journal article·2006-12

Study of corrosion–erosion behaviour of stainless alloys in industrial phosphoric acid medium

Abdellah Guenbour, Mohamed-Adil Hajji, El Miloudi Jallouli, Ali Ben Bachir

Applied Surface Science· Volume 253· Issue 5
Publisher page

Abstract

The corrosion and corrosion-abrasion resistance of some stainless steels in industrial phosphoric acid 30% P2O5 has been studied using electrochemical techniques. The corrosion rate of materials increases with the increase of temperature. Alloys which contain chromium, molybdenum and nitrogen in sufficient quantities present the best behaviour. In the abrasion-corrosion conditions, the experimental device set up allowed to follow continually samples electrochemical behaviour. Under dynamic conditions and without solid particles, the increase of acid projection speed has no effect on the alloys corrosion behaviour. The adding of abrasive leads to a general increase of corrosion rate and to a decrease of material resistance. Under these conditions, materials attack is controlled by synergistic effect between the abrasion and the impurities. The cast 30% Cr shows good resistance according to his high chromium content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. M.A. Hajji, Thèse de Doctorat, Fac. Sci. Rabat, 1996.
2. Jallouli · 1994 · 9.1
3. Bellaouchou · Corros. Nace · 1993 · 49 · 65610.5006/1.3316097 ↗
4. Hajjaji · Br. Corros. J. · 1993 · 28 · 20110.1179/000705993798318498 ↗
5. Bui · Ann. Chim. · 1983 · 8 · 411
6. Idrissi · J. Mater. Sci. · 1996 · 31 · 49910.1007/BF00366357 ↗
7. Hajji · Ann. Chim. Sci. Mater. · 2002 · 274 · 2710.1016/S0151-9107(02)80016-2 ↗
8. Guenbour · Br. Corros. J. · 1988 · 23 · 23410.1179/000705988798270631 ↗
9. White · Corros. Nace · 1996 · 433
10. Benhardson · Inform. Chim. · 1978 · 176 · 125
11. Charles · Mater. Technol. · 1987 · 8 · 30910.1051/mattech/198775070309 ↗
12. Sedrik · Corros. Nace · 1986 · 42 · 37610.5006/1.3584918 ↗
13. Nassif · Surf. Technol. · 1985 · 26 · 18910.1016/0376-4583(85)90115-3 ↗
14. Guenbour · Corrosion · 1990 · 30 · 213
15. Guenbour · Corros. Nace · 1988 · 44 · 21410.5006/1.3583928 ↗
16. Bems · Mater. Sci. For. · 1999 · 318–320 · 517
17. Gunpel · 1988 · 272
18. Haminen · Mater. Sci. For. · 1999 · 318–320 · 479
19. Toroa · 2002
20. Toro · 2001
21. Neville · Br. Corros. J. · 1997 · 32 · 19710.1179/bcj.1997.32.3.197 ↗