Thermodynamic Ground States of Complex Oxide Heterointerfaces
Source abstract
Abstract
The formation mechanism of 2-dimensional electron gases (2DEGs) at heterointerfaces between nominally insulating oxides is addressed with a thermodynamical approach. We provide a comprehensive analysis of the thermodynamic ground states of various 2DEG systems directly probed in high temperature equilibrium conductivity measurements. We unambiguously identify two distinct classes of oxide heterostructures: For epitaxial perovskite/perovskite heterointerfaces (LaAlO 3 /SrTiO 3, NdGaO 3 /SrTiO 3, and (La,Sr)(Al,Ta)O 3 /SrTiO 3 ), we find the 2DEG formation being based on charge transfer into the interface, stabilized by the electric field in the space charge region. In contrast, for amorphous LaAlO 3 /SrTiO 3 and epitaxial γ-Al 2 O 3 /SrTiO 3 heterostructures, the 2DEG formation mainly relies on the formation and accumulation of oxygen vacancies. This class of 2DEG structures exhibits an unstable interface reconstruction associated with a quenched nonequilibrium state.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Electronic Materials, IWE2, RWTH Aachen University, 52056 Aachen, Germany
Peter Gruenberg Institute and JARA-FIT, Forschungszentrum Juelich GmbH, 52425 Juelich, Germany
Department of Energy Conversion and Storage, Technical University of Denmark, Risø Campus, 4000 Roskilde, Denmark
References (30)
Show source-provided references
1. 10.1038/nmat322310.1038/nmat3223 ↗
2. 10.1038/nmat296510.1038/nmat2965 ↗
3. 10.1038/nature0230810.1038/nature02308 ↗
4. 10.1038/nmat156910.1038/nmat1569 ↗
5. 10.1126/science.113109110.1126/science.1131091 ↗
6. 10.1126/science.114600610.1126/science.1146006 ↗
7. 10.1063/1.479250910.1063/1.4792509 ↗
8. 10.1021/nl504622w10.1021/nl504622w ↗
9. 10.1063/1.349644010.1063/1.3496440 ↗
10. 10.1103/PhysRevB.86.08545010.1103/PhysRevB.86.085450 ↗
11. Huang, Z.; Han, K.; Zeng, S.; Motapothula, M.; Borisevich, A. Y.; Ghosh, S.; L, W.; Li, C.; Zhou, W.; Liu, Z.; Coey, M.; Venkatesan, T.; Ariando, The Effect of Polar Fluctuation and Lattice Mismatch on Carrier Mobility at Oxide Interfaces.Nano Lett. 2016.10.1021/acs.nanolett.5b04814 ↗
12. 10.1021/nl201821j10.1021/nl201821j ↗
13. 10.1063/1.481598910.1063/1.4815989 ↗
14. 10.1103/PhysRevX.3.02101010.1103/PhysRevX.3.021010 ↗
15. 10.1038/ncomms239410.1038/ncomms2394 ↗
16. 10.1038/nature0972010.1038/nature09720 ↗
17. 10.1021/nl302214x10.1021/nl302214x ↗
18. 10.1038/nmat430310.1038/nmat4303 ↗
19. 10.1103/PhysRevB.93.24543110.1103/PhysRevB.93.245431 ↗
20. 10.1063/1.367913910.1063/1.3679139 ↗
21. 10.1063/1.345738610.1063/1.3457386 ↗
22. 10.1111/j.1551-2916.2006.01178.x10.1111/j.1551-2916.2006.01178.x ↗
23. Smyth D. M. · 2000
24. 10.1111/j.1151-2916.1997.tb03157.x10.1111/j.1151-2916.1997.tb03157.x ↗
25. 10.1038/nmat193110.1038/nmat1931 ↗
26. 10.1038/srep2241010.1038/srep22410 ↗
27. 10.1103/PhysRevX.6.03103510.1103/PhysRevX.6.031035 ↗
28. 10.1016/j.ssi.2012.08.00510.1016/j.ssi.2012.08.005 ↗
29. 10.1103/PhysRevLett.101.02680210.1103/PhysRevLett.101.026802 ↗
30. 10.1103/PhysRevB.91.16511810.1103/PhysRevB.91.165118 ↗