Abstract
To improve the anterior surface biocompatibility of hydrophobic acrylic intraocular lens (IOL) in a convenient and continuous way, poly(ethylene glycol)s (PEGs) were immobilized by atmospheric pressure glow discharge (APGD) treatment using argon as the discharge gas. The hydrophilicity and chemical changes on the IOL surface were characterized by static water contact angle and X-ray photoelectron spectroscopy to confirm the covalent binding of PEG. The morphology of the IOL surface was observed under field emission scanning electron microscopy and atomic force microscopy. The surface biocompatibility was evaluated by adhesion experiments with platelets, macrophages, and lens epithelial cells (LECs) in vitro. The results revealed that the anterior surface of the PEG-grafted IOL displayed significantly and permanently improved hydrophilicity. Cell repellency was observed, especially in the PEG-modified IOL group, which resisted the attachment of platelets, macrophages and LECs. Moreover, the spread and growth of cells were suppressed, which may be attributed to the steric stabilization force and chain mobility effect of the modified PEG. All of these results indicated that hydrophobic acrylic IOLs can be hydrophilic modified by PEG through APGD treatment in a convenient and continuous manner which will provide advantages for further industrial applications. (C) 2010 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intraocular Surgery and Lenses · Ocular Surface and Contact Lens · Retinal and Macular Surgery
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Biocompatibility of intraocular lens materials10.1097/ICU.0b013e3282f20132 ↗
2. ASCRS white paper: hydrophobic acrylic intraocular lenses in children10.1016/j.jcrs.2007.06.047 ↗
3. Practice styles and preferences of ASCRS members—2003 survey10.1016/j.jcrs.2004.02.064 ↗
4. Pediatric cataract surgery and intraocular lens implantation—practice styles and preferences of the 2001 ASCRS and AAPOS memberships10.1016/S0886-3350(03)00220-7 ↗
5. Uveal and capsular biocompatibility of hydrophilic acrylic, hydrophobic acrylic, and silicone intraocular lenses10.1016/S0886-3350(01)01122-1 ↗
6. Uveal and capsular biocompatibility of two foldable acrylic intraocular lenses in patients with endogenous uveitis—a prospective randomized study10.1007/s00417-008-0886-4 ↗
7. Inflammation after implantation of hydrophilic acrylic, hydrophobic acrylic, or silicone intraocular lenses in eyes with cataract and uveitis: comparison to a control group10.1016/S0886-3350(02)01321-4 ↗
8. Improvement of the surface biocompatibility of silicone intraocular lens by the plasma-induced tethering of phospholipid moieties10.1002/jbm.a.30741 ↗
9. Uveal and capsular biocompatibility of an intraocular lens with hydrophilic anterior and hydrophobic posterior surfaces10.1016/j.jcrs.2009.09.027 ↗
10. Impact of anterior capsule polishing on anterior capsule opacification after cataract surgery: a randomized clinical trial10.1038/eye.2008.355 ↗
11. Effect of anterior capsule polishing on fibrotic capsule opacification: three-year results
12. Drug delivery systems for the eye10.1586/erd.09.4 ↗
13. Effect on posterior capsule opacification of topical diclofenac sodium vs dexamethasone phosphate after cataract surgery10.1007/s12009-002-0044-2 ↗
14. Improved performances of intraocular lenses by poly(ethylene glycol) chemical coatings10.1021/bm0701649 ↗
15. Tethering poly(ethylene glycol)s to improve the surface biocompatibility of poly(acrylonitrile-co-maleic acid) asymmetric membranes10.1016/j.biomaterials.2004.03.008 ↗
16. Surface modification of polymethyl methacrylate intraocular lenses by plasma for improvement of antithrombogenicity and transmittance10.1016/j.apsusc.2009.03.029 ↗
17. Modification of the surface properties of a lens material to influence posterior capsular opacification10.1111/j.1442-9071.2006.01278.x ↗
18. Suppression of fibroblast and bacterial adhesion by MPC coating on acrylic intraocular lenses10.1016/j.jcrs.2006.02.010 ↗
19. Active oxygen processing for acrylic intraocular lenses to prevent posterior capsule opacification10.1016/j.jcrs.2006.02.042 ↗
20. A study of atmospheric pressure plasma discharges for surface functionalization of PTFE used in biomedical applications10.1088/0022-3727/39/16/S03 ↗
21. Comparison of atmospheric-pressure plasma versus low-pressure RF plasma for surface functionalization of PTFE for biomedical applications, plasma process
22. The surface oxidation of selected polymers using an atmospheric pressure air dielectric barrier discharge. Part I10.1016/S0169-4332(03)00879-1 ↗
23. The surface oxidation of selected polymers using an atmospheric pressure air dielectric barrier discharge. Part II10.1016/j.apsusc.2003.10.002 ↗
24. Surface modification of poly(epsilon-caprolactone) using a dielectric barrier discharge in atmospheric pressure glow discharge mode10.1016/j.actbio.2009.01.042 ↗
25. Acrylonitrile-based copolymer membranes containing reactive groups: effects of surface-immobilized poly(ethylene glycol)s on anti-fouling properties and blood compatibility10.1016/j.polymer.2003.11.007 ↗
26. Aging and annealing behavior of polycarbonate surfaces modified by direct-current glow discharge in air10.1002/app.29441 ↗
27. Studies on surface graft polymerization of acrylic acid onto PTFE film by remote argon plasma initiation10.1016/j.apsusc.2006.10.014 ↗
28. Short-time plasma surface modification of HDPE powder in a Plasma Downer Reactor—process, wettability improvement and ageing effects10.1016/j.apsusc.2005.02.099 ↗
29. Characterization of the surface changes and the aging effects of low-pressure nitrogen plasma treatment in a polyurethane film10.1016/j.polymertesting.2007.09.002 ↗
30. Polyethylene glycol-coated biocompatible surfaces10.1002/1097-4636(20000905)51:3<343::AID-JBM7>3.0.CO;2-D ↗
31. XPS and AFM analysis of antifouling PEG interfaces for microfabricated silicon biosensors10.1016/j.bios.2004.01.034 ↗
32. Cell adhesion to acrylic intraocular lens associated with lens surface properties10.1016/j.jcrs.2004.11.050 ↗
33. Synthesis and surface morphology of high-density poly(ethylene glycol) grafted layers10.1021/la034974r ↗
34. Surface modification of acrylate intraocular lenses with dielectric barrier discharge plasma at atmospheric pressure10.1007/s11426-009-0048-5 ↗
35. Comparison of anterior capsule contraction between 5 foldable intraocular lens models10.1016/j.jcrs.2008.04.039 ↗
36. Superior in vitro biological response and mechanical properties of an implantable nanostructured biomaterial: nanohydroxyapatite–silicone rubber composite10.1016/j.actbio.2009.04.029 ↗
37. Surface graft polymerization of poly(ethylene glycol) methacrylate onto polyurethane via thiol-ene reaction: preparation and characterizations10.1163/092050609X12457419024109 ↗
38. Influence of PEG architecture on protein adsorption and conformation10.1021/la051726h ↗
39. Results of hydrophilic acrylic, hydrophobic acrylic, and silicone intraocular lenses in uveitic eyes with cataract: comparison to a control group10.1016/S0886-3350(02)01425-6 ↗
40. Cellular reaction on the anterior surface of 4 types of intraocular lenses10.1016/S0886-3350(01)00846-X ↗
41. Effect of the hydrophilicity of acrylic intraocular lens material and haptic angulation on anterior capsule opacification10.1136/bjo.2006.103390 ↗
42. Lens epithelial cell ongrowth: comparison of 6 types of hydrophilic intraocular lens models10.1016/j.jcrs.2005.05.030 ↗