Abstract

A measurement technique, i.e. reflectance anisotropy/difference spectroscopy (RAS/RDS), which had originally been developed for in-situ epitaxial growth control, is employed here for in-situ real-time etch-depth control during reactive ion etching (RIE) of cubic crystalline III/V semiconductor samples. Temporal optical Fabry-Perot oscillations of the genuine RAS signal (or of the average reflectivity) during etching due to the ever shrinking layer thicknesses are used to monitor the current etch depth. This way the achievable in-situ etch-depth resolution has been around 15 nm. To improve etch-depth control even further, i.e. down to below 5 nm, we now use the optical equivalent of a mechanical vernier scale– by employing Fabry-Perot oscillations at two different wavelengths or photon energies of the RAS measurement light – 5% apart, which gives a vernier scale resolution of 5%. For the AlGaAs(Sb) material system a 5 nm resolution is an improvement by a factor of 3 and amounts to a precision in in-situ etch-depth control of around 8 lattice constants.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Analytical Chemistry and Sensors · Semiconductor materials and devices · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Integrated Optoelectronics and Microoptics Research Group, Physics Department, Technische Universitaet Kaiserslautern (TUK) , PO Box 3049, D-67653 Kaiserslautern, Germany

Funding

Deutsche Forschungsgemeinschaft · Stiftung Rheinland-Pfalz für Innovation

References (21)

Show source-provided references
1. Above-bandgap optical anisotropies in cubic semi-conductors—A visible near ultraviolet probe of surfaces10.1116/1.582974 ↗
2. Application of reflectance difference spectroscopy to molecular-beam epitaxy growth of GaAs and AlAs10.1116/1.575694 ↗
3. Optical reflectance measurements of transients during molecular-beam epitaxial growth on (001) GaAs10.1116/1.584362 ↗
4. Kinetic limits of monolayer growth on (001) GaAs by organometallic chemical-vapor deposition10.1103/PhysRevLett.61.2782 ↗
5. Optical characterization of surface electronic and vibrational properties of epitaxial antimony monolayers on III–V (110) surfaces10.1002/pssa.2211520119 ↗
6. Reflection anisotropy spectroscopy10.1088/0034-4885/68/6/R01 ↗
7. Exciton-dominated optical response of ultra-narrow graphene nanoribbons10.1038/ncomms5253 ↗
8. Site-sensitive gas sensing and analyte discrimination in Langmuir-Blodgett porphyrin films10.1021/jp200303t ↗
9. Monitoring of (reactive) ion etching (RIE) with reflectance anisotropy spectroscopy (RAS) equipment10.1016/j.apsusc.2014.12.038 ↗
10. Influence of plasma composition on reflectance anisotropy spectra for in situ III-V semiconductor dry-etch monitoring10.1016/j.apsusc.2015.09.040 ↗
11. Precise in-situ etch depth control of multilayered III-V semiconductor samples with reflectance anisotropy spectroscopy (RAS) equipment10.3762/bjnano.7.171 ↗
12. Atomic structure and optical anisotropy of III-V (001) surfaces10.1116/1.1394730 ↗
13. Maskless laser interferometric monitoring of InP/InGaAsP heterostructure reactive ion etching10.1063/1.103751 ↗
14. In situ spectroscopic ellipsometry studies of electron cyclotron resonance (ECR) plasma etching of oxides of silicon and GaAs10.1016/0169-4332(93)90057-I ↗
15. Highly accurate etching of ridge-wave-guide directional-couplers using in situ reflectance monitoring and periodic multilayers10.1063/1.108805 ↗
16. Etch rates of (100), (111) and (110) single-crystal silicon in TMAH measured in situ by laser reflectance interferometry10.1016/S0924-4247(00)00309-5 ↗
17. Two-channel spectroscopic reflectometry for in situ monitoring of blanket and patterned structures during reactive ion etching10.1116/1.1327301 ↗
18. Precise etch-depth control of microlens-integrated intracavity contacted vertical-cavity surface-emitting lasers by in-situ laser reflectometry and reflectivity modeling10.1016/j.tsf.2009.03.198 ↗
19. Chloride-induced morphology transformations of the Cu(110) surface in dilute HCl10.1021/la502589k ↗
20. Atomic layer sensitive in-situ plasma etch depth control with reflectance anisotropy spectroscopy (RAS)10.1117/12.2269708 ↗
21. K. A. Stetson, “Method for measurement of surface profile change using a vernier scale in hologram interferometry,” US patent US3612693A (1971).