Erosion–corrosion resistance of electroplated Co-Pd film on 316L stainless steel in a hot sulfuric acid slurry environment

Sirui Li, Yu Zuo, Pengfei Ju

Publisher page

Abstract

Abstract A Co-Pd film was deposited on 316L stainless steel by electroplating. The erosion–corrosion behavior of the Co-Pd plated samples in hot sulfuric acid solution with SiO 2 particles was investigated. The results showed that there was a significant synergistic effect between erosion and corrosion. At higher stirring speed, even in such strong corrosive environment the erosion–corrosion rate of Co-Pd plated samples was controlled mainly by the erosion resistance. The erosion–corrosion resistance of pure Pd plated sample decreased rapidly with increasing stirring speed, whereas that of Co-Pd plated sample kept almost stable under the tested conditions due to the high micro-hardness and good corrosion resistance of the film.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Stainless steel in construction: a review of research, applications, challenges and opportunities10.1016/j.jcsr.2008.07.011 ↗
2. El-Sayed M. Sherif, J.H. Potgieter, J.D. Comins, L. Cornish, P.A. Olubambi, C.N. Machio, The beneficial effect of ruthenium additions on the passivation of duplex stainless steel corrosion in sodium chloride solutions, Corros. Sci. 51 (2009) 1364–1371.10.1016/j.corsci.2009.03.022 ↗
3. Corrosion behaviour of superferritic stainless steels cathodically modified with minor additions of ruthenium in sulphuric and hydrochloric acids10.1016/j.matdes.2008.08.019 ↗
4. Self-passivation of Fe-Cr-PGM alloys in reducing acids studied by electrochemical and electron spectroscopic techniques10.1016/0169-4332(90)90040-7 ↗
5. The enhanced passivation of 316L stainless steel in a simulated fuel cell environment by surface plating with palladium10.1016/j.corsci.2012.09.037 ↗
6. Study on corrosion resistance of palladium films on 316L stainless steel by electroplating and electroless plating10.1016/j.corsci.2008.07.014 ↗
7. Chromium-palladium films on 316L stainless steel by pulse electrodeposition and their corrosion resistance in hot sulfuric acid solutions10.1016/j.corsci.2011.07.029 ↗
8. The electroplated palladium-copper alloy film on 316L stainless steel and its corrosion resistance in mixture of acetic and formic acids10.1016/j.corsci.2009.05.008 ↗
9. The characteristics of a Pd-Ni/Pd-Cu double coating on 316L stainless steel and the corrosion resistance in stirred boiling acetic and formic acids mixture10.1016/j.matchemphys.2013.12.024 ↗
10. The electroplated Pd-Co alloy film on 316L stainless steel and the corrosion resistance in boiling acetic acid and formic acid mixture with stirring10.1016/j.apsusc.2014.10.013 ↗
11. Erosion-corrosion behaviour of high-velocity oxy-fuel Ni-Cr-Mo-Si-B coatings under high-velocity seawater jet impingement10.1016/j.wear.2005.01.038 ↗
12. The synergistic effect between erosion and corrosion in acidic slurry medium10.1016/0043-1648(95)07132-6 ↗
13. M.M. Stack, T.M. Abd El Badia, Mapping erosion–corrosion of WC/Co-Cr based composite coatings: particle velocity and applied potential effects, Surf. Coat. Technol. 201 (2006) 1335–1347.10.1016/j.surfcoat.2006.01.069 ↗
14. The electrochemical response of stainless steels in liquid-solid impingement10.1016/j.wear.2004.09.043 ↗
15. The influence of impingement angle on the erosion of ductile metals by angular abrasive particles10.1016/0043-1648(92)90206-N ↗
16. Erosion–corrosion of passive metals by solid particles10.1016/0010-938X(93)90198-P ↗
17. The erosion of four materials using seven erodents–towards an understanding10.1016/S0043-1648(99)00176-3 ↗
18. Effect of impact angle on the slurry erosion-corrosion of 304L stainless steel10.1016/S0043-1648(00)00344-6 ↗
19. Slurry erosion–corrosion behaviour of high-velocity oxy-fuel (HVOF) sprayed Fe-based amorphous metallic coatings for marine pump in sand-containing NaCl solutions10.1016/j.corsci.2011.05.062 ↗
20. Erosion–corrosion resistance of microcrystalline and near-nanocrystalline WC-17Co high velocity oxy-fuel thermal spray coatings10.1016/j.corsci.2011.02.028 ↗
21. The effect of TiN coating on erosion-corrosion resistance of α-Ti alloy in saline slurry10.1016/S0010-938X(99)00050-5 ↗
22. Effect of plasma immersion ion implantation of nitrogen on the wear and corrosion behavior of 316LVM stainless steel10.1016/j.surfcoat.2006.08.149 ↗
23. Electrolytic deposition of Ni-Co-Al2O3 composite coating on pipe steel for corrosion/erosion resistance in oil sand slurry10.1016/j.electacta.2007.07.013 ↗
24. Erosion-corrosion resistance of Ni composite coatings with embedded SiC nanoparticles10.1016/j.electacta.2013.08.185 ↗
25. Corrosion, erosion-corrosion and wear resistance of HVOF sprayed WC type coatings with a corrosion resistant binder
26. Erosion resistance of CO2 corrosion scales formed on API P110 carbon steel10.1016/j.corsci.2014.04.051 ↗
27. Moulder · 1992
28. XPS and XRD investigation of Co/Pd/TiO2 catalysts by different preparation methods10.1016/j.elspec.2009.05.012 ↗
29. Microstructure and tribological properties of electrodeposited Ni-Co alloy deposits10.1016/j.apsusc.2004.08.033 ↗
30. Corrosion resistance and microstructure of electrodeposited nickel-cobalt alloy coatings10.1016/j.surfcoat.2006.06.017 ↗
31. In situ X-ray diffraction study of stacking fault formation in the near-surface region of transformation induced plasticity steels10.1016/j.tsf.2012.07.067 ↗
32. Effect of stacking fault energy on mechanical properties of nanostructured FCC materials processed by the ARB process10.1016/j.msea.2014.03.126 ↗
33. Effect of cold work on erosion-corrosion of 304 stainless steel10.1016/j.corsci.2010.09.059 ↗
34. The effect of substrate hardness on the erosion-corrosion resistance of materials in low-velocity conditions10.1016/0010-938X(93)90323-9 ↗
35. A study of the erosion-corrosion behaviour of engineering steels for marine pumping applications10.1016/0043-1648(95)07145-8 ↗
36. Effects of particle angular velocity and friction force on erosion enhanced corrosion of 304 stainless steel10.1016/j.corsci.2010.05.012 ↗
37. Single particle impingement current transients for prediction of erosion-enhanced corrosion on 304 stainless steel10.1016/j.corsci.2010.03.007 ↗
38. Single particle impact experiments for studying particle induced flow corrosion10.1016/j.corsci.2006.05.021 ↗
39. Erosion-corrosion behavior of nano-particle-reinforced Ni matrix composite alloying layer by duplex surface treatment in aqueous slurry environment10.1016/j.corsci.2009.02.029 ↗
40. Effects of thickness and field strength of anodic oxide film on aluminum on its compressive rupture10.1515/corrrev-2012-0009 ↗
41. Erosion-corrosion of stainless steel under impingement by a fluid jet10.1016/j.corsci.2006.05.012 ↗
42. An electrochemical impedance spectroscopy and polarization study of nanocrystalline Co and Co-P alloy in 0.1M H2SO4 solution10.1016/j.electacta.2005.06.037 ↗
43. Effect of conducting composite polypyrrole/polyaniline coatings on the corrosion resistance of type 304 stainless steel for bipolar plates of proton-exchange membrane fuel cells10.1016/j.jpowsour.2008.04.056 ↗
44. Effect of temperature and erosion on pitting corrosion of X100 steel in aqueous silica slurries containing bicarbonate and chloride content10.1016/j.corsci.2014.01.021 ↗
45. Velocity effects on erosion-corrosion of CrN/NbN superlattice PVD coatings10.1016/j.surfcoat.2005.11.143 ↗
46. Relationship between the effects of velocity and alloy corrosion resistance in erosion-corrosion environments at elevated temperatures10.1016/0043-1648(94)06536-5 ↗
47. Effect of particle velocity and impact angle on the corrosion-erosion of AISI 304 and AISI 420 stainless steels10.1016/j.wear.2005.02.032 ↗
48. Erosion and corrosion properties of WC coatings and duplex stainless steel in sand-containing synthetic sea water10.1016/0043-1648(95)07148-2 ↗