Observation of intermediate bands in Eu3+ doped YPO4 host: Li+ ion effect and blue to pink light emitter
Source abstract
Abstract
This article explores the tuning of blue to pink colour generation from Li+ ion co-doped YPO4:5Eu nanoparticles prepared by polyol method at ∼100-120 °C with ethylene glycol (EG) as a capping agent. Interaction of EG molecules capped on the surface of the nanoparticles and/or created oxygen vacancies induces formation of intermediate/mid gap bands in the host structure, which is supported by UV-Visible absorption data. Strong blue and pink colors can be observed in the cases of as-prepared and 500 °C annealed samples, respectively. Co-doping of Li+ enhances the emission intensities of intermediate band as well as Eu3+. On annealing as-prepared sample to 500 °C, the intermediate band emission intensity decreases, whereas Eu3+ emission intensity increases suggesting increase of extent of energy transfer from the intermediate band to Eu3+ on annealing. Emission intensity ratio of electric to magnetic dipole transitions of Eu3+ can be varied by changing excitation wavelength. The X-ray photoelectron spectroscopy (XPS) study of as-prepared samples confirms the presence of oxygen vacancies and Eu3+ but absence of Eu2+. Dispersed particles in ethanol and polymer film show the strong blue color, suggesting that these materials will be useful as probes in life science and also in light emitting device applications.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Lanthanide and Transition Metal Complexes · Quantum Dots Synthesis And Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Banaras Hindu University 1 Department of Physics, , Varanasi 221 005, India
Bhabha Atomic Research Centre 2 Chemistry Division, , Mumbai 400 085, India
Bhabha Atomic Research Centre 3 Material Science Division, , Mumbai 400 085, India
CSIR-National Metallurgical Laboratory 4 , Jamshedpur 831 007, India
UGC-DAE Consortium for Scientific Research 5 , Indore 452 001, India
Dr. Hari Singh Gour University 6 Department of Physics, , Sagar 470 003, India
References (47)
Show source-provided references
1. J. Mater. Chem. · 2011 · 21 · 311310.1039/c0jm03275a ↗
2. J. Mater. Chem. · 2011 · 21 · 532610.1039/c0jm03470c ↗
3. Dalton Trans. · 2011 · 40 · 759510.1039/c1dt10878f ↗
4. Dalton Trans. · 2011 · 40 · 735710.1039/c1dt10460h ↗
5. Dalton Trans. · 2011 · 40 · 997110.1039/c1dt10043b ↗
6. J. Mater. Chem. · 2011 · 21 · 1931010.1039/c1jm12871j ↗
7. Dalton Trans. · 2012 · 41 · 631010.1039/c2dt30380a ↗
8. Phys. Chem. Chem. Phys. · 2012 · 14 · 697410.1039/c2cp24044k ↗
9. Chem. Rev. · 2009 · 109 · 428310.1021/cr8003983 ↗
10. Nanoscale · 2011 · 3 · 156810.1039/c0nr00774a ↗
11. Anal. Chem. · 2001 · 73 · 547210.1021/ac010162t ↗
12. Rai · 2012
13. Dalton Trans. · 2011 · 40 · 759010.1039/c1dt10327j ↗
14. Dalton Trans. · 201210.1039/C2DT31257C ↗
15. J. Appl. Phys. · 2012 · 112 · 01430610.1063/1.4731644 ↗
16. J. Lumin. · 2012 · 132 · 140010.1016/j.jlumin.2012.01.037 ↗
17. J. Alloys Comp. · 201210.1016/j.jallcom.2012.06.103 ↗
18. Phy. Rev. B · 2009 · 80 · 08510310.1103/PhysRevB.80.085103 ↗
19. Mater. Res. Bull. · 2009 · 44 · 17310.1016/j.materresbull.2008.03.016 ↗
20. J. Phys. Chem. B · 2006 · 110 · 2143810.1021/jp0552224 ↗
21. Hyperf. Interact. · 2007 · 175 · 13110.1007/s10751-008-9597-9 ↗
22. J. Lumin. · 2002 · 96 · 5110.1016/S0022-2313(01)00211-3 ↗
23. J. Rare Earth. · 2008 · 26 · 49510.1016/S1002-0721(08)60125-8 ↗
24. J. Am. Chem. Soc. · 2010 · 132 · 275910.1021/ja909578s ↗
25. Opt. Mater. · 2010 · 32 · 85710.1016/j.optmat.2009.12.011 ↗
26. Phys. Stat. Sol. (a) · 2007 · 204 · 117810.1002/pssa.200623033 ↗
27. Chem. Mater. · 2002 · 14 · 214010.1021/cm0109701 ↗
28. Chem. Commun. · 2006 · 352210.1039/b606531g ↗
29. J. Mater. Chem. · 2010 · 20 · 45910.1039/b917384f ↗
30. Chem. Mater. · 2003 · 15 · 460410.1021/cm034495d ↗
31. J. Am. Ceram. Soc. · 2011 · 94 · 165110.1111/j.1551-2916.2011.04532.x ↗
32. Mater. Res. Bull. · 2010 · 45 · 87010.1016/j.materresbull.2010.02.020 ↗
33. 1959
34. 1975
35. J. Raman Spectrosc. · 1981 · 11 · 27310.1002/jrs.1250110411 ↗
36. J. Solid State Chem. · 2007 · 180 · 247810.1016/j.jssc.2007.06.025 ↗
37. 1986
38. Appl. Phys. Lett. · 2006 · 88 · 17311810.1063/1.2198821 ↗
39. See supplementary material at http://dx.doi.org/10.1063/1.4739504 for parameters obtained after mono-exponential equation fitting to decay data, deconvolution of O(1s) peak, luminescence spectra of 3 and 7 at.% Li+ co-doped YPO4:5Eu, Behavior of electric and magnetic dipole transitions of Eu3+ under different Li+ ion co-doping at different excitation wavelengths and mono-exponential fitting to luminescence decay data.
40. Phys. Rev. · 1962 · 127 · 75010.1103/PhysRev.127.750 ↗
41. J. Chem. Eur. · 2005 · 11 · 218310.1002/chem.200400649 ↗
42. J. Lumin. · 2007 · 127 · 74710.1016/j.jlumin.2007.05.004 ↗
43. J. Nanosci. Nanotechn. · 2008 · 8 · 305910.1166/jnn.2008.152 ↗
44. Opt. Mater. · 2010 · 32 · 61610.1016/j.optmat.2009.12.009 ↗
45. Physica B · 2000 · 279 · 26210.1016/S0921-4526(99)00876-5 ↗
46. J. Mater. Chem. · 201210.1039/C2JM32049E ↗
47. AIP. Conf. Proc. · 2010 · 1313 · 39110.1063/1.3530556 ↗