Effect of extremely aggressive environment on the nature of corrosion scales of HP-13Cr stainless steel
Source abstract
Abstract
Abstract The nature of corrosion scales formed on HP-13Cr stainless steel (HP-13Cr SS) in the extremely aggressive environment was investigated by means of microstructure characterization and high-temperature-high-pressure electrochemical measurements. The results of these studies indicated that the precipitation of Cr(OH)3 is the dominating factor affecting on the formation of corrosion scales, and its effect can be categorized based on two compromising aspects. On the one hand, Cr(OH)3 precipitation contributed to the increase of scales thickness. On the other hand, it inhibited the precipitation of FeCO3 due to the hydrolysis of Cr3+. Because of these reasons, the corrosion scales undergo significant microstructural changes, i.e., from monolayer (95 °C/2.8 MPa) to bilayer (120 °C/3.2 MPa and 150 °C/3.6 MPa), then to single layer (180 °C/3.8 MPa). Therefore, the corrosion-resistance performance of corrosion scales decreased with increasing temperature and CO2 pressure, wherein the decreasing pitting potential and repassivation potential accompanied with the increasing density and diffusivity of acceptor in the scales.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. The geometry and origin of strike-slip faults cutting the Tazhong low rise mega anticline (central uplift, Tarim Basin, China) and their control on hydrocarbon distribution in carbonate reservoirs10.1016/j.jngse.2014.12.030 ↗
2. Surface damage mitigation of Ti6Al4V alloy via thermal oxidation for oil and gas exploitation application: characterization of the microstructure and evaluation of the surface performance10.1039/C6RA28421C ↗
3. Investigation of stress corrosion cracking behavior of super 13Cr tubing by full-scale tubular goods corrosion test system10.1016/j.engfailanal.2015.02.001 ↗
4. Pourbaix diagram for HP-13Cr stainless steel in the aggressive oilfield environment characterized by high temperature, high CO2 partial pressure and high salinity
5. Impact of reversed austenite on the pitting corrosion behavior of super 13Cr martensitic stainless steel10.1016/j.electacta.2016.01.094 ↗
6. The effects of temperature and hydrodynamics on the CO2 corrosion of 13Cr and 13Cr5Ni2Mo stainless steels in the presence of free acetic acid10.1016/j.corsci.2004.05.020 ↗
7. Influence of chloride ions on corrosion of modified martensitic stainless steels at high temperatures under a CO2 environment10.5006/1141 ↗
8. Effect of CO2 on the stability of steels with 1% and 13% Cr in saline water10.1016/j.corsci.2009.01.025 ↗
9. Investigation on carbon dioxide corrosion behaviour of HP13Cr110 stainless steel in simulated stratum water10.1016/j.corsci.2009.08.056 ↗
10. Effects of temperature on the corrosion behavior of 13Cr martensitic stainless steel during exposure to CO2 and Cl− environment10.1016/j.matlet.2005.06.002 ↗
11. Characterization of corrosion films formed on austenitic stainless steel in supercritical CO2 containing H2O and O210.5006/2726 ↗
12. Comparison of surface fractal dimensions of chromizing coating and P110 steel for corrosion resistance estimation10.1016/j.apsusc.2014.05.062 ↗
13. An investigation on the continuous and uniform thin membrane passive film formed on sputtered nanocrystalline stainless steel10.1016/j.corsci.2015.11.031 ↗
14. Influence of grain size on the corrosion behavior of a Ni-based superalloy nanocrystalline coating in NaCl acidic solution10.1016/j.electacta.2007.10.048 ↗
15. Influence of nanocrystallization on passive behavior of Ni-based superalloy in acidic solutions10.1016/j.electacta.2006.08.070 ↗
16. Passivity breakdown, pit initiation and propagation of pits in metallicmaterials—review10.1016/j.corsci.2014.10.006 ↗
17. Unmasking chloride attack on the passive film of metals
18. Full depth profile of passive films on 316L stainless steel based on high resolution HAXPES in combination with ARXPS10.1016/j.apsusc.2012.02.099 ↗
19. Morphological and compositional analysis of passive film on austenitic stainless steel in nitric acid medium10.1016/j.apsusc.2011.01.026 ↗
20. Cation profiling of passive films on stainless steel formed in sulphuricand acetic acid by deconvolution of angle-resolved X-ray photoelectronspectra10.1016/j.apsusc.2013.07.158 ↗
21. Quasi-in-situ observing the growth of native oxide film on the FeCr 15 Ni 15 austenitic alloy by TEM10.1016/j.corsci.2018.06.029 ↗
22. The electrochemical corrosion behavior of nanocrystalline 304 stainless steel prepared by magnetron sputtering10.1149/2.034211jes ↗
23. Semiconducting properties of passive films formed on stainless steels: influence of thealloying elements10.1149/1.1838880 ↗
24. Direct imaging of native passive film on stainless steel by aberration corrected STEM10.1016/j.corsci.2010.08.025 ↗
25. Observation of passive films on Fe–20Cr–xNi (x= 0, 10, 20wt.%) alloys using TEM and Cs-corrected STEM–EELS10.1016/j.corsci.2013.10.023 ↗
26. In situ study on the effects of Ni and Mo on the passive film formed on Fe–20Cr alloys by photoelectrochemical and Mott-Schottky techniques10.1016/j.jelechem.2006.02.031 ↗
27. The semiconducting properties of passive films formed on AISI 316 L and AISI 321 stainless steels: a test of the point defect model (PDM)10.1016/j.corsci.2011.05.063 ↗
28. Semiconducting and passive film properties of nitrogen-containing type 316LN stainless steels10.1016/j.corsci.2006.05.041 ↗
29. Study on passivation and erosion-enhanced corrosion resistance by Mott-Schottky analysis10.1016/j.electacta.2006.07.026 ↗
30. A point defect model for anodic passive films I. Film growth kinetics10.1149/1.2127591 ↗
31. A point-defect model for anodic passive films. 2. Chemical breakdown and pit initiation10.1149/1.2127592 ↗
32. Electrochemical investigation and ab initio computation of passive film properties on copper in anaerobic sulphide solutions10.1016/j.corsci.2016.12.010 ↗
33. External reference electrodes for use in high-temperature aqueous systems10.1149/1.2129192 ↗
34. ASTM G61-86. Standard Test Method for Conducting Cyclic Potentiodynamic Polarization Measurements for Localized Corrosion Susceptibility of Iron-, Nickel-, or Cobalt-Based Alloys, 2009.
35. Effect of electropolishing on corrosion of Alloy 600 in high temperature water10.1016/j.corsci.2015.05.026 ↗
36. Characterization of corrosion scale formed on 3Cr steel in CO2-saturated formation water10.1016/j.corsci.2016.04.033 ↗
37. Corrosion of alloy steels containing 2% chromium in CO2 environments10.1016/j.corsci.2012.06.006 ↗
38. The evolution of electrochemical behavior and oxide film properties of 304 stainless steel in high temperature aqueous environment10.1016/j.electacta.2012.03.148 ↗
39. On the existence of our metals-based civilization. I. Phasespace analysis10.1149/1.2195877 ↗
40. The point defect model for the passive state10.1149/1.2069096 ↗
41. The point defect model for bilayer passive films10.1149/1.3496427 ↗
42. Physicochemical performance of FeCO3 films influenced by anions10.1039/C4RA14313B ↗
43. A new method for estimating thediffusivities of vacancies in passive films10.1016/0013-4686(95)00312-6 ↗
44. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
45. On the fundamentals of electrochemical corrosion of X65 steel in CO2-containing formation water in the presence of acetic acid in petroleum production10.1016/j.corsci.2008.10.013 ↗
46. A mechanistic model for carbon dioxide corrosion of mild steel in the presence of protective iron carbonates films—Part 1: Theory and verification10.5006/1.3277576 ↗
47. Formation mechanism and protective property of corrosion product scale on X70 steel under supercritical CO2 environment10.1016/j.corsci.2015.08.016 ↗
48. Effect of temperature on the 3Cr low-alloyed steel initial corrosion behavior in CO2 solution10.1016/j.matchemphys.2016.04.083 ↗
49. The effect of temperature and ionic strength on iron carbonate (FeCO3) solubility limit10.1016/j.corsci.2009.03.009 ↗
50. G. Schmitt, M. Horstemeier, Fundamental aspects of CO2 metal loss corrosion part II: influence of different parameters on CO2 corrosion mechanisms, CORROSION/2006, Paper No. 112, NACE, Houston, TX, 2006.10.5006/C2006-06112 ↗
51. K. Chokshi, W. Sun, S. Nesic, Iron Carbonate scale growth and the effect of inhibition in CO2 corrosion of mild steel, CORROSION/2005, Paper No. 285, NACE, Houston, TX, 2005.10.5006/C2005-05285 ↗
52. Effect of chromium on the pitting resistance of oil tube steel in a carbon dioxide corrosion system10.5006/1.3278195 ↗
53. Investigation of the specific adsorption of HSO4−, (SO42−) and Cl− ions on Co and Fe by radiotracer technique in the course of corrosion of the metals in perchlorate media10.1016/j.corsci.2003.11.002 ↗
54. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗