journal article·2024-11

Exploration of pretreatment process and wettability of high bonding Ni-P coatings on W-Cu composites for electronic packaging

Jinxin Zou, Chong Ma, Hui Liu, Shasha Chang, Chunfu Hong, Dongguang Liu, Laima Luo

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Progress, challenges and potentials/trends of tungsten-copper (WCu) composites/pseudo-alloys: fabrication, regulation and application10.1016/j.ijrmhm.2021.105648 ↗
2. Recent progress in development of tungsten-copper composites: fabrication, modification and applications10.1016/j.ijrmhm.2018.03.014 ↗
3. Microstructure and properties of silver-added W-Cu prepared by infiltration sintering10.1016/j.ijrmhm.2022.105947 ↗
4. Microstructure and properties of WCu composites with low copper content at different sintering temperatures10.1016/j.ijrmhm.2023.106219 ↗
5. Microstructure, mechanical properties and hermeticity of W-Cu/HTCC brazed joints with surface metallization10.1016/j.ijrmhm.2023.106473 ↗
6. Corrosion characteristics of electroless Ni-P coatings deposited on W-Cu composite10.1179/174327809X419212 ↗
7. Electroless Ni-P coating on W-Cu alloy via potential activation process10.1179/026708408X375325 ↗
8. Study on Electroless Ni-P deposit on W-Cu alloy and its anti-corrosion mechanism
9. Interfacial reactions between Sn-2.5Ag-2.0Ni solder and electroless Ni(P) deposited on SiCp/Al composites10.1016/S1003-6326(09)60242-9 ↗
10. Electroless multilayer coatings on aluminium-silicon carbide composites for electronics packaging10.1016/j.jeurceramsoc.2007.02.079 ↗
11. Effects of isothermal aging on interfacial microstructure evolution and shear behavior of Au-12Ge/Ni(P)/Kovar solder joints10.1016/j.intermet.2020.106865 ↗
12. Solid state and liquid phase sintering of mechanically activated W-20wt.% Cu powder mixture10.1016/j.jallcom.2007.08.080 ↗
13. The activated sintering of WCu composites through spark plasma sintering10.1016/j.ijrmhm.2019.02.015 ↗
14. A feasibility study of W-Cu compositesproduction by high pressure compression of tungsten powder10.1016/j.ijrmhm.2010.09.002 ↗
15. Interface structure and work function of W-Cu interfaces10.1063/1.4833249 ↗
16. Simulation of Meso-scale accumulateddamage and induced crack behaviors of CuW alloy10.1016/S1875-5372(17)30148-0 ↗
17. Low-temperature densificationand microstructure of W-Cu composites with Sn additives10.1016/j.jmrt.2020.12.013 ↗
18. Effects of Zn additions on the solid-state sintering of W-Cu composites10.1016/j.matdes.2011.10.006 ↗
19. Assessment of solid state and liquid phase sintering models by comparison of isothermal densification kinetics in W and W-Cu systems10.1016/j.actamat.2015.12.041 ↗
20. Research on the densification of W-40wt.%Cu by liquid sintering and hot-hydrostatic extrusion10.1016/j.ijrmhm.2007.06.004 ↗
21. Improvement of physical properties of Cu-infiltrated W compacts via electroless nickel plating of primary tungstenpowder10.1016/j.surfcoat.2009.02.055 ↗
22. Densification and properties investigation of W-Cu composites prepared by electroless-plating and activated sintering10.1016/j.ijrmhm.2017.11.042 ↗
23. Thermal properties of W-Cu composites manu-factured by copper infiltration into tungsten fiber matrix10.1016/j.ijrmhm.2014.05.022 ↗
24. Improvement of machinability of tungsten by copper infiltration technique10.1016/j.ijrmhm.2007.12.005 ↗
25. Effect of current density on the texture, residual stress, microhardness and corrosion resistance of electrodeposited chromium coating10.1016/j.surfcoat.2023.129868 ↗
26. Influence of mode of electrodeposition, current density and saccharin on the microstructure and hardness of electrodeposited nanocrystalline nickel coatings10.1016/j.surfcoat.2016.02.024 ↗
27. Corrosion tests of nickelcoatings prepared from a Watts-type bath10.1007/s11998-011-9343-0 ↗
28. Effect of heat treatment on the properties of HA/BG composite films10.1016/j.ceramint.2018.01.173 ↗
29. Micro- and nano-testing of calcium phosphate coatings produced by pulsed laser deposition10.1016/S0142-9612(03)00202-3 ↗
30. Studies on crystallization of electroless Ni-P deposits10.1016/0924-0136(96)85110-7 ↗
31. Crystallisation and phase transformation behaviour of electroless nickel phosphorus platings during continuous heating10.1016/S0925-8388(03)00069-0 ↗
32. Thermal evolution, phase composition and fracture toughness of electroless Ni-P, Ni-W-P and Ni-Mo-W-P films for solderable surfaces on copper10.1016/j.surfcoat.2023.129722 ↗
33. Correlating tribological performance with phase transformation behavior for electroless Ni-(high)P coating10.1016/j.surfcoat.2017.08.043 ↗
34. The heat treatment effects on the structure and wear behavior of pulse electroforming Ni-P alloy coatings10.1016/j.jallcom.2006.07.120 ↗
35. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗
36. A systematic literature review: The effects of surface roughness on the wettability and formation of intermetallic compound layers in lead-free solder joints10.1016/j.jmapro.2022.08.045 ↗
37. Solder wetting kinetics in narrow V-grooves10.1016/S1359-6454(97)00205-X ↗
38. Effects of roughness on the wettability of high temperature wetting system10.1016/j.surfcoat.2015.12.092 ↗
39. Wetting of Ni-based amorphous and crystalline alloys by Sn and Sn-based solders10.1016/j.microrel.2020.113722 ↗
40. The wetting of Fe78B13Si9 by liquid Sn10.1016/S0167-577X(02)00429-9 ↗
41. Microstructure, mechanical and thermal properties of Ni-P(-SiC) coating on high volume fraction SiCp/Al composite10.1007/s12598-017-0934-5 ↗
42. High corrosion protection performance of the LDH/Ni-P composite coating on AM60B magnesium alloy10.1016/j.surfcoat.2020.125979 ↗
43. The study of electroless nickel plating directly on magnesium alloy10.1016/j.surfcoat.2014.03.043 ↗
44. Effect of micro-texture on substrate surface on adhesion performance of electroless NiP coating10.1016/j.jmapro.2021.12.025 ↗