journal article·2025-07-16Open access

Micro-nanoscale laser subsurface vertical modification of 4H-SiC semiconductor materials: mechanisms, processes, and challenges

Hongmei Li, Hongwei Wang, Yuxin Li, Xiwen Lu, Lin Li, Yinzhou Yan, Wei Guo

Discover Nano· Volume 20· Issue 1

Abstract

Abstract Wide-bandgap semiconductor materials, exemplified by silicon carbide (SiC), have emerged as pivotal materials in semiconductor devices due to their exceptional chemical stability, high electron mobility, and thermal stability. With the rapid development of microelectronic devices and integrated optical circuits, the demand for high-yield and high-quality processing of SiC wafer has intensified. Traditional SiC wafer processing technologies suffer from low efficiency and high material loss, making it difficult to meet industrial demands. Therefore, the development of efficient, low-damage processing techniques has become a pressing issue in the SiC wafer processing field. Ultrashort pulsed laser processing, with its advantages of contact free processing, no mechanical stress, and small heat-affected zones, has garnered significant attention in SiC wafer processing in recent years. By generating a modified layer within the material, laser processing plays a crucial role in wafer fabrication. However, the key challenge lies in precisely controlling the thickness of the modified layer down to the micro-nano scale to minimize material loss. This review systematically discusses the interaction mechanisms and modification processes of laser with wide-bandgap semiconductor SiC materials. It focuses on the core issue in laser modification technology, where nonlinear effects make it difficult to precisely control the modification layer depth, thereby affecting both modification quality and processing efficiency. To address this, the paper summarizes the differences in modification mechanisms with lasers of varying pulse durations and proposes a multi-strategy solution to improve modification quality and processing efficiency through pulse control and synergistic optimization of process parameters. Additionally, this review provides a comprehensive overview of advanced SiC wafer detachment processes, including cold cracking stripping, chemically assisted stripping, ultrasonic stripping, and multi-laser composite stripping, and identifies the primary challenges and future directions in the field of SiC wafer processing.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (98)

Show source-provided references
1. Miyamoto I, Okamoto Y, Hansen A, et al. High speed, high strength microwelding of si/glass using ps-laser pulses. Opt Express. 2015;23(3):3427–39. https://doi.org/10.1364/OE.23.003427.10.1364/OE.23.003427 ↗
2. Lee SA, Hwang JY, Kim JP, et al. Dielectric characterization of transparent epitaxial Ga2O3 thin film on n-GaN∕ Al2O3 prepared by pulsed laser deposition. Appl Phys Lett. 2006;89(18). https://doi.org/10.1063/1.2374806.10.1063/1.2374806 ↗
3. Li Z, Wang X, Wang J, et al. Stealth dicing of Sapphire sheets with low surface roughness, zero Kerf width, debris/crack-free and zero taper using a femtosecond bessel beam. Opt Laser Technol. 2021;135:106713. https://doi.org/10.1016/j.optlastec.2020.106713.10.1016/j.optlastec.2020.106713 ↗
4. Choyke WJ, Pensl G. Physical properties of SiC. MRS Bull. 1997;22(3):25–9. https://doi.org/10.1557/S0883769400032723.10.1557/S0883769400032723 ↗
5. DiMarino CM, Burgos R, Dushan B. High-temperature silicon carbide: characterization of state-of-the-art silicon carbide power transistors. IEEE Ind Electron Mag. 2015;9(3):19–30. https://doi.org/10.1109/MIE.2014.2360350.10.1109/MIE.2014.2360350 ↗
6. Xiong H, Mao W, Wang R, et al. Characterizations on the doping of single-crystal silicon carbide. Mater Today Phys. 2022;29:100906. https://doi.org/10.1016/j.mtphys.2022.100906.10.1016/j.mtphys.2022.100906 ↗
7. Tsuchida H, Kamata I, Miyazawa T, et al. Recent advances in 4H-SiC epitaxy for high-voltage power devices. Mater Sci Semiconduct Process. 2018;78:2–12. https://doi.org/10.1016/j.mssp.2017.11.003.10.1016/j.mssp.2017.11.003 ↗
8. Kimoto T. Bulk and epitaxial growth of silicon carbide. Prog Cryst Growth Charact Mater. 2016;62(2):329–51. https://doi.org/10.1016/j.pcrysgrow.2016.04.018.10.1016/j.pcrysgrow.2016.04.018 ↗
9. Siddiqui A, Khosa RY, Usman M. High-k dielectrics for 4H-silicon carbide: present status and future perspectives. J Mater Chem C. 2021;9(15):5055–81. https://doi.org/10.1039/D0TC05008C.10.1039/D0TC05008C ↗
10. Eddy CR Jr, Gaskill DK. Silicon carbide as a platform for power electronics. Science. 2009;324(5933):1398–400. https://doi.org/10.1126/science.116870.10.1126/science.116870 ↗
11. Chen PC, Miao WC, Ahmed T, et al. Defect inspection techniques in SiC. Nanoscale Res Lett. 2022;17(1):30. https://doi.org/10.1186/s11671-022-03672-w.10.1186/s11671-022-03672-w ↗
12. Yan L, Zhang X, Li H, et al. Machinability improvement in three-dimensional (3D) ultrasonic vibration assisted diamond wire sawing of SiC. Ceram Int. 2022;48(6):8051–68. https://doi.org/10.1016/j.ceramint.2021.12.006.10.1016/j.ceramint.2021.12.006 ↗
13. Gao Y, Chen Y. Sawing stress of SiC single crystal with void defect in diamond wire saw slicing. Int J Adv Manuf Technol. 2019;103:1019–31. https://doi.org/10.1007/s00170-019-03579-4.10.1007/s00170-019-03579-4 ↗
14. Li S, Tang A, Liu Y, et al. Analytical force modeling of fixed abrasive diamond wire saw machining with application to SiC monocrystal wafer processing. J Manuf Sci Eng. 2017;139(4):041003. https://doi.org/10.1115/1.4034792.10.1115/1.4034792 ↗
15. Qiu J. Fundamental research on machining performance of diamond wire sawing and diamond wire electrical discharge sawing quartz glass. Ceram Int. 2022;48(17):24332–45. https://doi.org/10.1016/j.ceramint.2022.04.327.10.1016/j.ceramint.2022.04.327 ↗
16. Wang Y, Bai T, Shu L, et al. Analytical prediction of subsurface damage depth of monocrystalline silicon in ultrasonic vibration assisted wire sawing. Int J Adv Manuf Technol. 2024;133(5):2445–60. https://doi.org/10.1007/s00170-024-13846-8.10.1007/s00170-024-13846-8 ↗
17. Jiang L, Wang AD, Li B et al. Electrons dynamics control by shaping femtosecond laser pulses in micro/nanofabrication: modeling, method, measurement and application. Light: Sci Appl. 2018;7(2):17134. https://doi.org/10.1038/lsa.2017.134.10.1038/lsa.2017.134 ↗
18. Gattass RR, Mazur E. Femtosecond laser micromachining in transparent materials. Nat Photonics. 2008;2(4):219–25. https://doi.org/10.1038/nphoton.2008.47.10.1038/nphoton.2008.47 ↗
19. Malinauskas M, Žukauskas A, Hasegawa S et al. Ultrafast laser processing of materials: from science to industry. Light Sci Appl. 2016;5(8):e16133. https://doi.org/10.1038/lsa.2016.133.10.1038/lsa.2016.133 ↗
20. Chen Z, Song L, Wang Y, et al. Air pocket-optimization strategy for micro/nanostructures fabricated by femtosecond laser technology for anti-icing performance improvement. Appl Surf Sci. 2024;655:159454. https://doi.org/10.1016/j.apsusc.2024.159454.10.1016/j.apsusc.2024.159454 ↗
21. Ye F, Song L, Wang Y, et al. Femtosecond laser-based construction of 3D spatially distributed graphene oxide surface for enhancing boiling heat transfer. Int J Heat Mass Transf. 2025;237:126405. https://doi.org/10.1016/j.ijheatmasstransfer.2024.126405.10.1016/j.ijheatmasstransfer.2024.126405 ↗
22. Ye F, Wang Y, Yang Y, et al. An internal/external dual heat transfer mode constructed by femtosecond-laser direct writing for enhancing water boiling in graphene oxide surface. Appl Therm Eng. 2025;263:125343. https://doi.org/10.1016/j.applthermaleng.2024.125343.10.1016/j.applthermaleng.2024.125343 ↗
23. Musumeci S, Barba V. Gallium nitride power devices in power electronics applications: state of Art and perspectives. Energies. 2023;16(9):3894. https://doi.org/10.3390/en16093894.10.3390/en16093894 ↗
24. Sugioka K, Cheng Y. Ultrafast lasers—reliable tools for advanced materials processing. Light Sci Appl. 2014;3(4):e149. https://doi.org/10.1038/lsa.2014.30.10.1038/lsa.2014.30 ↗
25. Keller U. Recent developments in compact ultrafast lasers. Nature. 2003;424(6950):831–8. https://doi.org/10.1038/nature01938.10.1038/nature01938 ↗
26. Yamanouchi K, Agostini P, Chin SL, et al. Progress in ultrafast intense laser science II[M]. Springer; 2015. https://doi.org/10.1007/978-3-540-38156-3.10.1007/978-3-540-38156-3 ↗
27. Jiang L, Tsai HL. Energy transport and material removal in wide bandgap materials by a femtosecond laser pulse. Int J Heat Mass Transf. 2005;48(3–4):487–99. https://doi.org/10.1016/j.ijheatmasstransfer.2004.09.016.10.1016/j.ijheatmasstransfer.2004.09.016 ↗
28. Chichkov BN, Momma C, Nolte S, et al. Femtosecond, picosecond and nanosecond laser ablation of solids. Appl Phys A. 1996;63:109–15. https://doi.org/10.1007/BF01567637.10.1007/BF01567637 ↗
29. Jiang K, Zhang P, Song S, et al. A review of ultra-short pulse laser micromachining of wide bandgap semiconductor materials: SiC and GaN. Mater Sci Semiconduct Process. 2024;180:108559. https://doi.org/10.1016/j.mssp.2024.108559.10.1016/j.mssp.2024.108559 ↗
30. Liu X, Du D, Mourou G. Laser ablation and micromachining with ultrashort laser pulses. IEE J Quantum Electron. 1997;33(10):1706–16. https://doi.org/10.1109/3.631270.10.1109/3.631270 ↗
31. Hu K, Guo Z, Cao T, et al. Study on the polarization dependence of nonlinear absorption of ultrafast laser pulses in bulk fused silica. Opt Express. 2022;30(6):8949–58. https://doi.org/10.1364/OE.449608.10.1364/OE.449608 ↗
32. Wu S, Wu D, Xu J, et al. Characterization and mechanism of glass microwelding by double-pulse ultrafast laser irradiation. Opt Express. 2012;20(27):28893–905. https://doi.org/10.1364/OE.20.028893.10.1364/OE.20.028893 ↗
33. Li JQ, Yan JF, Li X, et al. Research advancement on ultrafast laser microprocessing of transparent dielectrics. Chin J Lasers. 2021;48(2):0202019. https://doi.org/10.3788/CJL202148.0202019.10.3788/CJL202148.0202019 ↗
34. Apostolopoulos V, Laversenne L, Colomb T, et al. Femtosecond-irradiation-induced refractive-index changes and channel waveguiding in bulk Ti3+: Sapphire. Appl Phys Lett. 2004;85(7):1122–4. https://doi.org/10.1063/1.1781737.10.1063/1.1781737 ↗
35. Ramirez LPR, Heinrich M, Richter S, et al. Tuning the structural properties of femtosecond-laser-induced nanogratings. Appl Phys A. 2010;100:1–6. https://doi.org/10.1007/s00339-010-5684-2.10.1007/s00339-010-5684-2 ↗
36. Juodkazis S, Vailionis A, Gamaly EG, et al. Femtosecond laser-induced confined microexplosion: tool for creation high-pressure phases. MRS Adv. 2016;1(17):1149–55. https://doi.org/10.1557/adv.2015.41.10.1557/adv.2015.41 ↗
37. Zhang Y, Xie X, Huang Y, et al. Internal modified structure of silicon carbide prepared by ultrafast laser for wafer slicing. Ceram Int. 2023;49(3):5249–60. https://doi.org/10.1016/j.ceramint.2022.10.043.10.1016/j.ceramint.2022.10.043 ↗
38. Miura K, Qiu J, Inouye H, et al. Photowritten optical waveguides in various glasses with ultrashort pulse laser. Appl Phys Lett. 1997;71(23):3329–31. https://doi.org/10.1063/1.120327.10.1063/1.120327 ↗
39. Shimotsuma Y, Kazansky PG, Qiu J, et al. Self-organized nanogratings in glass irradiated by ultrashort light pulses. Phys Rev Lett. 2003;91(24):247405. https://doi.org/10.1103/PhysRevLett.91.247405.10.1103/PhysRevLett.91.247405 ↗
40. Juodkazis S, Nishimura K, Tanaka S, et al. Laser-Induced microexplosion confined in the bulk of a Sapphire crystal: evidence of multimegabar pressures. Phys Rev Lett. 2006;96(16):166101. https://doi.org/10.1103/PhysRevLett.96.166101.10.1103/PhysRevLett.96.166101 ↗
41. Kiyota H, Hara K, Jankowski M, et al. Numerical simulation and validation of subsurface modification and crack formation induced by nanosecond-pulsed laser processing in monocrystalline silicon. J Appl Phys. 2020;127(8). https://doi.org/10.1063/1.5130701.10.1063/1.5130701 ↗
42. Li Y, Zhang Z, Song Q, et al. Surface micromorphology and nanostructures evolution in hybrid laser processes of slicing and Polishing single crystal 4H-SiC. J Mater Sci Technol. 2024;184:235–44. https://doi.org/10.1016/j.jmst.2023.09.046.10.1016/j.jmst.2023.09.046 ↗
43. Dutto C, Fogarassy E, Mathiot D. Numerical and experimental analysis of pulsed excimer laser processing of silicon carbide. Appl Surf Sci. 2001;184(1–4):362–6. https://doi.org/10.1016/S0169-4332(01)00518-9.10.1016/S0169-4332(01)00518-9 ↗
44. Han S, Yu H, He C, et al. Laser slicing of 4H-SiC wafers based on picosecond laser-induced micro-explosion via multiphoton processes. Opt Laser Technol. 2022;154:108323. https://doi.org/10.1016/j.optlastec.2022.108323.10.1016/j.optlastec.2022.108323 ↗
45. Sun W, Ji L, Lin Z, et al. Low-energy UV ultrafast laser controlled lift‐off for high‐quality flexible GaN‐based device. Adv Funct Mater. 2022;32(8):2111920. https://doi.org/10.1002/adfm.202111920.10.1002/adfm.202111920 ↗
46. Li J, Liu F, Zhou W, et al. The influence of cracks in the coupling region of micro-grinding and laser stealth combined dicing on the quality of cutting side walls. J Manuf Process. 2024;119:856–66. https://doi.org/10.1016/j.jmapro.2024.04.020.10.1016/j.jmapro.2024.04.020 ↗
47. Choi I, Jeong HY, Shin H, et al. Laser-induced phase separation of silicon carbide. Nat Commun. 2016;7(1):13562. https://doi.org/10.1038/ncomms13562.10.1038/ncomms13562 ↗
48. Suproniuk M, Kamiński P, Kozłowski R, et al. Current status of modelling the semi-insulating 4H–SiC transient photoconductivity for application to photoconductive switches. Opto-Electron Rev. 2017;25(3):171–80. https://doi.org/10.1016/j.opelre.2017.03.006.10.1016/j.opelre.2017.03.006 ↗
49. Hu G, Zhong G, Xiong X, et al. Improvement of the resistivity uniformity of 8-inch 4H–SiC wafers by optimizing the thermal field. Vacuum. 2024;222:112961. https://doi.org/10.1016/j.vacuum.2024.112961.10.1016/j.vacuum.2024.112961 ↗
50. Cheng Z, Liang J, Kawamura K, et al. High thermal conductivity in wafer-scale cubic silicon carbide crystals. Nat Commun. 2022;13(1):7201. https://doi.org/10.1038/s41467-022-34943-w.10.1038/s41467-022-34943-w ↗
51. Kusunoki K, Seki K, Kishida Y et al. Development of high quality 4H-SiC single crystal wafers grown by solution growth technique. Nippon Steel & Sumimoto Metal Technical Report, 2017: 50–7. https://api.semanticscholar.org/CorpusID:13843506
52. Patel A, Mittal M, Rao DVS, et al. Syntaxy and defect distribution during the bulk growth of 4H-SiC single crystal. J Mater Sci Mater Electron. 2021;32:2187–92. https://doi.org/10.1007/s10854-020-04983-3.10.1007/s10854-020-04983-3 ↗
53. Liu YL. Recent progress on single-crystal growth and epitaxial growth of 4H silicon carbide. Solid State Phenom. 2022;332:73–84. https://doi.org/10.4028/p-4x61u9.10.4028/p-4x61u9 ↗
54. Tsuchida H, Kanda T. Advances in fast 4H–SiC crystal growth and defect reduction by high-temperature gas-source method. Mater Sci Semiconduct Process. 2024;176:108315. https://doi.org/10.1016/j.mssp.2024.108315.10.1016/j.mssp.2024.108315 ↗
55. Yang XL, Pan YN, Gao C, et al. Development of high quality 8 inch 4H-SiC substrates. Solid State Phenom. 2023;344:41–6. https://doi.org/10.4028/p-x44871.10.4028/p-x44871 ↗
56. Chen X, Yang X, Xie X et al. Research progress of large size SiC single crystal materials and devices. Light: Sci Appl. 2023, 12(1): 28. https://doi.org/10.1038/s41377-022-01037-710.1038/s41377-022-01037-7 ↗
57. Yang Y, Tong Z, Pi X, et al. Advances and challenges in 4H silicon carbide: defects and impurities. Phys Scr. 2024. https://doi.org/10.1088/1402-4896/ad6697.10.1088/1402-4896/ad6697 ↗
58. Luo H, Li J, Yang G, et al. Electronic and optical properties of threading dislocations in n-type 4H-SiC. ACS Appl Electron Mater. 2022;4(4):1678–83. https://doi.org/10.1021/acsaelm.1c01330.10.1021/acsaelm.1c01330 ↗
59. Ferro G, Chaussende D. A new model for in situ nitrogen incorporation into 4H-SiC during epitaxy. Sci Rep. 2017;7(1):43069. https://doi.org/10.1038/srep43069.10.1038/srep43069 ↗
60. Li MY, Zhang Q, Pandey P, et al. From the Au nano-clusters to the nanoparticles on 4H-SiC (0001). Sci Rep. 2015;5(1):13954. https://doi.org/10.1038/srep13954.10.1038/srep13954 ↗
61. Nakamura D, Gunjishima I, Yamaguchi S, et al. Ultrahigh-quality silicon carbide single crystals. Nature. 2004;430:1009–12. https://doi.org/10.1038/nature02810.10.1038/nature02810 ↗
62. Chen XF, Xu XG, Hu XB, et al. Anisotropy of chemical mechanical Polishing in silicon carbide substrates. Mater Sci Engineering: B. 2007;142(1):28–30. https://doi.org/10.1016/j.mseb.2007.06.015.10.1016/j.mseb.2007.06.015 ↗
63. Shi S, Yu Y, Wang N, et al. Investigation of the anisotropy of 4H-SiC materials in nanoindentation and scratch experiments. Materials. 2022;15(7):2496. https://doi.org/10.3390/ma15072496.10.3390/ma15072496 ↗
64. Liu X, Wang R, Zhang J, et al. Anisotropic deformation of 4H-SiC wafers: insights from nanoindentation tests. J Phys D. 2022;55(49):494001. https://doi.org/10.1088/1361-6463/ac9535.10.1088/1361-6463/ac9535 ↗
65. Meng B, Yuan D, Xu S. Coupling effect on the removal mechanism and surface/subsurface characteristics of SiC during grinding process at the nanoscale. Ceram Int. 2019;45(2):2483–91. https://doi.org/10.1016/j.ceramint.2018.10.175.10.1016/j.ceramint.2018.10.175 ↗
66. Wen Q, Yang Y, Lu J, et al. Study on picosecond laser stealth dicing of 4H-SiC along $$[11\bar{2}0]$$ and $$[1\bar{1}00]$$ crystal orientations on Si-face and C-face. Opt Laser Technol. 2023;162:109300. https://doi.org/10.1016/j.optlastec.2023.10930010.1016/j.optlastec.2023.109300 ↗
67. Yao Y, Chen Q, Li B, et al. Influence of crystal orientation and incident plane on n-type 4H-SiC wafer slicing by using picosecond laser. Opt Laser Technol. 2025;182:112174. https://doi.org/10.1016/j.optlastec.2024.112174.10.1016/j.optlastec.2024.112174 ↗
68. Qiang K, Xianguang K, Xudong F, et al. Improving machinability and inhibiting surface damage of SiC wafer by ion implantation modification. Chin J Aeronaut. 2025;38(3):103394. https://doi.org/10.1016/j.cja.2024.103394.10.1016/j.cja.2024.103394 ↗
69. Tsai HY, Lin YH, Huang KC, et al. Precision material removal and hardness reduction in silicon carbide using ultraviolet nanosecond pulse laser. Appl Phys A. 2025;131(3):203. https://doi.org/10.1007/s00339-025-08296-2.10.1007/s00339-025-08296-2 ↗
70. Huang Y, Zhou Y, Li J, et al. Femtosecond laser surface modification of 4H-SiC improves machinability. Appl Surf Sci. 2023;615:156436. https://doi.org/10.1016/j.apsusc.2023.156436.10.1016/j.apsusc.2023.156436 ↗
71. Liu H, Li Z, Li J, et al. Removal mechanism on 4H–SiC single crystal by picosecond laser ablation-assisted chemical mechanical Polishing (CMP). Ceram Int. 2024;50(8):13266–75. https://doi.org/10.1016/j.ceramint.2024.01.239.10.1016/j.ceramint.2024.01.239 ↗
72. Wang H, Gao S, Guo X, et al. Atomic Understanding of the plastic deformation mechanism of 4H-SiC under different grain depth-of-cut during nano-grinding. J Electron Mater. 2023;52(7):4865–77. https://doi.org/10.1007/s11664-023-10457-z.10.1007/s11664-023-10457-z ↗
73. Wang W, Lu X, Wu X, et al. Chemical–mechanical Polishing of 4H silicon carbide wafers. Adv Mater Interfaces. 2023;10(13):2202369. https://doi.org/10.1002/admi.202202369.10.1002/admi.202202369 ↗
74. Wang H, Chen Q, Yao Y, et al. Influence of surface preprocessing on 4H-SiC wafer slicing by using ultrafast laser. Crystals. 2022;13(1):15. https://doi.org/10.3390/cryst13010015.10.3390/cryst13010015 ↗
75. Wang L, Zhang C, Liu F, et al. Ultrafast pulsed laser stealth dicing of 4H-SiC wafer: structure evolution and defect generation. J Manuf Process. 2022;81:562–70. https://doi.org/10.1016/j.jmapro.2022.06.064.10.1016/j.jmapro.2022.06.064 ↗
76. Wang L, Zhang C, Liu F, et al. Process mechanism of ultrafast laser multi-focal-scribing for ultrafine and efficient stealth dicing of SiC wafers. Appl Phys A. 2022;128(10):872. https://doi.org/10.1007/s00339-022-06012-y.10.1007/s00339-022-06012-y ↗
77. Zhou Y, Liu F, Cao S, et al. Modulation of ultrafast laser-induced modified structure inside silicon carbide for thin wafer dicing. Mater Sci Semiconduct Process. 2024;182:108730. https://doi.org/10.1016/j.mssp.2024.108730.10.1016/j.mssp.2024.108730 ↗
78. Kim E, Shimotsuma Y, Sakakura M, et al. 4H-SiC wafer slicing by using femtosecond laser double-pulses. Opt Mater Express. 2017;7(7):2450–60. https://doi.org/10.1364/OME.7.002450.10.1364/OME.7.002450 ↗
79. Kim E, Shimotsuma Y, Sakakura M, et al. Ultrashort pulse laser slicing of wide bandgap 4H-SiC crystal. JSAP-OSA joint Symposia. Optica Publishing Group. 2016. https://doi.org/10.11470/jsapmeeting.2016.2.0_1205.10.11470/jsapmeeting.2016.2.0_1205 ↗
80. Kim E, Shimotsuma Y, Sakakura M, et al. Nano periodic structure formation in 4H–SiC crystal using femtosecond laser double-pulses. J Superhard Mater. 2018;40:259–66. https://doi.org/10.3103/S1063457618040056.10.3103/S1063457618040056 ↗
81. Kim E, Shimotsuma Y, Sakakura M, et al. Ultrashort pulse laser slicing of semiconductor crystal. SPIE. 2016;9983:40–5. https://doi.org/10.1117/12.2235146. Pacific Rim Laser Damage 2016: Optical Materials for High-Power Lasers.10.1117/12.2235146 ↗
82. Hirata K. New laser slicing technology named KABRA process enables high speed and high efficiency SiC slicing. Laser-based Micro-and nanoprocessing XII. SPIE. 2018;10520:1052003. https://doi.org/10.1117/12.2291458.10.1117/12.2291458 ↗
83. Siders CW, Siders JLW, Taylor AJ, et al. Efficient high-energy pulse-train generation using a 2n-pulse Michelson interferometer. Appl Opt. 1998;37(22):5302–5. https://doi.org/10.1364/ao.37.005302.10.1364/ao.37.005302 ↗
84. Wang A, Sopeña P, Grojo D. Burst mode enabled ultrafast laser inscription inside gallium arsenide. Int J Extreme Manuf. 2022;4(4):045001. https://doi.org/10.1088/2631-7990/ac8fc3.10.1088/2631-7990/ac8fc3 ↗
85. Xie X, Liu T, Lv K, et al. The internal modified layer structure of silicon carbide induced by ultrafast laser and its application in stealth dicing. Precis Eng. 2024;88:895–904. https://doi.org/10.1016/j.precisioneng.2024.05.006.10.1016/j.precisioneng.2024.05.006 ↗
86. Liu X, Hong M. Micro-cracks generation and growth manipulation by all-laser processing for low kerf-loss and high surface quality SiC slicing. Opt Express. 2024;32(22):38758–67. https://doi.org/10.1364/OE.540604.10.1364/OE.540604 ↗
87. Ma R, Ji L, Yan T. Laser multi-focus precision cutting of Thick Sapphire by spherical aberration rectification. Opt Lasers Eng. 2020;126:105876. https://doi.org/10.1016/j.optlaseng.2019.105876.10.1016/j.optlaseng.2019.105876 ↗
88. Jiang M, Sun S, Wang J, et al. Axial multi-focus stealth cutting method based on the fractional fourier transform for quartz glass. Ceram Int. 2023;49(11):18296–304. https://doi.org/10.1016/j.ceramint.2023.02.201.10.1016/j.ceramint.2023.02.201 ↗
89. Geng Q, Wang D, Chen P, et al. Ultrafast multi-focus 3-D nano-fabrication based on two-photon polymerization. Nat Commun. 2019;10(1):2179. https://doi.org/10.1038/s41467-019-10249-2.10.1038/s41467-019-10249-2 ↗
90. Du J, Zhao S, Lu X et al. Multi-focal picosecond laser vertical slicing of 6 inch 4H-SiC ingot. 2024. https://doi.org/10.48550/arXiv.2411.18093.10.48550/arXiv.2411.18093 ↗
91. Lu X, Zhao S, Du J, et al. Laser double-layer slicing of SiC wafers by using axial dual-focus. Opt Express. 2025;33(5):9775–89. https://doi.org/10.1364/OE.553210.10.1364/OE.553210 ↗
92. Swoboda M, Beyer C, Rieske R et al. Laser assisted SiC wafering using COLD SPLIT. Materials Science Forum. Trans Tech Publications Ltd, 2017;897:403–06. https://doi.org/10.4028/www.scientific.net/MSF.897.403.10.4028/www.scientific.net/MSF.897.403 ↗
93. Geng W, Shao Q, Pei Y, et al. Slicing of 4H-SiC wafers combining ultrafast laser irradiation and bandgap‐selective photo‐electrochemical exfoliation. Adv Mater Interfaces. 2023;10(21):2300200. https://doi.org/10.1002/admi.202300200.10.1002/admi.202300200 ↗
94. Lv B, Ye L, Zhu X, et al. Ultrasonic-assisted stripping of single-crystal SiC after laser modification. Ceram Int. 2024;50(22):48517–25. https://doi.org/10.1016/j.ceramint.2024.09.200.10.1016/j.ceramint.2024.09.200 ↗
95. Lumley RM. Controlled separation of brittle materials using a laser. Ceramic Bull. 1969;48(9):850. https://cir.nii.ac.jp/crid/1570854174493273472.
96. Huang KC, Wu WH, Tseng SF et al. The mixed processing models development of thermal fracture and laser ablation on glass substrate. AIP Conference Proceedings. American Institute of Physics, 2011;1315(1):1612–7. https://doi.org/10.1063/1.3552422.10.1063/1.3552422 ↗
97. Deng L, Yang H, Zeng X, et al. Study on mechanics and key technologies of laser nondestructive mirror-separation for KDP crystal. Int J Mach Tools Manuf. 2015;94:26–36. https://doi.org/10.1016/j.ijmachtools.2015.04.001.10.1016/j.ijmachtools.2015.04.001 ↗
98. Jiang L, Zhao S, Han S, et al. CW laser-assisted splitting of SiC wafer based on modified layer by picosecond laser. Opt Laser Technol. 2024;174:110700. https://doi.org/10.1016/j.optlastec.2024.110700.10.1016/j.optlastec.2024.110700 ↗