Abstract

Abstract Laser alloying was carried out on the surface of pure titanium substrate with TiN–B–Si–Ni mixed powders. The result of X-ray diffraction (XRD) analysis shows that the alloyed layer consists of many kinds of intermetallic compounds. The test results show that the alloyed layers have high microhardness (1500–1600 HV0.1), low friction coefficient (about 0.4), and are more resistant to oxidation than untreated substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · Surface Treatment and Coatings · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Protection of titanium alloy components against high temperature corrosion10.1016/S0921-5093(03)00150-3 ↗
2. Microstructure and wear resistance of CP titanium laser alloyed with a mixture of reactive gases10.1016/S0043-1648(97)00043-4 ↗
3. Laser treatment and PVD TiN coating of Ti–6Al–4V alloy10.1016/S0257-8972(00)00715-5 ↗
4. Laser boronizing of some titanium alloys10.1016/0169-4332(92)90074-8 ↗
5. Wear resistance of laser clad Ti2Ni3Si reinforced intermetallic composite coatings on titanium alloy10.1016/j.apsusc.2004.01.045 ↗
6. NiTi cladding on stainless steel by TIG surfacing process: Part II: corrosion behavior10.1016/S0257-8972(03)00346-3 ↗
7. In situ processing of Al–TiB2 composite by the stir-casting technique10.1016/S0924-0136(99)00038-2 ↗
8. Laser boronising of Ti–6Al–4V as a result of laser alloying with pre-placed BN10.1016/S0921-5093(98)00964-2 ↗