Microscopic and elemental analysis of temperature-induced changes in sulfur/silicon nitride stack-passivated Si surface
Source abstract
Abstract
Sulfur (S) passivation on phosphorus (n+) diffused n-type textured Czochralski (Cz) Si wafers capped with a 100 nm hydrogenated amorphous silicon nitride (a-SiNX:H) layer demonstrated excellent stability under heat and light with saturation current density (J0n+) < 80 fA/cm2. However, S-passivation with only a thin (30 nm) a-SiNX:H capping layer showed rather unstable behavior after thermal treatment. This degradation was correlated to the unstable surface chemistry due to blister formation after thermal treatment at ≥300OC and possible oxidation of the S-passivated surface. Photoluminescence (PL) imaging showed that decrement of effective carrier lifetime (τeff) occurs because of disrupted surface passivation after thermal treatment. Fourier transform infrared spectroscopy (FTIR) demonstrated that these blister formations were caused by hydrogen (H2) effusion from Si-H and N-H bonds dissociation upon thermal processing. Time of flight secondary ion mass spectroscopy (ToF-SIMS) provided proof of S-reacted surface oxidation after thermal treatment which degraded the passivation quality.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Ion-surface interactions and analysis · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Laser-powered co-firing process for highly efficient Si solar cells10.1109/JPHOTOV.2020.3043856 ↗
2. 22.8% efficient silicon solar cell10.1063/1.101596 ↗
3. Progress in p-type tunnel oxide-passivated contact solar cells with screen-printed contacts10.1002/solr.202100152 ↗
4. Instability of dielectric surface passivation quality at elevated temperature and illumination10.1016/j.egypro.2016.07.061 ↗
5. Investigation of charge carrier injection in silicon nitride/silicon junctions10.1063/1.117772 ↗
6. Surface passivation of high-efficiency silicon solar cells by atomic-layer-deposited Al2O310.1002/pip.823 ↗
7. Low-temperature surface passivation of moderately doped crystalline silicon by atomic-layer-deposited hafnium oxide films10.1016/j.egypro.2012.02.010 ↗
8. Improving the performance of amorphous and crystalline silicon heterojunction solar cells by monitoring surface passivation10.1016/j.jnoncrysol.2011.12.063 ↗
9. Improving ALD-Al2O3 surface passivation of Si utilizing pre-existing SiOx10.1109/JPHOTOV.2022.3169985 ↗
10. Plasma treatment for chemical SiOx enables excellent passivation of p-type polysilicon passivating contact featuring the lowest J0 of ∼6 fA/cm210.1016/j.solmat.2023.112354 ↗
11. Improving surface passivation on very thin substrates for high efficiency silicon heterojunction solar cells10.1016/j.solmat.2020.110715 ↗
12. Plasma-initiated rehydrogenation of amorphous silicon to increase the temperature processing window of silicon heterojunction solar cells10.1063/1.4958831 ↗
13. Degradation and regeneration of n+-doped poly-Si surface passivation on p-Type and n-Type Cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
14. Direct detection of free H2 outgassing in blisters formed in Al2O3 atomic layers deposited on Si and methods of its prevention10.1021/acsami.1c20660 ↗
15. Very low surface recombination velocities on p- and n-type silicon wafers passivated with hydrogenated amorphous silicon films
16. Surface passivation by rehydrogenation of silicon-nitride-coated silicon wafers10.1002/pip.580 ↗
17. “On the blistering of atomic layer deposited Al2O3 as Si surface passivation
18. Electronic passivation of silicon surfaces by thin films of atomic layer deposited gallium oxide10.1063/1.4890737 ↗
19. L. Hennen, E.H.A. Granneman, W.M.M. Kessels, Analysis of blister formation in spatial ALD Al2O3 for silicon surface passivation, in: 38th IEEE Photovoltaic Specialists Conference, pp. 001049–001054, 2012, doi: 10.1109/PVSC.2012.6317783.10.1109/PVSC.2012.6317783 ↗
20. Impact of doping and silicon substrate resistivity on the blistering of atomic layer deposited aluminium oxide10.1016/j.apsusc.2020.146400 ↗
21. The impact of deposition and annealing temperature on the growth properties and surface passivation of silicon dioxide films obtained by atomic layer deposition10.1016/j.apsusc.2020.148889 ↗
22. Optimum hydrogen injection in phosphorus-doped polysilicon passivating contacts10.1021/acsami.1c17342 ↗
23. Formation and suppression of hydrogen blisters in tunnelling oxide passivating contact for crystalline silicon solar cells10.1038/s41598-020-66801-4 ↗
24. U.K. Das, R. Theisen, G. Hanket, A. Upadhyaya, A. Rohatgi, A. Hua, L. Weinhardt, D. Hauschild, C. Heske, Sulfurization as a promising surface passivation approach for both n-and p-type Si, in: 47th IEEE PVSC Conf. Proc. p 1167, 2020, doi: 10.1109/PVSC45281.2020.9300395.10.1109/PVSC45281.2020.9300395 ↗
25. High-efficiency Si Solar Cell: Si/SiO2, interface parameters and their impact on device performance
26. Grain boundary passivation in multicrystalline silicon using hydrogen sulfide10.1149/2.0301505jss ↗
27. Efficient passivation of n-type and p-type silicon surface defects by hydrogen sulfide gas reaction10.1088/1361-648X/ac1ec8 ↗
28. I.K. Lam, Advances for solar cells: CIGS absorber fabrication; capacitance-voltage characterization and predictive modelling, Doctoral dissertation, University of Delaware, https://udspace.udel.edu/handle/19716/32464.
29. Dopant diffused Si surface passivation by H2S gas reaction and quinhydrone-methanol treatment
30. Hydrogen sulfide passivation for p-type passivated emitter and rear contact solar cells10.1109/JPHOTOV.2023.3338095 ↗
31. Analysis of silicon wafer surface preparation for heterojunction solar cells using X-ray photoelectron spectroscopy and effective minority carrier lifetime10.1016/j.solmat.2018.03.006 ↗
32. Surface defect passivation and reaction of c-Si in H2S10.1021/acs.langmuir.7b03520 ↗
33. Contactless determination of current–voltage characteristics and minority-carrier lifetimes in semiconductors from quasi-steady-state photoconductance data10.1063/1.117723 ↗
34. Measuring and interpreting the lifetime of silicon wafers10.1016/j.solener.2003.07.033 ↗
35. Silicon nitride film for solar cells10.1016/j.renene.2007.12.015 ↗
36. Si surface passivation by sulfur and reduction of interface defect recombination
37. Silicon lifetime enhancement by SiNx: H anti-reflective coating deposed by PECVD using SiH4 and N2 reactive gas10.1016/j.solener.2012.01.021 ↗
38. Reaction of H2S with Si (100)10.1021/jp0002446 ↗
39. Al-enhanced PECVD SiNX induced hydrogen passivation in string ribbon silicon10.1007/s11664-001-0093-0 ↗
40. The effect of low and high temperature anneals on the hydrogen content and passivation of Si surface coated with SiO2 and SiN films
41. Occurrence of sharp hydrogen effusion peaks of hydrogenated amorphous silicon film and its connection to void structures10.1002/pssb.202000097 ↗
42. Rapid thermal annealing of p-type polysilicon passivated contacts silicon solar cells10.1109/JPHOTOV.2023.3241790 ↗
43. Effect of temperature on graphite oxidation behavior10.1016/j.nucengdes.2003.11.004 ↗