Zhili Liang, Abdulaziz Baubaid, Mariusz Radtke, Maximilian Mellin, Clément Maheu, Sandipan Maiti, Hadar Sclar, Igor Píš, Silvia Nappini, Elena Magnano, Federica Bondino, Robert Winkler, René Hausbrand, Christian Hess, Lambert Alff, Boris Markovsky, Doron Aurbach, Wolfram Jaegermann, Gennady Cherkashinin

Advanced Science· Volume 12· Issue 7

Abstract

Abstract The design of cathode/electrolyte interfaces in high‐energy density Li‐ion batteries is critical to protect the surface against undesirable oxygen release from the cathodes when batteries are charged to high voltage. However, the involvement of the engineered interface in the cationic and anionic redox reactions associated with (de‐)lithiation is often ignored, mostly due to the difficulty to separate these processes from chemical/catalytic reactions at the cathode/electrolyte interface. Here, a new electron energy band diagrams concept is developed that includes the examination of the electrochemical‐ and ionization‐ potentials evolution upon batteries cycling. The approach enables to forecast the intrinsic stability of the cathodes and discriminate the reaction pathways associated with interfacial electronic charge‐transfer mechanisms. Specifically, light is shed on the evolution of cationic and anionic redox in high‐energy density lithium‐rich 0.33Li2MnO3·0.67LiNi0.4Co0.2Mn0.4O2 (HE‐NCM) cathodes, particularly those that undergo surface modification through SO2 and NH3 double‐gas treatment to suppress the structural degradation. The chemical composition and energy distribution of the occupied and unoccupied electronic states at the different charging/discharging states are quantitatively estimated by using advanced spectroscopy techniques, including operando Raman spectroscopy. The concept is successfully demonstrated in designing artificial interfaces for high‐voltage olivine structure cathodes enabling stable battery operation up to 5.1 V versus Li+/Li.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Materials Science Technische Universität Darmstadt Peter‐Grünberg‐Str. 2 D‐64287 Darmstadt Germany

Department of Chemistry Eduard‐Zintl‐Institut für Anorganische und Physikalische Chemie Technische Universität Darmstadt Peter‐Grünberg‐Str. 8 D‐64287 Darmstadt Germany

Department of Chemistry Institute for Nanotechnology and Advanced Materials (BINA) Bar‐llan University 5290002 Ramat‐Gan Israel

CNR – Istituto Officina dei Materiali (IOM) Strada Statale 14, km. 163,5 in Area Science Park Basovizza 34149 Trieste Italy

Nanotechnology Research Laboratory Faculty of Engineering University of Sydney 2006 Camperdown Australia

Department of Chemistry BINA – BIU Institute of Nanothechnology and Advanced Materials INIES – Israel National Institute of Energy Storage (supported by Israel Ministry of Energy and Infrastructures) Bar‐Ilan University 5290002 Ramat‐Gan Israel

References (72)

Show source-provided references
1. 10.1021/ja06202710.1021/ja062027 ↗
2. 10.1149/2.038306jes10.1149/2.038306jes ↗
3. 10.1021/jp412197z10.1021/jp412197z ↗
4. 10.1016/j.matt.2020.12.00410.1016/j.matt.2020.12.004 ↗
5. 10.1038/nchem.247110.1038/nchem.2471 ↗
6. 10.1021/cm901452z10.1021/cm901452z ↗
7. 10.1038/s41560-018-0097-010.1038/s41560-018-0097-0 ↗
8. 10.1038/s41467-022-28793-910.1038/s41467-022-28793-9 ↗
9. 10.1149/2.0111514jes10.1149/2.0111514jes ↗
10. 10.1038/nchem.252410.1038/nchem.2524 ↗
11. 10.1016/j.elecom.2004.08.00210.1016/j.elecom.2004.08.002 ↗
12. 10.1016/j.jpowsour.2008.07.07310.1016/j.jpowsour.2008.07.073 ↗
13. 10.1039/b702425h10.1039/b702425h ↗
14. 10.1038/s41578-022-00416-110.1038/s41578-022-00416-1 ↗
15. 10.1021/cm070435m10.1021/cm070435m ↗
16. 10.1038/s41560-024-01615-610.1038/s41560-024-01615-6 ↗
17. 10.1002/anie.20150640810.1002/anie.201506408 ↗
18. 10.1038/ncomms1359810.1038/ncomms13598 ↗
19. 10.1002/adma.20180175110.1002/adma.201801751 ↗
20. 10.1016/j.ensm.2019.01.00410.1016/j.ensm.2019.01.004 ↗
21. 10.1103/PhysRevB.104.07510910.1103/PhysRevB.104.075109 ↗
22. 10.1002/aesr.20200008910.1002/aesr.202000089 ↗
23. 10.1002/adfm.20200808310.1002/adfm.202008083 ↗
24. 10.1039/C5TA00009B10.1039/C5TA00009B ↗
25. 10.1002/aenm.20170070810.1002/aenm.201700708 ↗
26. 10.1149/1945-7111/aba6cb10.1149/1945-7111/aba6cb ↗
27. 10.1002/aenm.20180210510.1002/aenm.201802105 ↗
28. 10.1002/adma.20210956410.1002/adma.202109564 ↗
29. 10.1016/j.ensm.2021.11.04410.1016/j.ensm.2021.11.044 ↗
30. 10.1021/acsaem.0c0009810.1021/acsaem.0c00098 ↗
31. 10.1039/D3MA00236E10.1039/D3MA00236E ↗
32. 10.1103/PhysRevB.40.571510.1103/PhysRevB.40.5715 ↗
33. 10.1021/acs.chemrev.9b0043910.1021/acs.chemrev.9b00439 ↗
34. 10.1039/C6RA01915C10.1039/C6RA01915C ↗
35. 10.1023/A:101908900204110.1023/A:1019089002041 ↗
36. 10.1002/sia.129210.1002/sia.1292 ↗
37. 10.1103/PhysRevB.39.619410.1103/PhysRevB.39.6194 ↗
38. 10.1021/acs.jpcc.5b0579310.1021/acs.jpcc.5b05793 ↗
39. 10.1016/j.ccr.2004.03.01810.1016/j.ccr.2004.03.018 ↗
40. 10.1103/PhysRevB.32.489910.1103/PhysRevB.32.4899 ↗
41. b)K.Küpper Ph.D. Thesis Universität Osnabrück Germany 2005;
42. 10.1103/PhysRevB.82.19543110.1103/PhysRevB.82.195431 ↗
43. 10.1021/cm504753410.1021/cm5047534 ↗
44. 10.1149/1.205511510.1149/1.2055115 ↗
45. 10.1039/cs997260025910.1039/cs9972600259 ↗
46. 10.1149/2.0441903jes10.1149/2.0441903jes ↗
47. 10.1021/acsami.1c1629610.1021/acsami.1c16296 ↗
48. 10.1038/s41598-024-65230-x10.1038/s41598-024-65230-x ↗
49. 10.1039/C8EE01286E10.1039/C8EE01286E ↗
50. Hikima K. · Communicat. Chem. · 2022 · 5 · 52
51. 10.1103/PhysRevB.65.11310210.1103/PhysRevB.65.113102 ↗
52. 10.1039/C8CS00426A10.1039/C8CS00426A ↗
53. 10.1038/s41563-022-01278-210.1038/s41563-022-01278-2 ↗
54. 10.1038/s41563-024-01833-z10.1038/s41563-024-01833-z ↗
55. 10.1002/batt.20180012610.1002/batt.201800126 ↗
56. 10.1371/journal.pone.004918210.1371/journal.pone.0049182 ↗
57. 10.1103/PRXEnergy.2.04301010.1103/PRXEnergy.2.043010 ↗
58. 10.1149/1.183757110.1149/1.1837571 ↗
59. 10.1111/j.1945-5100.2008.tb00627.x10.1111/j.1945-5100.2008.tb00627.x ↗
60. 10.1016/j.joule.2018.07.02110.1016/j.joule.2018.07.021 ↗
61. 10.1016/j.jpowsour.2012.04.03110.1016/j.jpowsour.2012.04.031 ↗
62. 10.1002/admi.20200027610.1002/admi.202000276 ↗
63. a)Z.Liang presented atLithium Battery Discussions Arcachon June2023;
64. b)A. M.Baubaid Z.Liang L.Alff G.Cherkashinin unpublished.
65. 10.1016/0167-2738(94)90267-410.1016/0167-2738(94)90267-4 ↗
66. 10.1038/ncomms1210810.1038/ncomms12108 ↗
67. 10.1038/s41560-024-01664-x10.1038/s41560-024-01664-x ↗
68. 10.1021/cm501480b10.1021/cm501480b ↗
69. 10.1021/acs.jpclett.0c0077810.1021/acs.jpclett.0c00778 ↗
70. 10.1016/j.mseb.2014.11.01410.1016/j.mseb.2014.11.014 ↗
71. 10.1107/S160057751501082610.1107/S1600577515010826 ↗
72. 10.1016/j.apsusc.2005.01.11010.1016/j.apsusc.2005.01.110 ↗