journal article·2016-12

Improved wear resistance by phase transformation of surface nanocrystalline 1090 steel prepared by sandblasting technique

Rong Peng, Licai Fu, Lingping Zhou

Publisher page

Abstract

Abstract A surface nanocrystalline 1090 steel has been fabricated by using sandblasting technique. The surface average grain size was about 78 nm. The high strain rate and strain in sandblasting were main reasons for surface nanocrystallization. The wear resistance of 1090 steel was considerably enhanced as grain size decreased. The microstructure and hardness of contact zones before and after wear tests have been examined by XRD, SEM and TEM. Except the higher hardness, the results demonstrated that parts of ferrite transferred to cementite and martensite. It was additional beneficial for improving the wear resistance of 1090 steel as the grain size decreased.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Metal and Thin Film Mechanics · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Koch · 2007
2. Fabrication of bulk nanostructured materials from metallic nanopowders: structure and mechanical behaviour10.1016/S1359-6462(01)00782-5 ↗
3. ynthesis and characterization of electrodeposited nanocrystalline nickel–iron alloys10.1016/S0921-5093(02)00586-5 ↗
4. Nanocrystalline metals crystallized from amorphous solids: nanocrystallization, structure, and properties10.1016/0927-796X(95)00187-5 ↗
5. Microstructural evolution and mechanical properties of a two-phase Cu–Ag alloy processed by high-pressure torsion to ultrahigh strains10.1016/j.actamat.2011.01.017 ↗
6. Production of alloyed nanocrystalline surfaces by combined punching, sandblasting and recovery treatments10.1016/j.scriptamat.2008.02.007 ↗
7. Dry sliding wear behavior of cold sprayed aluminum amorphous/nanocrystalline alloy coatings10.1016/j.surfcoat.2013.10.055 ↗
8. Sliding wear behaviour of nanocrystalline Fe88Si12 alloy under low load and speed10.1007/s11249-012-0028-3 ↗
9. Cavitation erosion of stainless steels10.1016/0043-1648(82)90278-2 ↗
10. The effects of additive elements on the sliding wear behavior of Fe-base hardfacing alloys10.1016/S0043-1648(03)00155-8 ↗
11. Some metallurgical aspects of chips formed in high speed machining of high strength low alloy steel10.1016/j.scriptamat.2005.01.031 ↗
12. The formation of martensite during wear of AISI 304 stainless steel10.1016/j.wear.2007.01.107 ↗
13. Deformation structures induced by sliding contact10.1080/01418619208201580 ↗
14. Enhancing wear resistance of Cu–Al alloy by controlling subsurface dynamic recrystallization10.1016/j.scriptamat.2015.01.023 ↗
15. Surface damage resulting from rolling contact operating in magnetic field10.1088/0022-3727/40/24/006 ↗
16. Czichos · 1978
17. The mechanism of formation of nanostructure and dissolution of cementite in a pearlitic steel during high pressure torsion10.1016/S1359-6454(03)00419-1 ↗
18. Formation of nanostructured surface layer on 304 stainless steel by means of surface mechanical attrition treatment10.1016/S1359-6454(02)00594-3 ↗
19. Nanocrystallization induced by quasi-static fracture of metallic glasses at room temperature10.1080/09500830802438115 ↗
20. A new method for the measurement of the diffusivity of carbon in alpha-iron using an electrochemical cell10.1007/BF00648633 ↗
21. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
22. XRD analysis of carbide phase in heat resistant steels
23. Martensite and its reverse transformation in nanocrystalline bulk Co10.1016/j.msea.2006.02.191 ↗
24. Dependence of martensite start temperature on fine austenite grain size10.1016/j.scriptamat.2007.09.017 ↗
25. Temperature maps for frictional heating in dry sliding10.1080/10402009108982074 ↗
26. On the correlation between wear and entropy in dry sliding contact10.1016/j.wear.2011.01.034 ↗
27. Comparison of different theoretical models for flash temperature calculation under fretting conditions10.1016/S0301-679X(01)00083-4 ↗
28. Wear resistance of amorphous alloys and related materials10.1179/095066001225001067 ↗
29. Sliding wear of nanocrystalline Ni–W: structural evolution and the apparent breakdown of Archard scaling10.1016/j.actamat.2010.04.005 ↗