journal article·2007-05

Performance of La0.75Sr0.25Cr0.5Mn0.5O3−δ perovskite-structure anode material at lanthanum gallate electrolyte for IT-SOFC running on ethanol fuel

Bo Huang, S.R. Wang, R.Z. Liu, X.F. Ye, H.W. Nie, X.F. Sun, T.L. Wen

Journal of Power Sources· Volume 167· Issue 1
Publisher page

Abstract

Abstract Perovskite-structure La 0.75 Sr 0.25 Cr 0.5 Mn 0.5 O 3− δ (LSCM) powders were prepared using a simple combustion process. Thermal analysis was carried out on the perovskite precursor to investigate the oxide-phase formation. The structural phase of the powders was determined by X-ray diffraction. These results showed that the decomposition of the precursors occurs in a two-step reaction and temperatures higher than 1100 °C are required for these decomposition reactions. For the electrochemical characterization, LSCM anode materials and (Pr 0.7 Ca 0.3 ) 0.9 MnO 3 (PCM) cathode materials were screen-printed on two sides of dense La 0.8 Sr 0.2 Ga 0.8 Mg 0.2 O 3 (LSGM) electrolyte layers prepared by tape casting with a thickness of about 600 μm, respectively. The morphology of the screen-printed La 0.75 Sr 0.25 Cr 0.5 Mn 0.5 O 3− δ perovskite thick films (65 μm) was investigated by field emission scanning electron microscope and showed a porous microstructure. In addition, fuel cell tests were carried out using humidified hydrogen or ethanol stream as fuel and oxygen as oxidant. The performance of the conventional electrolyte-supported cell LSCM/LSGM/PCM while operating on humidified hydrogen was modest with a maximum power density of 165, 99 and 62 mW cm −2 at 850, 800 and 750 °C, respectively, the corresponding values for the cell while operating on ethanol stream was 160, 101 and 58 mW cm −2 , respectively. Cell stability tests indicate no significant degradation in performance has been observed after 60 h of cell testing when LSCM anode was exposed to ethanol steam at 750 °C, suggesting that carbon deposition was limited during cell operation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
2. Lu · Solid State Ionics · 2002 · 152–153 · 39310.1016/S0167-2738(02)00346-6 ↗
3. Liu · Solid State Ionics · 2003 · 158 · 1110.1016/S0167-2738(02)00769-5 ↗
4. Koh · Solid State Ionics · 2002 · 149 · 15710.1016/S0167-2738(02)00243-6 ↗
5. Wang · J. Power Sources · 2003 · 122 · 12210.1016/S0378-7753(03)00438-5 ↗
6. Bartholomew · Catal. Rev. Sci. Eng. · 1982 · 24 · 6710.1080/03602458208079650 ↗
7. Baker · Carbon · 1989 · 27 · 31510.1016/0008-6223(89)90062-6 ↗
8. Steele · Solid State Ionics · 1996 · 86–88 · 122310.1016/0167-2738(96)00291-3 ↗
9. Hernadi · Appl. Catal. A · 2000 · 199 · 24510.1016/S0926-860X(99)00561-X ↗
10. Koh · Solid State Ionics · 2002 · 149 · 15710.1016/S0167-2738(02)00243-6 ↗
11. Ishihara · J. Am. Chem. Soc. · 1994 · 116 · 380110.1021/ja00088a016 ↗
12. Kim · J. Power Sources · 2001 · 93 · 27910.1016/S0378-7753(00)00567-X ↗
13. Sora · Solid State Ionics · 2005 · 176 · 8110.1016/j.ssi.2004.06.002 ↗
14. Ishihara · Solid State Ionics · 1998 · 113–115 · 59310.1016/S0167-2738(98)00390-7 ↗
15. Goodenough · Nature · 2000 · 404 · 82110.1038/35009177 ↗
16. Mori · J. Am. Ceram. Soc. · 2001 · 84 · 257310.1111/j.1151-2916.2001.tb01056.x ↗
17. 2003 · 803
18. Sfeir · J. Catal. · 2001 · 202 · 22910.1006/jcat.2001.3286 ↗
19. Sfeir · J. Power Sources · 2003 · 118 · 27610.1016/S0378-7753(03)00099-5 ↗
20. Tao · Nat. Mater. · 2003 · 2 · 32010.1038/nmat871 ↗
21. Tao · J. Electrochem. Soc. · 2004 · 151 · A25210.1149/1.1639161 ↗
22. Jain · Combust. Flame · 1981 · 40 · 7110.1016/0010-2180(81)90111-5 ↗
23. Ye · J. Power Sources · 2007 · 164 · 20310.1016/j.jpowsour.2006.10.056 ↗
24. Baythoun · J. Mater. Sci. · 1982 · 17 · 275710.1007/BF00543914 ↗
25. Du · 2005 · 1127
26. de Souza · J. Electrochem. Soc. · 1997 · 144 · L3510.1149/1.1837484 ↗
27. Kim · J. Electrochem. Soc. · 1999 · 146 · 6910.1149/1.1391566 ↗