journal article·2015-10

Tin and iron co-doping strategy for developing active and stable oxygen reduction catalysts from SrCoO3−δ for operating below 800 °C

Yubo Chen, Baoming Qian, Zongping Shao

Publisher page

Abstract

Abstract SrCoO 3−δ has long been a promising catalyst for the oxygen reduction reaction in solid oxide fuel cells (SOFCs). However, its rather unstable cubic phase structure greatly hinders its practical application. Stabilizing the simple cubic phase structure of SrCoO 3−δ while preserving a suitable oxygen reduction activity is an important topic of research. Herein, we propose a Sn and Fe co-doping strategy for tuning the B-site of SrCoO 3−δ to stabilize its oxygen vacancy-disordered cubic lattice structure at the operating temperatures of intermediate-temperature SOFCs (600–800 °C). Fe doping can greatly increase the solubility of Sn in SrCoO 3−δ , which mainly acts as the dopant for cubic phase structure stabilization. Materials with a nominal composition of SrCo 0.6 (Fe 0.4−x Sn x )O 3−δ (x = 0–0.15) are designed, and the solubility of Sn in SrCoO 3−δ can reach x = 0.1. For the first time, we prepare a phase-pure Sn-doped and SrCoO 3−δ -based cubic perovskite oxide of SrCo 0.6 (Fe 0.3 Sn 0.1 )O 3−δ with long-term cubic structure stability. More importantly, the Sn doping does not harm the oxygen reduction activity of SrCo 0.6 Fe 0.4 O 3−δ , and the electrode composed of SrCo 0.6 (Fe 0.3 Sn 0.1 )O 3−δ possesses a low polarization resistance of ∼0.1 Ω cm 2 at 600 °C. A 400-h-long stability test demonstrates that the SrCo 0.6 (Fe 0.3 Sn 0.1 )O 3−δ material is a promising oxygen reduction catalyst for SOFCs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Solid oxide fuel cells10.1039/b105764m ↗
2. Materials for fuel-cell technologies10.1038/35104620 ↗
3. Intermediate temperature solid oxide fuel cells10.1039/b612060c ↗
4. Solid oxide fuel cells-a challenge for materials chemists?10.1039/B603620A ↗
5. Oxygen transport in selected nonstoichiometric perovskite-structure oxides10.1016/0167-2738(92)90435-R ↗
6. Simulation of thermal stresses in anode-supported solid oxide fuel cell stacks. part I: probability of failure of the cells10.1016/j.jpowsour.2008.12.050 ↗
7. A single-chamber SOFC stack operating in engine exhaust10.1149/1.2824502 ↗
8. Materials for solid oxide fuel cells10.1021/cm902640j ↗
9. New chemical systems for solid oxide fuel cells10.1021/cm902687z ↗
10. Electrochemical performances of spinel oxides as cathodes for intermediate temperature solid oxide fuel cells10.1016/j.ijhydene.2012.10.095 ↗
11. Praseodymium-cerium oxide thin film cathodes: study of oxygen reduction reaction kinetics10.1007/s10832-011-9678-z ↗
12. A High-performance cathode for the next generation of solid-oxide fuel cells10.1038/nature02863 ↗
13. Novel BaCo0.7Fe0.3−yNbyO3−δ (y=0–0.12) as a cathode for intermediate temperature solid oxide fuel cell10.1016/j.elecom.2009.02.034 ↗
14. Novel B-site ordered double perovskite Ba2Bi0.1Sc0.2Co1.7O6−δ for highly efficient oxygen reduction reaction10.1039/C0EE00451K ↗
15. Surprisingly high activity for oxygen reduction reaction of selected oxides lacking long oxygen-ion diffusion paths at intermediate temperatures: A case study of cobalt-free BaFeO3−δ10.1021/am502240m ↗
16. Investigation of Ba1−xSrxCo0.8Fe0.2O3−δ as cathodes for low-temperature solid oxide fuel cells both in the absence and presence of CO210.1016/j.jpowsour.2008.06.088 ↗
17. Visualization by neutron diffraction of 2D oxygen diffusion in the Sr0.7Ho0.3CoO3−δ cathode for solid-oxide fuel cells10.1021/am501297z ↗
18. Ceramic microstructure and oxygen permeability of SrCo(Fe, M)O3 (M = Cu or Cr) perovskite membranes10.1149/1.1838467 ↗
19. Perovskite Sr1–xCexCoO3−δ (0.05 ≤ x ≤ 0.15) as superior cathodes for intermediate temperature solid oxide fuel cells10.1021/am3029238 ↗
20. High-performance SrNb0.1Co0.9−xFexO3−δ perovskite cathodes for low-temperature solid oxide fuel cells10.1039/C4TA03208J ↗
21. Oxygen permeation studies of SrCo0.8Fe0.2O3−δ10.1016/0167-2738(94)00296-5 ↗
22. Double-site yttria-doped Sr1−xYxCo1−yYyO3−δ perovskite oxides as oxygen semi-permeable membranes10.1016/j.jallcom.2008.06.120 ↗
23. SrCo0.85Fe0.1P0.05O3−δ Perovskite as a cathode for intermediate-temperature solid oxide fuel cells10.1039/c3ta12781h ↗
24. SrCo0.7Fe0.2Ta0.1O3−δ Perovskite as a cathode material for intermediate-temperature solid oxide fuel cells10.1016/j.ijhydene.2014.05.150 ↗
25. Remarkable dependence of electrochemical performance of SrCo0.8Fe0.2O3−δ on A-site nonstoichiometry10.1039/c2cp41060e ↗
26. Re-evaluation of Ba0.5Sr0.5Co0.8Fe0.2O3−δ perovskite as oxygen semi-permeable membrane10.1016/j.memsci.2007.01.003 ↗
27. Structure and oxygen stoichiometry of SrCo0.8Fe0.2O3−δ and Ba0.5Sr0.5Co0.8Fe0.2O3−δ10.1016/j.ssi.2006.03.041 ↗
28. Structural behavior of oxygen permeable SrFe0.2Co0.8Ox ceramic membranes with and without pO2 gradients10.1111/j.1551-2916.2005.00171.x ↗
29. Tin-doped perovskite mixed conducting membrane for efficient air separation10.1039/C4TA00926F ↗
30. BaCo0.6Fe0.3Sn0.1O3−δ perovskite as a new superior oxygen reduction electrode for intermediate-to-low temperature solid oxide fuel cells10.1039/C4TA02869D ↗
31. The chemical stability and conductivity of BaCe0.9−xYxSn0.1O3−δ solid proton conductor for SOFC10.1016/j.jallcom.2008.12.120 ↗
32. Characteristics of SrCo1−xSnxO3−δ cathode materials for use in solid oxide fuel cells10.1016/j.ssi.2012.08.020 ↗
33. Preparation and characterization of SrCo0.8Fe0.2O3−δ–SrSnO3 oxygen-permeable composite membrane10.1016/j.ssi.2003.12.002 ↗
34. Mechanical stability and transport properties of the Sn-promoted SrCo0.8Fe0.2O3−δ ceramic membrane10.1016/j.memsci.2006.12.015 ↗
35. Studies on electrical properties of La0.8Sr0.2Ga0.8Mg0.2O2.80 (LSGM) and LSGM–SrSn1−xFexO3 (x =0.8; 0.9) composites and their chemical reactivity10.1016/j.electacta.2004.08.039 ↗
36. Electrical conductivity and oxygen sensing behavior of SrSn1−xFexO3−δ (x=0–0.2)10.1016/j.jallcom.2010.07.005 ↗
37. Role of silver current collector on the operational stability of selected cobalt-containing oxide electrodes for oxygen reduction reaction10.1016/j.jpowsour.2012.03.019 ↗
38. EXPGUI, A graphical user interface for GSAS10.1107/S0021889801002242 ↗
39. Phase transitions in the SrSnO3–SrFeO3 solid solutions: X-ray diffraction and mössbauer studies10.1016/S0022-4596(03)00258-5 ↗
40. Oxygen nonstoichiometry, the defect equilibrium model and thermodynamic quantities of the Ruddlesden-Popper oxide Sr3Fe2O7−δ10.1039/C4CP05719H ↗
41. Electrical conductivity relaxation measurements: statistical investigations using sensitivity analysis, optimal experimental design and ECRTOOLS10.1016/j.ssi.2013.03.020 ↗
42. Kresse · 2003
43. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
44. First-principles modelling of complex perovskite (Ba1−xSrx)(Co1−yFey)O3−δ for solid oxide fuel cell and gas separation membrane applications10.1039/c0ee00096e ↗
45. Investigation of mixed conductor BaCo0.7Fe0.3−xYxO3−δ with high oxygen permeability10.1021/jp106220z ↗
46. A low-operating-temperature solid oxide fuel cell in hydrocarbon-air mixtures10.1126/science.288.5473.2031 ↗
47. Improvement of a reduction-resistant Ce0.8Sm0.2O1.9 electrolyte by optimizing a thin BaCe1−xSmxO3−δ layer for intermediate-temperature SOFCs10.1016/j.ssi.2004.12.007 ↗