Source abstract
Abstract
High Resolution Image Download MS PowerPoint Slide Li x La (1– x )/3 NbO 3 is an A-site-deficient perovskite material that exhibits structure-dependent ionic conductivity. La 1/3 NbO 3 has a larger unit cell volume, lower concentration of La 3+ ions, and higher concentration of intrinsic vacancies than La 2/3 TiO 3 . As such, it should exhibit higher Li ion conductivity and, therefore, be a good candidate for all ceramic Li secondary batteries or fast Li ion transport solid-state electrolyte batteries. However, experimental observations show otherwise. Information on the local atomic arrangements would facilitate the analysis of the gap between the theoretical and experimental results. Ab initio density functional theory calculations are useful for calculating the atomic arrangements and energies. However, because of cell size limitations, long-range ordering in La/Li/vacancy arrangements cannot be observed using ab initio calculations. In this study, cluster expansion and Monte Carlo simulations were utilized to bridge this gap. The computational results reproduce the stacking of alternate La-rich and La-poor layers along the c -axis, consistent with the experimental data. In addition, two possible modulated structures for the La-rich layers were discovered. These should help explain the lower-than-expected ionic conductivity and the possible Li ion migration pathways in the material. Based on the presented Monte Carlo simulations, we conclude that the two types of low-energy structures, the closed and striped arrangements, may coexist in the real system. The modulated structures in experimental studies are likely to be numberless nanodomains composed of these two arrangements. If the majority of the structure shows a closed arrangement at room temperature, most of the Li ions will be trapped at the center of the periodic units in the closed arrangement. This could explain the lower-than-expected Li ion conductivity in Li x La (1– x )/3 NbO 3 .
Source: openalex_inverted_index · Quality: baseline
Affiliations
Department of Advanced Ceramics, Nagoya Institute of Technology, Gokiso, Showa, Nagoya, Aichi 466-8555, Japan
MaDIS/CMI2, National Institute for Materials Science (NIMS), 1-2-1, Sengen, Tsukuba, Ibaraki 305-0047, Japan
Unit of Elements Strategy Initiative for Catalysts & Batteries (ESICB), Kyoto University, Katsura, Saikyo-ku, Kyoto 615-8520, Japan
Frontier Research Institute for Materials Science (FRIMS), Nagoya Institute of Technology, Gokiso, Showa, Nagoya, Aichi 466-8555, Japan