journal article·2006-04

Enhancement of coercivity with reduced grain size in CoCrPt film grown by pulsed laser deposition

Q. Liang, X.F. Hu, H.Q. Li, X.X. He, Xiaoru Wang, W. Zhang

Applied Surface Science· Volume 252· Issue 13
Publisher page

Abstract

Abstract We report a pulsed laser deposition (PLD) growth of VMn/CoCrPt bilayer with a magnetic coercivity ( H c ) of 2.2 kOe and a grain size of 12 nm. The effects of VMn underlayer on magnetic properties of CoCrPt layer were studied. The coercivity, H c , and squareness, S , of VMn/CoCrPt bilayer, is dependent on the thickness of VMn. The grain size of the CoCrPt film can also be modified by laser parameters. High laser fluence used for CoCrPt deposition produces a smaller grain size. Enhanced H c and reduced grain size in VMn/CoCrPt is explained by more pronounced surface phase segregation during deposition at high laser fluence.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic properties of thin films · ZnO doping and properties · Plasma Diagnostics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Parker · J. Appl. Phys. · 1993 · 73 · 566010.1063/1.353634 ↗
2. Abarra · IEEE Trans. Magn. · 1997 · 33 · 299510.1109/20.617822 ↗
3. Shiroishi · J. Appl. Phys. · 1993 · 73 · 556910.1063/1.353653 ↗
4. Chrisey · 1994
5. 1993 · vol. 124
6. Barnard · J. Appl. Phys. · 1994 · 73 · 637210.1063/1.352654 ↗
7. Dova · J. Appl. Phys. · 1999 · 85 · 277510.1063/1.369593 ↗
8. Pprotte · IEEE J. Solid State Circuits · 1994 · 29 · 100210.1109/4.297713 ↗
9. Zheng · J. Appl. Phys. · 2002 · 91 · 800710.1063/1.1456416 ↗