Thermoelectric properties of Fe_(0.92)Mn_(0.08)Si_x semiconductor
Source abstract
Abstract
Fe_(0.92)Mn_(0.08)Si__x_(_x_=1.9, 2.0, 2.1, 2.3, 2.5) thermoelectric alloys have been prepared by rapid solidification and hot uniaxial pressing (HUP) with 50 MPa for 30min at 975℃. XRD analyses showed that all samples reached to phase equilibrium after HUP and the α-Fe_2Si_5 transformed completely to β-FeSi_2 phase after 800℃ annealing for 20h. 93%~98% of the theoretical densities have been obtained by the annealed samples. It was found that a small amount of dispersed fine silicon particles were of benefit to the improvement of the thermoelectric figure of merit of β-FeSi_2 based alloys. The highest figure of merit, 0.18, has been obtained for the sample Fe_(0.92)Mn_(0.08)Si_(2.1) at 650℃. However, when more excessive silicon added, the thermoelectric figures of merit decrease due to higher thermal conductivities.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Metallurgical and Alloy Processes · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.