer coating for the corrosion protection of metallic surfaces10.1021/am505621x ↗
11. Dissolution engineering of platinum alloy counter electrodes in dye-sensitized solar cells10.1002/anie.201505339 ↗
12. Effect of alternating current on cathodic protection on pipelines10.1016/j.corsci.2012.09.028 ↗
13. In situ electrochemical regeneration of nanogap hotspots for continuously reusable ultrathin SERS sensors10.1038/s41467-024-46097-y ↗
14. V. Cicek, Cathodic Protection, in: Cathodic Protection: Industrial Solutions for Protecting Against Corrosion, Scrivener Publishing, 2013, pp. 131–156.10.1002/9781118737880.ch8 ↗
15. Anisotropic etching of platinum electrodes at the onset of cathodic corrosion10.1038/ncomms12653 ↗
16. Electrochemical deterioration of a gold thin film in bicarbonate solution: correlative optical, nano-mechanical, and chemical considerations10.1021/acs.langmuir.4c01527 ↗
17. Anisotropic cathodic corrosion of gold electrodes in the absence and presence of carbon monoxide10.1021/acs.jpcc.0c08574 ↗
18. The Butler-Volmer equation in electrochemical theory: Origins, value, and practical application10.1016/j.jelechem.2020.114145 ↗
19. E.E. Stansbury, R.A. Buchanan, Introduction and Overview of Electrochemical Corrosion, in: Fundamentals of Electrochemical Corrosion, ASM International, 2000, pp. 1-21.10.31399/asm.tb.fec.t65940001 ↗
20. Electron transfer in nano-scale contact electrification: Atmosphere effect on the surface states of dielectrics10.1016/j.nanoen.2019.103956 ↗
21. The relationship between the adsorption configuration and fermi energy levels in the conversion process of Li2S6/Li2S8 on the ZrO2 surface
22. Fermi level influence on the adsorption at semiconductor surfaces—ab initio simulations10.1063/1.4817903 ↗
23. Influence of the alloy element on corrosion morphology of the low alloy steels exposed to the atmospheric environments10.1016/j.corsci.2004.10.019 ↗
24. Monitoring uniform and localised corrosion by a radiofrequency sensing method10.1016/j.snb.2017.11.028 ↗
25. Corrosion of amorphous alumina in deionized water under mild condition10.1016/j.apsusc.2019.143906 ↗
26. Chain length dependence of ZnO nanofiller–polystyrene blend coating nanofilm: Morphology, surface mechanics, photochemistry, and chain packing
27. Electronic contribution to friction on GaAs: An atomic force microscope study10.1103/PhysRevB.77.184105 ↗
28. Interfacial forces at layered surfaces: substrate electrical double-layer forces acting through ultrathin polymer coatings10.1021/acs.langmuir.9b02176 ↗
29. Enhanced efficiency of dye-sensitized solar cells via controlled thickness of the WO3 Langmuir–Blodgett blocking layer in the Debye length regime10.1039/D4MA00063C ↗
30. Catalytic Hot-Electron SERS analytical substrates and a case study on graphene nanocomposite inspection10.1021/acs.jpcc.2c05432 ↗
31. Reusability, long-life storage and highly sensitive zirconium nitride (ZrN) Surface-enhanced raman spectroscopy (SERS) substrate fabricated by reactive gas-timing Rf magnetron sputtering10.1002/admi.202300472 ↗
32. Time-Dependence of Materials and Device Degradation
33. Degradation of encapsulated perovskite solar cells driven by deep trap states and interfacial deterioration10.1039/C7TC03733C ↗
34. Degradation of gold-aluminium ball bonds by aging and contamination10.1109/95.477471 ↗
35. Corrosion and corrosion products of hot dipped galvanized steel during long term atmospheric exposure at different sites world-wide10.1016/j.corsci.2017.06.025 ↗
36. Self-Limitation of Native Oxides Explained10.1007/s12633-015-9366-8 ↗
37. The 100th anniversary of the four-point probe technique: the role of probe geometries in isotropic and anisotropic systems10.1088/0953-8984/27/22/223201 ↗
38. Effect of the crystallinity of indium tin oxide on the charge transfer at the interfaces and the performances of flexible organic light emitting diodes10.1002/pssa.201431550 ↗
39. Influence of crystallinity and energetics on charge separation in polymer–inorganic nanocomposite films for solar cells10.1038/srep01531 ↗
40. Surface energy and work function of fcc and bcc crystals: density functional study10.1016/j.susc.2014.08.017 ↗
41. Surface energies of elemental crystals10.1038/sdata.2016.80 ↗
42. Size-dependent strain and surface energies of gold nanoclusters10.1039/C5CP06153A ↗
43. Experimental observation of size-dependent behavior in surface energy of gold nanoparticles through atomic force microscope
44. J. Říha, P. Šutta, J. Siegel, Z. Kolská, V. Švorčík, XRD real structure characterization of sputtered Au films different in thickness, in: European Powder Diffraction Conference; August 2010, Darmstadt, Germany, Oldenbourg Wissenschaftsverlag, 2011, pp. 215–220.10.1524/9783486991321-037 ↗
45. Thickness dependence of grain size and surface roughness for dc magnetron sputtered Au films
46. Microstructural evolution in nanostructured gold films10.1016/j.tsf.2012.01.010 ↗
47. Conductive scanning probe microscopy of the semicontinuous gold film and its SERS enhancement toward two-step photo-induced charge transfer and effect of the supportive layer10.1016/j.apsusc.2018.01.269 ↗
48. Characterization of Ba–Sr thin films deposited by spray pyrolysis and fabrication of Ag/Ba–Sr/n-Si/Ag diodes10.1016/j.optmat.2024.116176 ↗
49. Flexoelectronics of centrosymmetric semiconductors10.1038/s41565-020-0700-y ↗
50. Energetics at the Surface of Photoelectrodes and Its Influence on the Photoelectrochemical Properties10.1021/acs.jpclett.5b01372 ↗
51. Nonequilibrium Bond Forces in Single-Molecule Junctions10.1021/acs.nanolett.9b02845 ↗
52. Manifestation on the choice of a suitable combination of MIS for proficient Schottky diodes for optoelectronic applications: A comprehensive review10.1016/j.nanoen.2024.109534 ↗
53. G. Haugstad, Distance-Dependent Interactions, in: Atomic Force Microscopy: Understanding Basic Modes and Advanced Applications, John Wiley & Sons, 2012, pp. 33-90.10.1002/9781118360668.ch2 ↗
54. Electrical and microstructural properties of thermally annealed Ni/Au and Ni/Pt/Au Schottky contacts on AlGaN/GaN heterostructures10.1088/0268-1242/29/9/095005 ↗
55. Electrochemical water splitting by gold: evidence for an oxide decomposition mechanism10.1039/c3sc50301a ↗
56. Plasmon-induced hot electrons in nanostructured materials: generation, collection, and application to photochemistry10.1021/acs.chemrev.4c00165 ↗
57. Gold is noble but gold hydride anions are stable10.1002/anie.200351780 ↗
58. Identification of novel Cu, Ag, and Au ternary oxides from global structural prediction10.1021/acs.chemmater.5b00716 ↗
59. Structure and electron counting in ternary transition metal hydrides10.1021/ja982746r ↗