Laser conditioning of ZrO2:Y2O3/SiO2 mirror coatings prepared by E-beam evaporation
Source abstract
Abstract
Laser conditioning effects of the dielectric mirror coatings with different designs were investigated. Simple quarter-wave ZrO2:Y2O3/SiO2 mirrors and half-wave SiO2 over-coated ZrO2:Y2O3/SiO2 mirror coatings were fabricated by E-beam evaporation (EBE). The absorbance of the samples before and after laser conditioning was measured by surface thermal lensing (STL) technology and the defects density was detected under Nomarski microscope. The enhancement of the laser damage resistance was found after laser conditioning. The dependence of the laser conditioning on the coating design was also observed and the over-coated sample obtained greatest enhancement, whereas the absorbance of the samples did not change obviously. During the sub-threshold fluence raster scanning, the minor damage about defects size was found and the assumption of pre-damage mechanism, based on the functional damage concept, was put forward. The improvement of the laser induced damage threshold (LIDT) was attributed to the benign damage of the defects and the dependence on the coating design owed to the damage growth behavior of different coating designs. (C) 2004 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Solid State Laser Technologies · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Laser conditioning of LaF3/MgF2 dielectric coatings at 248 nm10.1364/AO.35.005613 ↗
2. Laser conditioning of optical thin films
3. Large-area conditioning of dielectric thin film mirrors
4. Temporary laser damage threshold enhancement by laser conditioning of antireflection-coated glass10.1063/1.98407 ↗
5. What is laser conditioning? A review focused on dielectric multilayers
6. Measuring weak absorptance of thin film coatings by surface thermal lensing technique
7. ISO 11254-1:2000, Lasers and laser-related equipment—determination of laser-induced damage threshold of optical surfaces. Part 1: 1-on-1 test.
8. Laser-induced damage threshold and certification procedure for optical materials”, NASA Reference Publication 1395, June 1997.
9. Large area conditioning of optics for high-power laser systems10.1117/12.180939 ↗
10. Towards predicting the laser damage threshold of larger-area optics10.1117/12.274250 ↗
11. Growth of laser-induced damage during repetitive illumination of HfO2–SiO2 multilayer mirror and polarizer coatings10.1117/12.274244 ↗
12. Influence of defect shape on laser-induced damage in multilayer coatings10.1117/12.192151 ↗