journal article·2022-12

Optimized mechanical and tribological properties of thermally sprayed ceramic coatings by constructing crystalline–amorphous heterojunctions

Shuangjian Li, Chuangyong Yu, Chunming Deng, Jun Liu, Xi Tan, Wei Zeng

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Controllable fabrication of magnesium silicate hydroxide reinforced MoS2 hybrid nanomaterials as effective lubricant additives in PAO10.1016/j.apsusc.2022.153777 ↗
2. Microstructure evolution and deformation mechanisms during high rate and cryogenic sliding of copper10.1016/j.actamat.2018.09.016 ↗
3. Lowering coefficient of friction in Cu alloys with stable gradient nanostructures10.1126/sciadv.1601942 ↗
4. Reusable chromium oxide coating with lubricating behavior from 25 to 1000 °C due to a self-assembled mesh-like surface structure10.1016/j.surfcoat.2016.12.082 ↗
5. Adaptive VN/Ag nanocomposite coatings with lubricious behavior from 25 to 1000 °C10.1016/j.actamat.2010.06.006 ↗
6. Tribocorrosion behaviour of thermally sprayed cermet coatings in paper machine environment10.1016/j.triboint.2019.106006 ↗
7. Plasma sprayed YSZ coatings deposited at different deposition temperatures, part 2: Tribological performance10.1016/j.surfcoat.2018.06.093 ↗
8. Microstructure and properties of ZrB2-SiC continuous gradient coating prepared by high speed laser cladding10.1016/j.triboint.2022.107645 ↗
9. Interfacial and tribological properties of laser deposited TiOxNy/Ti composite coating on Ti alloy10.1016/j.triboint.2020.106758 ↗
10. YSZ/MoS2 self-lubricating coating fabricated by thermal spraying and hydrothermal reaction10.1016/j.ceramint.2018.06.258 ↗
11. Microstructure and tribological properties of ZrO2(Y2O3) matrix composites doped with different solid lubricants from room temperature to 800 °C10.1016/j.wear.2008.11.017 ↗
12. Influence of doping graphite on microstructure and tribological properties of plasma sprayed 3Al2O3–2SiO2 coating10.1016/j.triboint.2016.04.028 ↗
13. In situ carbon nanotube reinforcements in a plasma-sprayed aluminum oxide nanocomposite coating10.1016/j.actamat.2007.10.038 ↗
14. Toughness enhancement and tribochemistry of the Nb-Ag-N films actuated by solute Ag10.1016/j.actamat.2017.07.034 ↗
15. Silver diffusion and high-temperature lubrication mechanisms of YSZ–Ag–Mo based nanocomposite coatings10.1016/j.compscitech.2006.09.008 ↗
16. Bioinspired Smart Coating with Superior Tribological Performance10.1021/acsami.7b03986 ↗
17. Comparative study on wear behavior of plasma sprayed Al2O3 coatings sliding against different counterparts10.1016/j.ceramint.2017.02.122 ↗
18. Microstructural, mechanical and tribological properties of suspension plasma sprayed YSZ/h-BN composite coating10.1016/j.jeurceramsoc.2018.06.007 ↗
19. Process map for plasma sprayed aluminum oxide–carbon nanotube nanocomposite coatings10.1016/j.surfcoat.2008.03.024 ↗
20. Multiscale wear of plasma-sprayed carbon-nanotube-reinforced aluminum oxide nanocomposite coating10.1016/j.actamat.2008.08.020 ↗
21. Friction and abrasive wear behaviour of Al2O3-13TiO2 and Al2O3-13TiO2+Ni Graphite coatings10.1016/j.triboint.2018.01.067 ↗
22. Novel Processing for Combined Coatings with Dry Lubrication Ability
23. Effect of Substrate Surface Texture Shapes on the Adhesion of Plasma-Sprayed Ni-Based Coatings10.1007/s11666-020-01126-2 ↗
24. Plasma sprayed YSZ coatings deposited at different deposition temperatures, part 1: Splats, microstructures, mechanical properties and residual stress10.1016/j.surfcoat.2018.07.074 ↗
25. Heredity and variation of hollow structure from powders to coatings through atmospheric plasma spraying10.1016/j.surfcoat.2016.08.007 ↗
26. Epitaxial growth and cracking of highly tough 7YSZ splats by thermal spray technology10.1007/s40145-017-0252-2 ↗
27. Preparation of plasma sprayed mullite coating on stainless steel substrate and investigation of its environmental dependence of friction and wear behavior10.1016/j.triboint.2015.06.022 ↗
28. Bioinspired Hybrid Materials from Spray-Formed Ceramic Templates10.1002/adma.201500303 ↗
29. A new methodology to prepare ceramic-organic composite coatings with good cavitation erosion resistance10.1016/j.ultsonch.2018.02.018 ↗
30. Formation of self-lubricating PEO coating via in-situ incorporation of PTFE particles10.1016/j.surfcoat.2018.01.022 ↗
31. Controllable in situ fabrication of self-lubricating nanocomposite coating for light alloys10.1016/j.scriptamat.2021.114493 ↗
32. Preparation and tribological behaviors of magnesium silicate hydroxide-MoS2 nanoparticles as lubricant additive10.1016/j.wear.2022.204237 ↗
33. Construction of a sp3/sp2 Carbon Interface in 3D N-Doped Nanocarbons for the Oxygen Reduction Reaction10.1002/ange.201907915 ↗
34. Raman “fingerprinting” of amorphous carbon films10.1063/1.357385 ↗
35. Combined Effects of Structural Transformation and Hydrogen Passivation on the Frictional Behaviors of Hydrogenated Amorphous Carbon Films10.1021/acs.jpcc.5b04533 ↗
36. Molecular dynamics simulation of shear-induced graphitization of amorphous carbon films10.1016/j.carbon.2009.03.040 ↗
37. Influence of surface passivation on the friction and wear behavior of ultrananocrystalline diamond and tetrahedral amorphous carbon thin films10.1103/PhysRevB.85.155448 ↗
38. Probing the low-friction mechanism of diamond-like carbon by varying of sliding velocity and vacuum pressure10.1016/j.carbon.2013.08.065 ↗
39. Molecular-Scale Tribology of Amorphous Carbon Coatings: Effects of Film Thickness, Adhesion, and Long-Range Interactions10.1021/ja0178618 ↗
40. Friction Regimes of Water-Lubricated Diamond (111): Role of Interfacial Ether Groups and Tribo-Induced Aromatic Surface Reconstructions10.1103/PhysRevLett.119.096101 ↗
41. Anchoring PdCu Amorphous Nanocluster on Graphene for Electrochemical Reduction of N2 to NH3 under Ambient Conditions in Aqueous Solution10.1002/aenm.201800124 ↗
42. Hydrothermal Dehydration of Aqueous Fructose Solutions in a Closed System10.1021/jp074188l ↗
43. Synthesis of carbon micro-spheres by a glucose hydrothermal method10.1016/j.matlet.2007.08.011 ↗
44. Surface and in-depth distribution of sp2 and sp3 coordinated carbon atoms in diamond-like carbon films modified by argon ion beam bombardment during growth10.1016/j.carbon.2018.03.072 ↗
45. Synthesis and characterization of γ-Fe2O3@C nanorod-carbon sphere composite and its application as microwave absorbing material10.1016/j.jallcom.2015.08.236 ↗
46. Hierarchical Formation of Intrasplat Cracks in Thermal Spray Ceramic Coatings10.1007/s11666-016-0420-x ↗
47. Imaging Slit Pores Under Delaminated Splats by White Light Interference10.1007/s11666-018-0686-2 ↗
48. Microstructure Controlled Shear Band Pattern Formation and Enhanced Plasticity of Bulk Metallic Glasses Containing in situ Formed Ductile Phase Dendrite Dispersions10.1103/PhysRevLett.84.2901 ↗
49. Designing metallic glass matrix composites with high toughness and tensile ductility10.1038/nature06598 ↗
50. Ductile crystalline-amorphous nanolaminates10.1073/pnas.0702344104 ↗
51. Tribochemical aspects of silicon nitride ceramic sliding against stainless steel under the lubrication of seawater10.1016/j.triboint.2013.01.011 ↗