Microstructure and properties of (Ti, Cr) C reinforced novel medium manganese steel

Zhengbing Meng, Wei Liu, Xia Lv, Chaoyang Zhou

AIP Advances· Volume 11· Issue 3

Abstract

In the casting process, alloying elements Mo and Cr are needed to improve the wear resistance of medium manganese steels for low impact energy. The element Ti is added to avoid the high cost of expenditure for using Mo. This paper studies the effect of Ti and Cr on microstructure and properties of medium manganese steel. It shows that a large number of polygon, column, and square (Ti, Cr) C particles (<13 μm) are formed in the casting samples using the present heat treatment process. A new type of Ti–Cr modified medium manganese steel (Ti content of 0.56%–1.48%) is produced by using (Ti, Cr) C reinforced phase particles. Compared with the traditional medium manganese steel (blank), the hardness increases twice with a slight decrease in impact toughness [traditional and modified medium manganese steels (blank and steels A, B, and C) have values of 42.1 J/cm2, 47.5 J/cm2, 43.8 J/cm2, and 37.9 J/cm2], and the wear resistance also increased nearly two times.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering, Guilin University of Technology 1 , Guilin 541004, China

Guangxi Chinalco Industrial Service Co., Ltd. 2 , Pingguo 531400, China

School of Metallurgical and Materials Engineering, Jiangsu University of Science and Technology 3 , Zhangjiagang 215600, China

Funding

Major Science and Technology Projects in Guangxi Province, China

References (19)

Show source-provided references
1. Improved work-hardening ability and wear resistance of austenitic manganese steel under non-severe impact-loading conditions10.1016/0043-1648(87)90024-x ↗
2. Effects of impact energy on the wear resistance and work hardening mechanism of medium manganese austenitic steel10.1007/s40544-017-0158-6 ↗
3. Impact of reversed austenite on the impact toughness of the high-strength steel of low carbon medium manganese10.1007/s11837-017-2732-9 ↗
4. Effect of Ti on austenite grain growth behavior in high carbon steels10.1016/s1006-706x(14)60109-6 ↗
5. A nanoscale dispersion of TiC in cast carbon steel through a reaction in melt10.1016/j.matchemphys.2012.12.007 ↗
6. Tempering behavior of TiC-reinforced SKD11 steel matrix composite10.1007/s12540-018-0065-z ↗
7. Intercritical tempering enables nanoscale austenite/ε-martensite formation in low-C medium-Mn steel: A pathway to control mechanical properties10.1016/j.msea.2018.08.082 ↗
8. Grain growth behavior of coarse-grained austenite in a Nb–V–Ti microalloyed steel10.1016/j.msea.2009.05.037 ↗
9. Effect of rare earth yttrium on hot ductility of20CrMnTi steel with 0.05% tin10.1051/metal/2015017 ↗
10. Phase diagram calculation of high chromium cast irons and influence of its chemical composition10.1016/j.matdes.2008.04.061 ↗
11. The abrasive wear resistance of TIC and (Ti, W) C-reinforced Fe–17Mn austenitic steel matrix composites10.1016/j.triboint.2009.12.057 ↗
12. The effect of production method on properties of Fe–TiC composite10.1016/j.minpro.2010.01.002 ↗
13. The impact wear-resistance enhancement mechanism of medium manganese steel and its applications in mining machines10.1016/j.wear.2017.01.015 ↗
14. Microstructure and wear behaviour of 38CrMoAl steel laser-processed with the addition of MoS2 or WS2
15. Effect of self-tempering temperature on precipitation of secondary phase in V–Ti–N high-strength seismic bars10.1007/s12666-019-01646-8 ↗
16. Effects of chromium sources on the microstructure and properties of TiC-steel composites10.1080/00325899.2018.1496006 ↗
17. Formation mechanism and phase evolution of in situ synthesizing TiC-reinforced 316L stainless steel matrix composites by laser melting deposition10.1016/j.matlet.2018.01.097 ↗
18. The effect of titanium on the abrasion resistance of 15Cr–3Mo white cast iron10.1016/s0043-1648(00)00523-8 ↗
19. Microstructures, wear behavior and mechanical properties of the TiC ceramic particulate locally reinforced Ni-Hard4 white cast iron matrix10.1007/s12666-015-0731-5 ↗