journal article·2023-09

Mitigation of metal whisker growth from MAX phases by A-site alloying strategy

Yushuang Liu, Chengjie Lu, Yue Chen, Miaoyan Huang, Ying Liu, Ru Wang, Hanyu Yao, ZhengMing Sun

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Ferroelectric and Negative Capacitance Devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. The MN+1AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Barsoum · 2013
3. On the chemical diversity of the MAX phases10.1016/j.trechm.2019.02.016 ↗
4. Extrusion-based additive manufacturing of Ti3SiC2 and Cr2AlC MAX phases as candidates for high temperature heat exchangers10.1016/j.jeurceramsoc.2021.10.042 ↗
5. Ti3AlC2, a candidate structural material for innovative nuclear energy system: the microstructure phase transformation and defect evolution induced by energetic heavy-ion irradiation10.1016/j.actamat.2020.03.008 ↗
6. Electrochemical interaction of Sn-containing MAX phase (Nb2SnC) with Li-Ions10.1021/acsenergylett.9b01580 ↗
7. Anisotropic arc erosion resistance of Ag/Ti3AlC2 composites induced by the alignment of Ti3AlC210.1016/j.corsci.2020.108633 ↗
8. MAX phases: bridging the gap between metals and ceramics
9. Studying the oxidation of Ti2AlC MAX phase in atmosphere: a review10.1016/j.ijrmhm.2016.07.006 ↗
10. Reducing the self-healing temperature of Ti2AlC MAX phase coating by substituting Al with Sn10.1016/j.jeurceramsoc.2019.09.009 ↗
11. Oxidation resistance of Ti3AlC2 and Ti3Al0.8Sn0.2C2 MAX phases: a comparison
12. Two-dimensional nanocrystals produced by exfoliation of Ti3AlC210.1002/adma.201102306 ↗
13. Synthesis of Ti3AuC2, Ti3Au2C2 and Ti3IrC2 by noble metal substitution reaction in Ti3SiC2 for high-temperature-stable Ohmic contacts to SiC10.1038/nmat4896 ↗
14. Element replacement approach by reaction with lewis acidic molten salts to synthesize nanolaminated MAX phases and MXenes10.1021/jacs.9b00574 ↗
15. Room-temperature deintercalation and self-extrusion of Ga from Cr2GaN10.1126/science.284.5416.937 ↗
16. Growing metallic whiskers: alternative interpretation10.1126/science.285.5432.1355i ↗
17. Mechanisms behind the spontaneous growth of Tin whiskers on the Ti2SnC ceramics10.1016/j.actamat.2019.12.027 ↗
18. Isotope study reveals atomic motion mechanism for the formation of metal whiskers in MAX phase10.1016/j.actamat.2020.11.017 ↗
19. Driving force and mechanism for spontaneous metal whisker formation10.1103/PhysRevLett.93.206104 ↗
20. Controllable growth of Ga wires from Cr2GaC-Ga and its mechanism10.1016/j.physb.2015.07.005 ↗
21. Mechanism and mitigation of spontaneous Ga whisker growth on Cr2GaC10.1007/s11431-018-9442-9 ↗
22. Method for inhibiting Sn whisker growth on Ti2SnC10.1007/s10853-022-07867-5 ↗
23. The effect of chemical disorder on defect formation and migration in disordered max phases10.1016/j.actamat.2019.11.033 ↗
24. Isothermal oxidation of Ti3Al0.6Ga0.4C2 MAX phase solid solution in air at 1000 degrees C to 1300 degrees C10.1149/1945-7111/ac58c1 ↗
25. Tailoring MAX phase magnetic property based on M-site and A-site double solid solution10.15541/jim20210126 ↗
26. Ti2Al(C, N) solid solution reinforcing TiAl-based composites: evolution of a core-shell structure, interfaces, and mechanical properties10.1021/acsami.8b02023 ↗
27. Spontaneous whisker growth on lead-free solder finishes10.1016/j.msea.2005.06.074 ↗
28. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
29. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
30. Ab initio modeling of the formation and migration of monovacancies in Ti2AlC10.1016/j.scriptamat.2008.06.044 ↗
31. Room temperature mushrooming of gallium wires and its growth mechanism10.1016/j.jallcom.2014.09.082 ↗
32. Interface energy-driven indium whisker growth on ceramic substrates10.1007/s10854-021-06250-5 ↗
33. Precipitation induced crack healing in a Ti2SnC ceramic in vacuum10.1016/j.ceramint.2017.02.120 ↗
34. Low-temperature instability of Ti2SnC: a combined transmission electron microscopy, differential scanning calorimetry, and x-ray diffraction investigations10.1557/JMR.2009.0012 ↗
35. Spontaneous Sn whisker formation on Ti2SnC10.1007/s10854-016-6249-8 ↗
36. G.W. Bentzel, M. Naguib, N.J. Lane, S.C. Vogel, V. Presser, S. Dubois, J. Lu, L. Hultman, M.W. Barsoum, E.A.N. Caspi, High‐temperature neutron diffraction, raman spectroscopy, and first‐principles calculations of Ti3SnC2 and Ti2SnC, J. Am. Ceram. Soc. 99 (2016) 2233–2242.10.1111/jace.14210 ↗
37. The structure, elastic and thermodynamic properties of Ti2GaC from first-principles calculation10.1142/S0217979219500309 ↗
38. Whisker growth in sn coatings: a review of current status and future prospects10.1007/s11664-020-08440-z ↗
39. Spontaneous growth of metal whiskers on surfaces of solids: a review10.1016/j.jmst.2015.04.001 ↗
40. Synthesis and characterization of Hf2PbC, Zr2PbC and M2SnC (M=Ti, Hf, Nb or Zr)10.1016/S0955-2219(00)00127-8 ↗