Dealloying of single-phase Al2Au to nanoporous gold ribbon/film with tunable morphology in inorganic and organic acidic media
Source abstract
Abstract
Abstract In this paper, the dealloying of single-phase Al 2 Au ribbons and morphological evolution of nanoporosity have been investigated in different inorganic and organic acid solutions. The results demonstrate that the acid strength coupled with the nature of acid anions can significantly influence the dealloying velocity, adatom diffusion and morphological evolution of the resultant nanoporous Au. Compared with those in inorganic acids, the dealloying velocities can be greatly reduced in organic carboxylic acids and severe passivation is prone to occur. The underlying mechanism of passivation occurring at the dealloying front in the organic acids has also been discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nanoporous metals and alloys · Electrocatalysts for Energy Conversion · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Corrosion micromorphology of noble metal alloys and depletion gilding10.1038/282597a0 ↗
2. Evolution of nanoporosity in dealloying10.1038/35068529 ↗
3. Nanoporous metals for catalytic and optical applications10.1557/mrs2009.156 ↗
4. Nanoporous metals by alloy corrosion: formation and mechanical properties10.1557/mrs2009.157 ↗
5. Hydrogen storage properties of nanoporous palladium fabricated by dealloying10.1021/jp909479m ↗
6. Monolithic nanoporous copper by dealloying Mn–Cu10.1557/jmr.2006.0322 ↗
7. Fabrication and surface functionalization of nanoporous gold by electrochemical alloying/dealloying of Au–Zn in an ionic liquid, and the self-assembly of l-cysteine monolayers10.1002/adfm.200400382 ↗
8. Electrochemical and morphological characterization of Pt–Cu dealloying10.1149/1.2048140 ↗
9. Formation and microstructure of nanoporous silver by dealloying rapidly solidified Zn–Ag alloys10.1016/j.electacta.2011.12.103 ↗
10. Fabrication of nanoporous palladium by dealloying and its thermal coarsening10.1016/j.jallcom.2008.12.078 ↗
11. CO oxidation over a fine porous gold catalyst fabricated by selective leaching from an ordered AuCu3 intermetallic compound10.1007/s10562-007-9344-x ↗
12. Generalized fabrication of nanoporous metals (Au, Pd, Pt, Ag, Cu) through chemical dealloying10.1021/jp811445a ↗
13. Nanoporous gold leaf: “ancient technology”/advanced material10.1002/adma.200400792 ↗
14. Formation, control and functionalization of nanoporous silver through changing dealloying media and elemental doping10.1039/c0ce00900h ↗
15. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
16. Passivation and pitting corrosion of α-brass (Cu/Zn: 63/37) in neutral buffer solutions containing chloride ions10.1002/maco.19900411106 ↗
17. The pitting potential of aluminum in halide solutions10.1002/maco.19910420404 ↗
18. Passive film structure of supersaturated Al–Mo alloys10.1149/1.2085392 ↗
19. The corrosion and passivity of aluminum exposed to dilute sodium sulfate solutions10.1016/0010-938X(87)90037-0 ↗
20. Evolution of structure composition, and stress in nanoporous gold thin films with grain-boundary cracks10.1007/s11661-008-9625-z ↗
21. A benign route to fabricate nanoporous gold through electrochemical dealloying of Al–Au alloys in a neutral solution10.1016/j.electacta.2009.05.089 ↗
22. Potential and concentration dependent electrochemical dealloying of Al2Au in sodium chloride solutions10.1021/jp210488t ↗
23. An atomistic description of dealloying10.1149/1.1784820 ↗
24. Ultrafine nanoporous gold by low-temperature dealloying and kinetics of nanopore formation10.1063/1.2773757 ↗
25. Kinetics of particle coarsening at gold electrode/electrolyte solution interfaces followed by in situ scanning tunneling microscopy10.1149/1.1836466 ↗
26. Dealloying of Ag–Au alloys in halide-containing electrolytes10.1149/1.1580824 ↗
27. Metallic corrosion10.1126/science.263.5154.1708 ↗
28. Nanoporous gold prism microassembly through a self-organizing route10.1021/nl0602443 ↗
29. On the electrochemical dealloying of Al-based alloys in a NaCl aqueous solution10.1039/B919313H ↗
30. The function of the repassivation process in the inhibition of pitting corrosion on aluminum10.1016/0010-938X(80)90098-0 ↗