Abstract

Perovskite Sr(1-x)Ce(x)CoO(3-δ) (0.05 ≤ x ≤ 0.15) have been prepared by a sol-gel method and studied as cathodes for intermediate temperature solid oxide fuel cells. As SOFC cathodes, Sr(1-x)Ce(x)CoO(3-δ) materials have sufficiently high electronic conductivities and excellent chemical compatibility with SDC electrolyte. The peak power density of cells with Sr(0.95)Ce(0.05)CoO(3-δ) is 0.625 W cm(-2) at 700 °C. By forming a composite cathode with an oxygen ion conductor SDC, the peak power density of the cell with Sr(0.95)Ce(0.05)CoO(3-δ)-30 wt %SDC composite cathode, reaches 1.01 W cm(-2) at 700 °C, better than that of Sm(0.5)Sr(0.5)CoO(3)-based cathode. All these results demonstrates that Sr(1-x)Ce(x)CoO(3-δ) (0.05 ≤ x ≤ 0.15)-based materials are promising cathodes for an IT-SOFC.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Beijing National Laboratory for Condensed Matter Physics, Institute of Physics, Chinese Academy of Sciences, Beijing 100190, China

Key Laboratory for Renewable Energy, Chinese Academy of Science, Beijing Key Laboratory for New Energy Materials and Devices, Beijing 100190, China

CAS Key Laboratory for Materials for Energy Conversion, Department of Materials Science and Engineering, University of Science and Technology of China, Hefei 230026, China

References (19)

Show source-provided references
1. Sun C. W. · J. Power Sources. · 2007 · 171 · 24710.1016/j.jpowsour.2007.06.086 ↗
2. Sun C. W. · J. Solid State Electrochem. · 2010 · 14 · 112510.1007/s10008-009-0932-0 ↗
3. Hui R. · Electrochim. Acta · 2010 · 55 · 477210.1016/j.electacta.2010.03.053 ↗
4. Shao Z. P. · Nature · 2004 · 431 · 17010.1038/nature02863 ↗
5. Yan A. Y. · Appl. Catal., B · 2006 · 66 · 6410.1016/j.apcatb.2006.02.021 ↗
6. Yan A. Y. · Appl. Catal., B · 2008 · 80 · 2410.1016/j.apcatb.2007.11.007 ↗
7. James M. · Mater. Res. Bull. · 2005 · 40 · 141510.1016/j.materresbull.2005.03.025 ↗
8. Maignan A. · J. Phys.: Condens. Mater. · 2006 · 18 · 4305
9. Wei Q. T. · J. Mater. Sci. · 2005 · 40 · 131710.1007/s10853-005-6961-x ↗
10. Larson A. C. · 2004
11. Tian R. F. · Solid State Ionics · 2011 · 192 · 58010.1016/j.ssi.2010.08.003 ↗
12. Sun C. W. · Nanotechnology · 2005 · 16 · 145410.1088/0957-4484/16/9/006 ↗
13. Shannon R. D. · Acta Crystallogr., Sect. A · 1976 · 32 · 75110.1107/S0567739476001551 ↗
14. Trofimenko N. E. · J. Eur. Ceram. Soc. · 2000 · 20 · 124110.1016/S0955-2219(99)00292-7 ↗
15. Huang C. · J. Power Sources · 2010 · 195 · 517610.1016/j.jpowsour.2010.02.080 ↗
16. Baek S. · J. Power Sources · 2009 · 193 · 43110.1016/j.jpowsour.2009.03.071 ↗
17. Jiang S. P. · Mater. Sci. Eng., A · 2006 · 418 · 19910.1016/j.msea.2005.11.052 ↗
18. Sun C. W. · Electrochem. Commun. · 2006 · 8 · 83310.1016/j.elecom.2006.03.018 ↗
19. Li Y. · Chem. Mater. · 2011 · 23 · 503710.1021/cm202542q ↗