journal article·2012-06

Screen-printed (La,Sr)CrO3 coatings on ferritic stainless steel interconnects for solid oxide fuel cells using nanopowders prepared by means of ultrasonic spray pyrolysis

Tomasz Brylewski, Jaroslaw Dabek, Kazimierz Przybylski, Jerzy Morgiel, Mieczyslaw Rekas

Publisher page

Abstract

Abstract In order to protect the cathode from chromium poisoning and improve electrical resistance, a perovskite (La,Sr)CrO3 coating was deposited on the surface of a DIN 50049 ferritic stainless steel by means of the screen-printing method, using a paste composed of an ultra-fine powder prepared via ultrasonic spray pyrolysis. Investigations of the oxidation process of the coated steel in air and the Ar–H2–H2O gas mixture at 1073 K for times up to 820 h showed high compactness of the protective film, good adhesion to the metal substrate, as well as area specific resistance (ASR) at a level acceptable for metallic SOFC interconnect materials. The microstructure, nanostructure, phase composition of the thick film, and in particular the film/substrate interface, were examined via chemical analyses by means of SEM-EDS and TEM-SAD. It was shown that the (La,Sr)CrO3 coating interacts with the steel during long-term thermal oxidation in the afore-mentioned conditions and intermediate, chromia-rich and/or spinel multilayer interfacial zones are formed. Cr-vaporization tests showed that the (La,Sr)CrO3 coating may play the role of barriers that decrease the volatilization rate of chromia species.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Singhal · 2003
2. Quadakkers · Mater. High Temp. · 2003 · 20 · 115
3. Yang · J. Electrochem. Soc. · 2003 · 150 · A118810.1149/1.1595659 ↗
4. Fergus · Mater. Sci. Eng. · 2005 · A397 · 27110.1016/j.msea.2005.02.047 ↗
5. Chen · Solid State Ionics · 2005 · 176 · 42510.1016/j.ssi.2004.10.004 ↗
6. Brylewski · Solid State Ionics · 2001 · 143 · 13110.1016/S0167-2738(01)00863-3 ↗
7. Cabouro · J. Power Sources · 2006 · 156 · 3910.1016/j.jpowsour.2005.08.039 ↗
8. Shaigan · J. Power Sources · 2010 · 195 · 152910.1016/j.jpowsour.2009.09.069 ↗
9. Kadowaki · Solid State Ionics · 1993 · 67 · 6510.1016/0167-2738(93)90310-Y ↗
10. Yang · J. Electrochem. Soc. · 2005 · 152 · A189610.1149/1.1990462 ↗
11. Montero · J. Electrochem. Soc. · 2009 · 156 · B18810.1149/1.3025914 ↗
12. Hua · J. Power Sources · 2008 · 185 · 41910.1016/j.jpowsour.2008.06.055 ↗
13. Hilpert · J. Electrochem. Soc. · 1996 · 143 · 364210.1149/1.1837264 ↗
14. Zhu · Mater. Sci. Eng. · 2003 · A348 · 22710.1016/S0921-5093(02)00736-0 ↗
15. Kurokawa · Solid State Ionics · 2007 · 178 · 28710.1016/j.ssi.2006.12.010 ↗
16. Brylewski · Ann. Chim. Sci. Mat. · 2008 · 33 · 75
17. Yang · J. Electrochem. Soc. · 2004 · 151 · 66910.1149/1.1810393 ↗
18. Barbucci · 2006 · 329
19. Yang · J. Electrochem. Soc. · 2006 · 153 · A185210.1149/1.2239371 ↗
20. Larring · J. Electrochem. Soc. · 2000 · 147 · 325110.1149/1.1393891 ↗
21. Yang · Electrochem. Solid State Lett. · 2005 · 8 · A16810.1149/1.1854122 ↗
22. Gannon · Int. J. Hydrogen Energy · 2008 · 33 · 399110.1016/j.ijhydene.2007.12.009 ↗
23. Fontana · J. Power Sources · 2007 · 171 · 65210.1016/j.jpowsour.2007.06.255 ↗
24. Qu · J. Power Sources · 2004 · 138 · 16210.1016/j.jpowsour.2004.06.063 ↗
25. Fergus · Solid State Ionics · 2004 · 171 · 110.1016/j.ssi.2004.04.010 ↗
26. Sujatha Devi · J. Solid State Chem. · 1992 · 98 · 23710.1016/S0022-4596(05)80231-2 ↗
27. Zhu · Surf. Coat. Technol. · 2004 · 177 · 6510.1016/j.surfcoat.2003.05.003 ↗
28. Mikkelsen · Surf. Coat. Technol. · 2007 · 202 · 126210.1016/j.surfcoat.2007.07.046 ↗
29. Gindorf · Steel Res. Int. · 2001 · 72 · 52810.1002/srin.200100163 ↗
30. Linderoth · Surf. Coat. Technol. · 1996 · 80 · 18510.1016/0257-8972(95)02708-4 ↗
31. Lee · J. Power Sources · 2006 · 157 · 70910.1016/j.jpowsour.2005.12.030 ↗
32. Kajimura · Solid State Ionics · 1995 · 82 · 10710.1016/0167-2738(95)00200-P ↗
33. Hwang · J. Am. Ceram. Soc. · 2005 · 88 · 327510.1111/j.1551-2916.2005.00591.x ↗
34. Przybylski · Mater. Trans. · 2011 · 52 · 34510.2320/matertrans.MB201013 ↗
35. Brylewski · Mater. Chem. Phys. · 2003 · 81 · 43410.1016/S0254-0584(03)00041-5 ↗
36. Wojciechowski · Solid State Ionics · 2003 · 157 · 34110.1016/S0167-2738(02)00231-X ↗
37. Przybylski · 2000 · vol. 15, Part II
38. Chevalier · J. Appl. Electrochem. · 2009 · 39 · 52910.1007/s10800-008-9726-9 ↗
39. Devi · J. Solid State Chem. · 1992 · 98 · 23710.1016/S0022-4596(05)80231-2 ↗
40. Azaroff · 1968
41. Lu · J. Power Sources · 2008 · 178 · 28210.1016/j.jpowsour.2007.11.105 ↗
42. Kofstad · 1988
43. Rapp · Corrosion · 1965 · 21 · 38210.5006/0010-9312-21.12.382 ↗
44. 1986
45. Kurokawa · Solid State Ionics · 2004 · 168 · 1310.1016/j.ssi.2004.02.008 ↗
46. Cox · Philos. Mag. · 1972 · 26 · 83910.1080/14786437208226960 ↗
47. Yurek · 1985
48. Peck · Solid State Ionics · 1999 · 123 · 5910.1016/S0167-2738(99)00088-0 ↗
49. Miyoshi · J. Solid State Chem. · 2004 · 177 · 411210.1016/j.jssc.2004.04.054 ↗
50. Maruyama · 1995 · 889
51. Mori · Solid State Ionics · 2000 · 135 · 74310.1016/S0167-2738(00)00372-6 ↗