Abstract

Abstract The influence of different variables (stirring, degreasing, oxidant additions, pH, Ce concentration, anion type, time and temperature of immersion) on the optimization of Ce conversion and electrolysis coatings on both A3xx.x alloys and aluminium metal matrix composites A3xx.x/SiCp was evaluated in 3.5 wt% NaCl at 22 °C using potentiodynamic polarization. Ce treated surfaces presented better corrosion behaviour in chloride media than original material surfaces without treatment. Both treatments preferentially covered the intermetallic compounds and SiCp. The electrolysis afforded a higher degree of protection than conversion treatment because the coating was more extensive. Coating microstructure was analysed by scanning electron microscopy (SEM), atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Hinton · Mater. Forum · 1986 · 9 · 162
2. Reduction of Hazardous Substances (RoHS) Directive (2002/95/EC), Official Journal of the European Union, January 27, L37/19, 2003.
3. Haley · J. Pharm. Sci. · 1965 · 54 · 63310.1002/jps.2600540431 ↗
4. Hedrick · J. Alloys Compd. · 1997 · 250 · 47110.1016/S0925-8388(96)02532-7 ↗
5. Rivera · Surf. Coat. Technol. · 2004 · 176 · 34910.1016/S0257-8972(03)00742-4 ↗
6. Creus · Surf. Coat. Tech. · 2006 · 200 · 463610.1016/j.surfcoat.2005.04.027 ↗
7. Davenport · Corros. Sci. · 1991 · 32 · 65310.1016/0010-938X(91)90113-4 ↗
8. Ferreira · Electrochim. Acta · 2004 · 49 · 292710.1016/j.electacta.2004.01.051 ↗
9. Arenas · Surf. Coat. Technol. · 2004 · 187 · 32010.1016/j.surfcoat.2004.02.033 ↗
10. Gray · J. Alloys Compd. · 2002 · 336 · 8810.1016/S0925-8388(01)01899-0 ↗
11. Aramaki · Corros. Sci. · 2005 · 47 · 128510.1016/j.corsci.2004.05.022 ↗
12. Presuel-Moreno · J. Electrochem. Soc. · 2005 · 152 · B37610.1149/1.1997165 ↗
13. Bethencourt · Corros. Sci. · 1998 · 40 · 180310.1016/S0010-938X(98)00077-8 ↗
14. Johnson · Mater. Sci. Eng. A · 2003 · 361 · 22510.1016/S0921-5093(03)00516-1 ↗
15. Hinton · Mater. Perform. · 1987 · 42 · 47
16. Mansfeld · Corros. Sci. · 1987 · 27 · 99710.1016/0010-938X(87)90065-5 ↗
17. L. Wilson, B.R.W. Hinton, Patent WO 1988. 88/06639.
18. Bethencourt · Appl. Surf. Sci. · 2004 · 238 · 27810.1016/j.apsusc.2004.05.268 ↗
19. Zhang · Rare Metals · 2002 · 21 · 95
20. Kendig · Corros. Sci. · 1993 · 34 · 4110.1016/0010-938X(93)90257-H ↗
21. Mansfeld · Electrochim. Acta · 1989 · 34 · 112310.1016/0013-4686(89)87145-2 ↗
22. Dabalà · Appl. Surf. Sci. · 2001 · 172 · 31210.1016/S0169-4332(00)00873-4 ↗
23. Bethencourt · Appl. Surf. Sci. · 2002 · 189 · 16210.1016/S0169-4332(02)00129-0 ↗
24. Gorman · Corros. Sci. · 2003 · 45 · 110310.1016/S0010-938X(02)00209-3 ↗
25. Neil · Corrosion · 1994 · 50 · 21510.5006/1.3293513 ↗
26. Decroly · Surf. Coat. Technol. · 2005 · 194 · 110.1016/j.surfcoat.2004.05.012 ↗
27. Campestrini · Surf. Coat. Technol. · 2004 · 176 · 36510.1016/S0257-8972(03)00743-6 ↗
28. Wang · Corrosion · 2004 · 60 · 23710.5006/1.3287726 ↗
29. Mansfeld · J. Electrochem. Soc. · 1991 · 138 · L7410.1149/1.2085513 ↗
30. Johnson · Mater. Charact. · 2005 · 54 · 4110.1016/j.matchar.2004.10.006 ↗
31. Turnbull · Br. Corros. J. · 1992 · 27 · 2710.1179/000705992798268864 ↗
32. Metzger · Ind. Eng. Chem. Prod. Res. · 1983 · 22 · 29610.1021/i300010a026 ↗
33. Lin · Corros. Sci. · 1992 · 33 · 133110.1016/0010-938X(92)90176-4 ↗
34. Chen · Corros. Sci. · 1997 · 39 · 107510.1016/S0010-938X(97)00008-5 ↗
35. Hamdy · Corr. Prev. Control · 2001 · 48 · 101
36. Hamdy · Surf. Interface Anal. · 2002 · 34 · 17110.1002/sia.1276 ↗
37. Hamdy · Surf. Coat. Tech. · 2006 · 200 · 378610.1016/j.surfcoat.2005.03.012 ↗
38. Hamdy · J. Appl. Electrochem. · 2005 · 35 · 47310.1007/s10800-004-8330-x ↗
39. Hughes · Surf. Interface Anal. · 1995 · 23 · 54010.1002/sia.740230714 ↗
40. Hinton · 2002
41. Corrosion of aluminum and aluminum alloys
42. Pourbaix · 1974
43. Cotton · 1972
44. B.R.W. Hinton, Review on Corrosion Inhibitor Science and Technology, in: A. Raman, P. Labine (eds.), Corrosion/89 Symposium, Nace, Paper I–11, p. 1.
45. Adam · 2002
46. L. Wilson, B.R.W. Hinton, A Method of Forming a Corrosion Resistant Coating, Patent WO 88/06639, 1988.
47. Johnson · Mater. Charact. · 2005 · 54 · 4110.1016/j.matchar.2004.10.006 ↗
48. Yu · J. Alloys Compd. · 2004 · 364 · 19310.1016/S0925-8388(03)00502-4 ↗
49. H. Zhou, Characterization of Conversion Coating on 7075-T6 Al Alloy, M.S. Thesis, University of Missouri, Rolla, 2001.
50. Dabala · Appl. Surf. Sci. · 2001 · 172 · 31210.1016/S0169-4332(00)00873-4 ↗
51. Wan · J. de Physique IV · 1997 · 7 · 1183
52. Aldykiewicz · J. Electrochem. Soc. · 1996 · 143 · 14710.1149/1.1836400 ↗
53. Fahrenholtz · Surf. Coat. Technol. · 2002 · 155 · 20810.1016/S0257-8972(02)00062-2 ↗
54. Pardo · Corros. Sci. · 2005 · 47 · 175010.1016/j.corsci.2004.08.010 ↗
55. Yu · Corros. Sci. · 2001 · 43 · 128310.1016/S0010-938X(00)00141-4 ↗
56. Pardo · Corrosion · 2005 · 62 · 14110.5006/1.3278259 ↗
57. Pardo · Surf. Coat. Technol. · 2005 · 200 · 293810.1016/j.surfcoat.2005.05.028 ↗
58. Pardo · Appl. Surf. Sci. · 2005 · 252 · 279410.1016/j.apsusc.2005.04.023 ↗
59. Hihara · Int. Mater. Rev. · 1994 · 39 · 24510.1179/095066094790151026 ↗
60. Hughes · Mater. Sci. Technol. · 1999 · 15 · 112410.1179/026708399101505167 ↗
61. Wang · Corros. Sci. · 2004 · 46 · 7510.1016/S0010-938X(03)00135-5 ↗
62. ASTM D3359-02, Standard Test Methods for Measuring Adhesion by Tape Test, vol. 6.01, ASTM International, 2002.