Influence of temperature on the soldering process of CLCC-3 package components using AuSn20 solder

Zhihuan Zhao, Guanghao Gong, Mingming Jiang, Chuanzhong Chen, Peng Li, Weihai Song, Zhibin Zhao, Li Zhang, Huijun Yu

AIP Advances· Volume 10· Issue 5

Abstract

In this study, a CLCC-3 shell and a cover were connected via soldering with AuSn20 as the solder. An Au–Sn eutectic reaction occurred during the sealing process. At high soldering temperatures, only the eutectic ζ′-Au5Sn and δ-AuSn phases remained. At the interface between the solder and the Au/Ni coating, Ni entered Au5Sn and AuSn to form (Au,Ni)5Sn and (Au,Ni)Sn and Au entered the lattice of the Ni3Sn2 phase to form the ternary compound (Ni,Au)3Sn2. The experimental results demonstrated that at a soldering heating plate temperature of 320 °C, the structure of the soldering area was compact and there were no holes in the soldering area. Under these conditions, the macroscopic appearance of the product improved, the solder was sufficiently melted, and the cover plate was well infiltrated, which resulted in the formation of a good, dense connection with the base plate.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials (Ministry of Education) and Shandong Engineering Research Center for Superhard Material, Department of Materials Science and Engineering, Shandong University 1 , Jinan 250061, China

School of Mechanical and Electronic Engineering, Shandong Agricultural and Engineering University 2 , Jinan 250100, China

Jinan Semiconductor Research Institute 3 , Jinan 250014, China

Lihuayi Group Co., Ltd. 4 , Lijin, Dongying 257400, China

Key Laboratory of High-Efficiency and Clean Mechanical Manufacture (Ministry of Education) and National Demonstration Center for Experimental Mechanical Engineering Education, School of Mechanical Engineering, Shandong University 5 , Jinan 250061, China

Funding

The Key R&D Project of Shandong Province

References (16)

Show source-provided references
1. Microelectron. Reliab. · 2017 · 75 · 7710.1016/j.microrel.2017.06.016 ↗
2. 2014
3. China Sci. Technol. Inf. · 2013 · 4 · 12510.3969/j.issn.1001-8972.2013.08.066 ↗
4. Semicond. Technol. · 2015 · 40 · 84010.13290/j.cnki.bdtjs.2015.11.008 ↗
5. 2018 · 3849
6. Spec. Cast. Nonferrous Alloys · 2018 · 38 · 71210.15980/j.tzzz.2018.07.005 ↗
7. Gold Bull. · 2002 · 35 · 2110.1007/bf03214833 ↗
8. Ceram. Int · 2020 · 46 · 1280610.1016/j.ceramint.2020.02.050 ↗
9. J. Electron. Mater. · 2019 · 48 · 792310.1007/s11664-019-07632-6 ↗
10. Semicond. Technol. · 2019 · 09 · 72310.13290/j.cnki.bdtjs.2019.09.012 ↗
11. AIP Adv. · 2014 · 4 · 03131210.1063/1.4867100 ↗
12. J. Changchun Univ. Sci. Technol. · 2017 · 4 · 7810.3969/j.issn.1672-9870.2017.02.020 ↗
13. Electron. Compon. Mater. · 2019 · 38 · 10610.14106/j.cnki.1001-2028.2019.08.018 ↗
14. J. Electron. Mater. · 2016 · 45 · 547810.1007/s11664-016-4733-9 ↗
15. AIP Adv. · 2018 · 8 · 03521310.1063/1.5024803 ↗
16. Sci. Technol. Adv. Mater. · 2019 · 20 · 87610.1080/14686996.2019.1640072 ↗