Abstract In this paper, neodymium-based conversion coating is used as a substitute for toxic chromate conversion coating on AZ91D magnesium alloys. Its formation and growth were observed via SEM, EDS, XPS, electrochemical tests and weighting experiment. The influence of post-treatment on neodymium conversion coating was measured by FTIR and electrochemical experiments in terms of morphology, component, surface functional group and corrosion resistance. The dissolution of matrix and the deposition of neodymium/magnesium oxides compete with each other in initial time. Then the deposition of neodymium oxides dominates the process. Compact coating is obtained after 20 min immersion and it is mainly made of neodymium oxides and a small amount of magnesium oxides/hydroxides. The coating post-treated is rich in OH− and PO43+. The post-treatment can improve the corrosion resistance of the neodymium conversion coating effectually examined by EIS.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Metallurgy and Material Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Conversion coating growth on 2024-T3 Al alloy. The effect of pre-treatments10.1016/j.surfcoat.2007.12.017 ↗
2. Investigation of the formation of the cerium-based conversion coating on 2024-T3 aluminium alloy
3. Growth of permanganate conversion coating on 2024-Al alloy10.1016/j.tsf.2007.04.164 ↗
4. Response of nanocrystalline cerium-based conversion coatings on Al 2024-T3 to chloride environments10.1016/j.matlet.2006.12.062 ↗
5. Effects of acid and alkaline based surface preparations on spray deposited cerium based conversion coatings on Al 2024-T310.1016/j.apsusc.2008.10.110 ↗
6. CeO2-filled sol–gel coatings for corrosion protection of AA2024-T3 aluminium alloy10.1016/j.corsci.2009.06.007 ↗
7. Cerium-based chemical conversion coating on AZ63 magnesium alloy10.1016/S0257-8972(03)00336-0 ↗
8. Characterization of rare-earth conversion films formed on the AZ31 magnesium alloy and its relation with corrosion protection10.1016/j.apsusc.2007.02.019 ↗
9. Cerium conversion coatings for AZ91D magnesium alloy in ethanol solution and its corrosion resistance10.1016/j.corsci.2009.08.003 ↗
10. Improvement of corrosion resistance of magnesium metal by rare earth elements10.1016/j.electacta.2007.03.027 ↗
11. Corrosion protection of magnesium alloys by cerium, zirconium and niobium-based conversion coatings10.1016/j.corsci.2008.03.015 ↗
12. Composition and corrosion behaviour of galvanised steel treated with rare-earth salts: the effect of the cation10.1016/S0300-9440(01)00250-8 ↗
13. Treatment of zinc surface with cerium (III) nitrate to prevent zinc corrosion in aerated 0.5M NaCl10.1016/S0010-938X(00)00189-X ↗
14. Toxicity and carcinogenicity of chromium compounds in humans10.1080/10408440500534032 ↗
15. Chronic toxicity and carcinogenicity studies of chromium picolinate monohydrate administered in feed to F344/N rats and B6C3F1 mice for 2 years10.1016/j.fct.2009.01.006 ↗
16. Evaluation of the potential genotoxicity of chromium picolinate in mammalian cells in vivo and in vitro10.1016/j.fct.2006.11.008 ↗
17. The nutritional supplement chromium picolinate generates oxidative DNA damage and peroxidized lipids in vivo10.1016/S0277-5387(02)01369-4 ↗
18. JNdi-1: a neodymium isotopic reference in consistency with LaJolla neodymium10.1016/S0009-2541(00)00198-4 ↗
19. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗