article·2009-01-01Open access

Interlining thick film process and dielectric property of uncooled infrared detector

Lifang Zhang

Open full text

Abstract

The stable precursor gel of thick film is formed by uniform dispersion of nano-powder into the BST sol.The nano-powder is obtained by a new sol-gel method by means of 4mol% Mn doping,with Ba,Sr and manganese acetate as raw materials.In addition,Ba/Sr ratio is 60/40,65/35 and 70/30,respectively.The BST thin film of with 0.4mol/L concentration is used to be the interlining between the thick films with different components.The BST dielectric-reinforced interlining thick film of around 6-10μm thickness is made in the composite LNO/Pt/Ti/SiO2/Si bottom electrode by spin-coating process.The XRD measurement shows that the interlining thick film by 2h heating treatment at 650℃ is a single perovskite phase.The relative dielectric constant er and dielectric loss tanδ of the interlining thick film by two-hour heating treatment at 700℃ are approximately 1200 and 0.03 in the case of 25℃ and 1kHz,respectively.The dielectric-temperature change rate is over 1.2%/℃ within a wide range near 25℃.The surface of BST interlining thick film is very smooth and compact without any fracture.Thus,the BST interlining thick film is seen as the preferable material for large UFPA.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Gas Sensing Nanomaterials and Sensors · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.