Oxidation behaviour of uncoated and PDC-SiAlOC glass-coated TiAl at 750 °C in dry and humid air

Maciej Bik, Mathias Galetz, Lukas Mengis, Emma White, Wojciech Wieczorek, Klaudia Łyszczarz, Krzysztof Mroczka, Jakub Marchewka, Maciej Sitarz

Abstract

In this work polymer derived ceramic (PDC) coatings, based on SiAlOC glasses, were successfully applied on 48-2-2 TiAl alloy samples. These coatings showed a significant improvement in oxidation resistance in both dry and humid air conditions. The uncoated 48-2-2 TiAl alloy material showed poor oxidation resistance independent of the atmosphere. SEM, EPMA and Raman confocal imaging were used to investigate the oxidation mechanisms of the uncoated and coated 48-2-2 TiAl alloy in dry and humid air. The coating suppressed outward Ti diffusion and promoted alumina scale formation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. The Science, Technology, and Implementation of TiAl Alloys in Commercial Aircraft Engines10.1557/opl.2013.44 ↗
2. TiAl alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
3. High temperature oxidation behavior and research status of modifications on improving high temperature oxidation resistance of titanium alloys and titanium aluminides: A review10.1016/j.jallcom.2016.06.212 ↗
4. Development of TiAl – Si Alloys — A Review
5. Modeling concepts for intermetallic titanium aluminides10.1016/j.pmatsci.2016.01.001 ↗
6. Optimization of the fluorine effect for improving the oxidation resistance of TiAl-alloys10.4028/www.scientific.net/MSF.706-709.1061 ↗
7. Effects of tungsten alloying and fluorination on the oxidation behavior of intermetallic titanium aluminides for aerospace applications10.1016/j.intermet.2021.107270 ↗
8. Microstructure evolution and oxidation resistance of silicon-aluminizing coating on γ-TiAl alloy10.1016/j.apsusc.2015.08.204 ↗
9. Microstructure and cyclic oxidation resistance of Si-aluminide coatings on γ-TiAl at 850 °C10.1016/j.surfcoat.2020.126361 ↗
10. The Si influence on the microstructure and oxidation resistance of Ti-Al slurry coatings on Ti-48Al-2Cr-2Nb alloy10.1016/j.materresbull.2021.111336 ↗
11. Oxidation protection of γ-TiAl-based alloys - A review10.1016/j.intermet.2014.08.002 ↗
12. Oxidation behaviour and related microstructural changes of two β0–phase containing TiAl alloys between 600 °C and 900 °C10.1016/j.corsci.2020.109085 ↗
13. Critical assessment of the cyclic oxidation resistance of the aluminized Ti-48Al-2Cr-2Nb TiAl alloy at 700 °C and its impact on mechanical properties10.1016/j.surfcoat.2020.126646 ↗
14. Influence of water vapour on the oxidation behaviour of TiAl based multielement alloys10.1016/j.intermet.2021.107229 ↗
15. Scale mass gain, morphology and phase composition of air and steam oxidized electron beam melted and cast Ti–48Al–2Nb-0.7Cr-0.3Si alloys10.1016/j.intermet.2022.107553 ↗
16. The fate and role of in situ formed carbon in polymer-derived ceramics
17. Polymeric and ceramic silicon-based coatings-a review10.1039/C8TA09054H ↗
18. Reactive Element Effect Applied by Alloying and SiHfBCN Coating on the Oxidation of Pure Chromium10.1007/s11085-019-09926-w ↗
19. M. Parchovianský, I. Parchovianská, P. Švančárek, D. Medveď, M. Lenz-leite, G. Motz, D. Galusek, High-Temperature Oxidation Resistance of PDC Coatings in Synthetic Air and Water Vapor Atmospheres, (2021).10.3390/molecules26082388 ↗
20. C. Wu, X. Pan, F. Lin, G. Chen, L. Xu, Y. Zeng, Y. He, D. Sun, High-Temperature Anti-Oxidative Composite Coating Fabricated by Direct Writing, (2022).10.3390/polym14163281 ↗
21. Free carbon phase in SiOC glasses derived from ladder-like silsesquioxanes10.1016/j.molstruc.2016.03.096 ↗
22. Silicon oxycarbide glasses and glass-ceramics: “All-Rounder” materials for advanced structural and functional applications10.1111/jace.15932 ↗
23. Protective-conducting coatings based on black glasses (SiOC) for application in Solid Oxide Fuel Cells10.1016/j.ijhydene.2017.09.069 ↗
24. Studies on the oxidation resistance of SiOC glasses coated TiAl alloy10.1016/j.intermet.2018.09.014 ↗
25. Fundamentals of TiAl oxidation – A critical review10.1002/maco.19950460503 ↗
26. Optimization of the formation of coatings based on SiAlOC glasses via structural, microstructural and electrochemical studies10.1016/j.electacta.2019.04.080 ↗
27. Polymer Derived Ceramics based on SiAlOC glasses as novel protective coatings for ferritic steel10.1016/j.apsusc.2021.151826 ↗
28. Improvement of steam oxidation resistance of the γ -TiAl alloy with microarc oxidation coatings at 900–1200 ℃10.1016/j.corsci.2022.110711 ↗
29. Effects of water vapor and nitrogen on oxidation of TNM alloy at 650 °C10.1016/j.corsci.2019.07.006 ↗
30. An advanced tial alloy for high-performance racing applications10.3390/ma13214720 ↗
31. Microstructural characterizations of γ-TiAl alloy after high-temperature steam oxidations at 900, 1000, 1100 and 1200 °C10.1016/j.matchar.2022.111979 ↗
32. High temperature steam oxidation of Al3Ti-based alloys for the oxidation-resistant surface layer on Zr fuel claddings10.1016/j.jnucmat.2013.01.338 ↗
33. Performance of advanced turbocharger alloys and coatings at 850–950°C in air with water vapor10.1016/j.surfcoat.2012.08.099 ↗
34. Influence of water vapour on the oxidation behaviour of titanium aluminides10.1016/S0966-9795(01)00104-2 ↗
35. Influence of Water Vapor and Temperature on the Oxide Scale Growth and Alpha - Case Formation in Ti - 6Al - 4V Alloy10.1007/s11085-021-10088-x ↗
36. SiAlOC glasses derived from sol-gel synthesized ladder-like silsesquioxanes10.1016/j.ceramint.2018.10.047 ↗
37. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
38. Raman Spectra of Amorphous A1203 and Al2O3/MoO3 Obtained by Visible and Infrared Excitation10.1002/jrs.1250220109 ↗
39. Steam oxidation of aluminide coatings under high pressure and for long exposures10.1016/j.corsci.2018.08.053 ↗
40. Electrochemical characterization of anti-corrosion coatings formed on 6061 aluminum alloy by plasma electrolytic oxidation in the corrosion inhibitor-enriched aqueous solutions10.1016/j.electacta.2022.140652 ↗
41. Structure sensitive photocatalytic reduction of nitroarenes over TiO210.1038/s41598-017-08599-2 ↗
42. A. Biedunkiewicz, K. Jach, A. Obrosov, D. Garbiec, M. Bik, M. Sitarz, Z. Kucia, S. Wei, International Journal of Refractory Metals and Hard Materials Ti-Mo- x TiC composites manufactured by U-FAST reactive sintering, 108 (2022). https://doi.org/10.1016/j.ijrmhm.2022.105960.10.1016/j.ijrmhm.2022.105960 ↗
43. The significance of sub-surface depletion layer composition for the oxidation behaviour of γ-titanium aluminides10.1016/0956-716X(95)00155-O ↗
44. Lactic Acid Production from Glucose Over a Novel Nb2O5 Nanorod Catalyst10.1007/s10562-017-1988-6 ↗
45. Nanostructured T-Nb2O5-based composite with reduced graphene oxide for improved performance lithium-ion battery anode10.1007/s10853-020-04910-1 ↗
46. A DFT investigation of the role of oxygen vacancies on the structural, electronic and magnetic properties of ATiO3 (A = Mn, Fe, Ni) multiferroic materials10.1039/C8CP04443K ↗
47. A Raman-scattering study on the interface structure of nanolayered TiAlNTiN and TiNNbN multilayer thin films grown by reactive dc magnetron sputtering10.1063/1.1946193 ↗
48. Structural and mechanical properties of CVD deposited titanium aluminium nitride (TiAlN) thin films10.1007/s00339-017-1032-0 ↗
49. Effects of Nb addition on oxidation behavior of TiAl10.1016/0966-9795(95)94254-C ↗
50. Effect of Nb on oxidation behavior of high Nb containing TiAl alloys10.1016/j.intermet.2010.08.029 ↗
51. Materials at High Temperatures Characterisation and oxidation behaviour of plasma surface alloyed on γ -TiAl alloy10.1080/09603409.2020.1859309 ↗
52. High temperature air oxidation resistance of TiAlCr-Y coated Ti45Al8Nb between 750°C-950°C
53. Amorphous Si–B–C–N coatings for high-temperature oxidation protection of the γ-TiAl alloy10.1016/j.surfcoat.2022.128544 ↗
54. Effect of Cr, Nb, Mn, V, W and Si on high temperature oxidation of TiAl alloys10.1007/BF03027458 ↗
55. The interaction of water with solid surfaces: Fundamental aspects10.1016/S0167-5729(01)00020-6 ↗