Characteristics and performance of lanthanum gallate electrolyte-supported SOFC under ethanol steam and hydrogen
Source abstract
Abstract
This study is focused on the electrochemical performance of perovskite-type materials based on doped LaGaO(3). La(0.8)Sr(0.2)Ga(0.8)Mg(0.2)O(3-delta) (LSGM) and La(0.8)Sr(0.2)Ga(0.8)Mg(0.115)Co(0.085)O(3-delta) (LSGMC) were used as electrolytes and (Pr(0.7)Ca(0.3))(0.9)MnO(3) (PCM) and La(0.75)Sr(0.25)Cr(0.25)Mn(0.5)O(3-delta) (LSCM) as cathode and anode material, respectively. LSGM and LSGMC electrolytes were prepared by tape casting with a thickness of about 600 mu m. The performance of LSCM/LSGMC/PCM was slightly superior to that obtained on LSCM/LSGM/PCM at different temperatures in both humidified hydrogen and ethanol steam atmospheres, good values of power Output in LSCM/LSGMC/PCM were 182 and 169 mW cm(-2) using humidified hydrogen and ethanol steam as fuel, respectively, and oxygen as oxidant at 850 degrees C. Cell stability tests indicate no significant degradation in performance after 60h of cell testing when LSCM anode was exposed to ethanol steam at 750 degrees C. Almost no carbon deposits were detected after testing in ethanol steam at 750 degrees C for >60 h on the LSCM anodes, Suggesting that carbon deposition was limited during cell operation. (c) 2008 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Catalytic Processes in Materials Science · Catalysis and Oxidation Reactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
2. Ishihara · Solid State Ionics · 2006 · 177 · 194910.1016/j.ssi.2006.01.044 ↗
3. Polini · J. Eur. Ceram. Soc. · 2007 · 27 · 429110.1016/j.jeurceramsoc.2007.02.147 ↗
4. Polini · J. Eur. Ceram. Soc. · 2004 · 24 · 136510.1016/S0955-2219(03)00592-2 ↗
5. Lu · Solid State Ionics · 2002 · 152/153 · 39310.1016/S0167-2738(02)00346-6 ↗
6. Liu · Solid State Ionics · 2003 · 158 · 1110.1016/S0167-2738(02)00769-5 ↗
7. Koh · Solid State Ionics · 2002 · 149 · 15710.1016/S0167-2738(02)00243-6 ↗
8. Wang · J. Power Sources · 2003 · 122 · 12210.1016/S0378-7753(03)00438-5 ↗
9. Atkinson · Nat. Mater. · 2004 · 3 · 1710.1038/nmat1040 ↗
10. Primdahl · J. Electrochem. Soc. · 2001 · 148 · A7410.1149/1.1344519 ↗
11. Singhal · 2004
12. Matsuzaki · Solid State Ionics · 2000 · 132 · 26110.1016/S0167-2738(00)00653-6 ↗
13. Zhu · Mater. Sci. Eng. A · 2003 · 362 · 22810.1016/S0921-5093(03)00620-8 ↗
14. Park · Nature · 2000 · 404 · 26510.1038/35005040 ↗
15. Perry · Nature · 1999 · 400 · 64910.1038/23220 ↗
16. Bartholomew · Catal. Rev. Sci. Eng. · 1982 · 24 · 6710.1080/03602458208079650 ↗
17. Baker · Carbon · 1989 · 27 · 31510.1016/0008-6223(89)90062-6 ↗
18. Steele · Solid State Ionics · 1996 · 86–88 · 122310.1016/0167-2738(96)00291-3 ↗
19. Hernadi · Appl. Catal. A · 2000 · 199 · 24510.1016/S0926-860X(99)00561-X ↗
20. Koh · Solid State Ionics · 2002 · 149 · 15710.1016/S0167-2738(02)00243-6 ↗
21. Ishihara · J. Eur. Ceram. Soc. · 2004 · 24 · 132910.1016/S0955-2219(03)00508-9 ↗
22. Ishihara · Chem. Mater. · 1999 · 11 · 208110.1021/cm981145w ↗
23. Mori · J. Am. Ceram. Soc. · 2001 · 84 · 257310.1111/j.1151-2916.2001.tb01056.x ↗
24. 2003 · vol. 2003-07
25. Sfeir · J. Catal. · 2001 · 202 · 22910.1006/jcat.2001.3286 ↗
26. Sfeir · J. Power Sources · 2003 · 118 · 27610.1016/S0378-7753(03)00099-5 ↗
27. Tao · Nat. Mater. · 2003 · 2 · 32010.1038/nmat871 ↗
28. Tao · J. Electrochem. Soc. · 2004 · 151 · A25210.1149/1.1639161 ↗
29. Bo Huang · J. Power Sources · 2007 · 167 · 3910.1016/j.jpowsour.2007.02.022 ↗
30. Du · 2005 · 1127
31. Tao · J. Phys. Chem. B · 2006 · 110 · 2177110.1021/jp062376q ↗