The effect of oxygen flow rate on metal–insulator transition (MIT) characteristics of vanadium dioxide (VO2) thin films by pulsed laser deposition (PLD)
Source abstract
Abstract
Abstract Vanadium dioxide (VO2), because of its unique metal–insulator phase transion around room temperature, has enormous potential for applications in thermochromic, electrochromic, microbolometery, and non-volatile switches. However, obtaining phase-pure VO2 has been challenging due to its narrow window of thermodynamic stability. Pulsed laser deposition (PLD) is considered to be one of the most promising technique to deposit phase-pure VO2 thin films. While optimizing PLD processing parameters, (such as oxygen pressure (PO2), substrate temperature (Ts), laser energy (EL), target-substrate distance (dT-S), and laser repetition rate (RR)) is crucial, and their effects have been reported, the effect of gas flow rate (QO2) has been largely neglected. Since the QO2 and PO2 of the PLD system are intertwined at the outset, most reports are focused only on either QO2 or PO2. We report on the effect of gas flow rate under constant PO2, on the quality of the VO2 thin films. Controlling flow rate affected the resistivity contrast between the metallic and insulator phases, the temperature ranges of the transition, and the width of hysteresis. We anticipate that this study will help set the standard for obtaining high quality VO2 thin films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials · Advanced Memory and Neural Computing · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Rare-earth nickelatesRNiO3: thin films and heterostructures10.1088/1361-6633/aaa37a ↗
2. Metal-insulator transition of strained SmNiO3 thin films: structural, electrical and optical properties10.1038/srep40915 ↗
3. Oxides which show a metal-to-insulator transition at the neel temperature10.1103/PhysRevLett.3.34 ↗
4. Recent progresses on physics and applications of vanadium dioxide10.1016/j.mattod.2018.03.029 ↗
5. Strain-induced pressure effect in pulsed laser deposited thin films of the strongly correlated oxide V2O310.1103/PhysRevB.74.195109 ↗
6. Phase transition behavior in microcantilevers coated with M1-phase VO2 and M2-phase VO2: Cr thin films10.1063/1.4716191 ↗
7. Vanadium dioxide as a natural disordered metamaterial: perfect thermal emission and large broadband negative differential thermal emittance
8. All optically driven memory device for terahertz waves10.1364/OL.384740 ↗
9. Diamagnetic to ferromagnetic switching in VO2 epitaxial thin films by nanosecond excimer laser treatment10.1063/1.4857155 ↗
10. Phase transformation induced modulation of the resonance frequency of VO2/TiO2 coated microcantilevers10.1557/adv.2018.140 ↗
11. Mott transition in VO2 revealed by infrared spectroscopy and nano-imaging10.1126/science.1150124 ↗
12. H.-T. Kim, B.-G. Chae, D.-H. Youn, S.-L. Maeng, G. Kim, K.-Y. Kang, a.Y.-S. Lim, Mechanism and observation of Mott transition in VO2-based two- and three-terminal devices, New J. Phys. 6 (2004): 1–20.10.1088/1367-2630/6/1/052 ↗
13. Epitaxial stabilization and phase instability of VO2 polymorphs10.1038/srep19621 ↗
14. Recent advances in fabrication strategies, phase transition modulation, and advanced applications of vanadium dioxide10.1063/1.5087864 ↗
15. VO2 thermochromic smart window for energy savings and generation10.1038/srep03029 ↗
16. Fabrication of phase change microstring resonators via top down lithographic techniques: incorporation of VO2/TiO2 into conventional processes10.1109/JMEMS.2019.2931805 ↗
17. S.A. Bukhari, A. Goswami, R. McGee, R. Abraham, D. Hume, H.J. Chung, T. Thundat, Bidirectional frequency tuning of vanadium dioxide (VO2) microstring resonator by optothermal excitation, in: 2020 IEEE 33rd International Conference on Micro Electro Mechanical Systems (MEMS), 2020, pp. 961–964.10.1109/MEMS46641.2020.9056248 ↗
18. Oxygen level: the dominant of resistive switching characteristics in cerium oxide thin films10.1088/0022-3727/45/35/355101 ↗
19. Electric-field-modulated nonvolatile resistance switching in VO2/PMN-PT(111) heterostructures10.1021/am405767q ↗
20. Nanostructured vanadium oxide thin film with high TCR at room temperature for microbolometer10.1016/j.infrared.2012.10.006 ↗
21. Gas sensor based on metal−insulator transition in VO2 nanowire thermistor10.1021/nl900676n ↗
22. Reductive transformation of V(iii) precursors into vanadium(ii) oxide nanowires10.1039/C8DT00848E ↗
23. Influence of different additives on the synthesis of VO2 polymorphs10.1016/j.ceramint.2013.04.016 ↗
24. Selective growth of single phase VO2(A, B, and M) polymorph thin films10.1063/1.4906880 ↗
25. Synthesis of phase pure vanadium dioxide (VO2) thin film by reactive pulsed laser deposition10.1063/1.5046455 ↗
26. Defect engineering of VO2 thin films synthesized by chemical vapor deposition10.1016/j.matchemphys.2019.122230 ↗
27. Correlation between surface morphology and electrical properties of VO2 films grown by direct thermal oxidation method10.1016/j.apsusc.2015.07.036 ↗
28. Sputtering deposition of sandwich-structured V2O5/Metal (V, W)/V2O5 Multilayers For The Preparation Of High-Performance Thermally Sensitive VO2 thin films with selectivity of VO2 (B) and VO2 (M) polymorph10.1021/acsami.6b00391 ↗
29. Tunable hysteresis in metal-insulator transition of nanostructured vanadium oxide thin films deposited by reactive direct current magnetron sputtering10.1016/j.tsf.2013.12.007 ↗
30. VO2–WO3 nanocomposite thin films synthesized by pulsed laser deposition technique10.1016/j.apsusc.2011.05.068 ↗
31. Transmission of reactive pulsed laser deposited VO2 films in the THz domain10.1016/j.apsusc.2016.04.018 ↗
32. Preparation of Y-Ba-Cu oxide superconductor thin films using pulsed laser evaporation from high Tc bulk material10.1063/1.98366 ↗
33. Pulsed laser deposition of oriented VO2 thin films on R-cut sapphire substrates10.1063/1.110177 ↗
34. Pulsed laser deposition of VO2 thin films10.1063/1.112476 ↗
35. Oxygen pressure induced structure, morphology and phase-transition for VO2/c-sapphire films by PLD10.1007/s00339-013-7972-0 ↗
36. Oxygen pressure dependent VO2 crystal film preparation and the interfacial epitaxial growth study10.1016/j.tsf.2012.05.086 ↗
37. Synthesis of vanadium oxides by pulsed laser deposition and rapid thermal annealing
38. Sharpness and intensity modulation of the metal-insulator transition in ultrathin VO2 films by interfacial structure manipulation
39. Effect of process parameters on phase stability and metal-insulator transition of vanadium dioxide (VO2) thin films by pulsed laser deposition10.1016/j.actamat.2017.07.025 ↗
40. Fabrication of smooth thin film of vanadium oxides (VOx) using pulsed laser deposition10.1007/s00339-020-3310-5 ↗
41. A metal-insulator transition study of VO2 thin films grown on sapphire substrates10.1063/1.4997437 ↗
42. Optical and electrical properties of vanadium dioxide films prepared under optimized RF sputtering conditions10.1016/S0927-0248(98)00166-4 ↗
43. Transport behavior and electronic structure of phase pure VO2 thin films grown on c-plane sapphire under different O2 partial pressure10.1063/1.4817174 ↗
44. Excitation kinetics of oxygen O(1D) state in low-pressure oxygen plasma and the effect of electron energy distribution function10.1515/jaots-2017-0002 ↗
45. Surface diffusion lengths of adatoms on 6H-SiC{0001} faces in chemical vapor deposition of SiC10.1063/1.359999 ↗
46. Influence of grain size on transition temperature of thermochromic VO210.1063/1.4906122 ↗
47. Comprehensive study of the metal-insulator transition in pulsed laser deposited epitaxial VO2 thin films10.1063/1.4788804 ↗
48. Observation of insulating–insulating monoclinic structural transition in macro-sized VO2 single crystals10.1002/pssr.201105011 ↗
49. Measurement of a solid-state triple point at the metal–insulator transition in VO210.1038/nature12425 ↗
50. In situ Raman spectroscopy study of metal-enhanced hydrogenation and dehydrogenation of VO2