journal article·2019-01

De-bondable SiC SiC wafer bonding via an intermediate Ni nano-film

Fengwen Mu, Miyuki Uomoto, Takehito Shimatsu, Yinghui Wang, Kenichi Iguchi, Haruo Nakazawa, Yoshikazu Takahashi, Eiji Higurashi, Tadatomo Suga

Publisher page

Abstract

Abstract In this study, a de-bondable wafer bonding method for silicon carbide (SiC) that can sustain rapid thermal annealing (RTA) at ∼1273 K has been realized. Two SiC wafers were bonded via an intermediate nickel (Ni) nano-film at room temperature without any pressure, which was characterized as a seamless and robust bonding. After the RTA process, the strength of the bonding interface was dramatically decreased and the de-bonding could happen at the interface during pulling test. Both of the mechanisms of bonding and de-bonding have been investigated through interface analyses. The sufficient atomic diffusion between two deposited Ni nano-films together with the interfacial mixing between amorphous SiC and the Ni nano-film contribute to the strong bonding of SiC SiC. The interfacial precipitation of layered carbon material parallel to the SiC substrates is assumed to be the reason of the interface weakening and de-bonding after annealing. It is believed that the further development of this bonding and de-bonding technology will advance thin SiC device fabrication, where the RTA process at ∼1273 K is widely used.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: 3D IC and TSV technologies · Silicon Carbide Semiconductor Technologies · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Kimoto · 2014
2. Rectifying electrical contacts to n-type 6H–SiC formed from energetically deposited carbon10.1016/j.carbon.2016.02.038 ↗
3. Effects of thermal annealing process on the electrical properties of p+-Si/n-SiC heterojunctions10.1063/1.4873113 ↗
4. Single-crystalline 3C-SiC anodically bonded onto glass: an excellent platform for high-temperature electronics and bioapplications10.1021/acsami.7b06661 ↗
5. Advances in silicon carbide science and technology at the micro-and nanoscales10.1116/1.4807902 ↗
6. A roadmap for future wide bandgap semiconductor power electronics10.1557/mrs.2015.97 ↗
7. 4H-SiC piezoresistive pressure sensors at 800°C with observed sensitivity recovery10.1109/LED.2014.2379262 ↗
8. Wijesundara · 2011
9. Photoelectrochemical etching to fabricate single-crystal SiC MEMS for harsh environments10.1016/j.matlet.2010.10.034 ↗
10. Anodic etching of SiC in alkaline solutions10.1088/0960-1317/17/4/S04 ↗
11. Kuchuk · Adv. Cond. Matter Phys. · 2016 · 2016 · 9273702
12. Wafer direct bonding: from advanced substrate engineering to future applications in micro/nanoelectronics10.1109/JPROC.2006.886026 ↗
13. Plasmonic-radiation-enhanced metal oxide nanowire heterojunctions for controllable multilevel memory10.1002/adfm.201601143 ↗
14. Surface activated bonding of silicon wafers at room temperature10.1063/1.115865 ↗
15. Direct wafer bonding of SiC-SiC by SAB for monolithic integration of SiC MEMS and electronics10.1149/2.0011609jss ↗
16. J. Hermanowski, Thin wafer handling-study of temporary wafer bonding materials and processes, in: IEEE Int. Conf. on 3D Syst. Integr. (3DIC), San Francisco, California. USA, 2009, pp. 1–5.10.1109/3DIC.2009.5306550 ↗
17. B. Dang, B. Webb, C. Tsang, P. Andry, J. Knickerbocker, Factors in the selection of temporary wafer handlers for 3D/2.5 D integration, in: 64th Electron. Compon. Technol. Conf. Orlando, Florida, USA, 2014, pp. 576–581.10.1109/ECTC.2014.6897343 ↗
18. UV-curing and thermal stability of dual curable urethane epoxy adhesives for temporary bonding in 3D multi-chip package process10.1016/j.ijadhadh.2013.02.005 ↗
19. Silicon carbide wafer bonding by modified surface activated bonding method10.7567/JJAP.54.030214 ↗
20. Room-temperature wafer bonding of SiC–Si by modified surface activated bonding with sputtered Si nanolayer10.7567/JJAP.55.04EC09 ↗
21. Surface activated bonding of GaAs and SiC wafers at room temperature for improved heat dissipation in high-power semiconductor lasers10.7567/JJAP.54.030207 ↗
22. Influence of relative wafer rotation on the electrical properties of the bonded SiC/SiC interface10.1063/1.1753065 ↗
23. Properties of a SiC Schottky barrier diode fabricated with a thin substrate
24. Performance of a 650V SiC diode with reduced chip thickness10.4028/www.scientific.net/MSF.717-720.921 ↗
25. Surface chemistry of Ni induced graphite formation on the 6H–SiC (0 0 0 1) surface and its implications for graphene synthesis10.1016/j.carbon.2010.02.007 ↗
26. Synthesis of graphene on silicon carbide substrates at low temperature10.1016/j.carbon.2009.03.051 ↗
27. Synthesis of graphene on silicon dioxide by a solid carbon source10.1021/nl902558x ↗
28. Local solid phase growth of few-layer graphene on silicon carbide from nickel silicide supersaturated with carbon10.1063/1.4795501 ↗
29. Oriented growth of silicide and carbon in SiC-based sandwich structures with nickel10.1016/j.matchemphys.2008.02.009 ↗
30. Cold welding of Ag nanowires by large plastic deformation10.1016/j.scriptamat.2015.12.010 ↗
31. Atomic diffusion bonding of wafers with thin nanocrystalline metal films10.1116/1.3437515 ↗
32. Room temperature bonding of wafers with thin nanocrystalline metal films10.1149/1.3483494 ↗
33. Room Temperature Bonding Using Thin Metal Films (Bonding Energy and Technical Potential)10.1149/06405.0317ecst ↗