Distinct Clockwise Capacitance−Voltage Hysteresis in Aminopropyl-silsesquioxane Thin Films
Source abstract
Abstract
Aminopropyl-silsesquioxane resins and thin films were synthesized from aminopropyltrimethoxysilane (APTMS). To investigate the changes in the molecular structure of the film with increasing curing temperature, Fourier transform infrared spectroscopy (FT-IR) was performed. The dielectric properties of the thin films were investigated by capacitance−voltage (C−V) measurements in a metal−insulator−semiconductor (MIS) structure. To explain the spectral changes in the FT-IR results, it is proposed that the Si−OH and aminopropyl groups freely exist without hydrogen bonding interactions in the curing temperature range 100−200 °C, while molecular structures such as N(Si≡) 3, N(Si≡) 2, and O(Si≡) 2 are formed at higher temperatures in the range 250−300 °C. The dielectric constant values and dissipation factors are regarded as being suitable for electronic applications, e.g., the gate insulators of organic thin film transistor (OTFT) devices. Interestingly, amphoteric charge trap behavior, such as a distinct clockwise C−V hysteresis, was observed in the sample cured at 300 °C. It is proposed that this originates from the coexistence of N(Si≡) 2 and E′ centers in the cured films, into which positive charges or negative charges originating from the metal gate electrode are trapped, depending on the polarity of the applied electric field. It seems that the nitrogen-related molecular defects act as electron trap centers in the aminopropyl-silsesquioxane thin films.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemistry, Chonnam National University, Gwangju-si, 500-575, Korea
References (28)
Show source-provided references
1. Gelink G. H. · Nat. Mater. · 2004 · 3 · 10610.1038/nmat1061 ↗
2. Sheraw C. D. · Appl. Phys. Lett. · 2002 · 80 · 108810.1063/1.1448659 ↗
3. Zhu Z. T. · Appl. Phys. Lett. · 2002 · 81 · 464310.1063/1.1527233 ↗
4. Baude P. F. · Appl. Phys. Lett. · 2003 · 82 · 396410.1063/1.1579554 ↗
5. Facchetti A. · Adv. Mater. · 2005 · 17 · 170510.1002/adma.200500517 ↗
6. Bao Z. · Adv. Funct. Mater. · 2002 · 12 · 52610.1002/1616-3028(20020805)12:8<526::AID-ADFM526>3.0.CO;2-S ↗
7. Choi C. G. · Org. Electron. · 2007 · 8 · 74310.1016/j.orgel.2007.06.006 ↗
8. Wu Y. · Appl. Phys. Lett. · 2006 · 89 · 01350510.1063/1.2219143 ↗
9. Liu P. · J. Am. Chem. Soc. · 2006 · 128 · 455410.1021/ja060620l ↗
10. Zhao N. · IEEE Trans. Electron Devices · 2005 · 52 · 215010.1109/TED.2005.856172 ↗
11. Satoshi M. · J. Mater. Chem. · 1999 · 9 · 59110.1039/a807068g ↗
12. Saal K. · Mater. Lett. · 2006 · 60 · 183310.1016/j.matlet.2005.12.035 ↗
13. Kim J. H. · Macromolecules · 2003 · 36 · 618310.1021/ma034314t ↗
14. Ishida H. · J. Polym. Sci. · 1980 · 18 · 233
15. Scarlete M. · Chem. Mater. · 2001 · 13 · 65510.1021/cm000522d ↗
16. Choong Kwet Yive N. S. · Chem. Mater. · 1992 · 4 · 14110.1021/cm00019a029 ↗
17. Unpublished results. The existence of a defect structure such as {≡Si−O•+•Si≡} is usually confirmed by the negative flat band shift (ΔVfb) in the C−V measurements. In our previous studies, most of the spin-on glass thin films with high tensile stress which were synthesized in our laboratory showed a negative ΔVfb.
18. Atkins, P.; de Paula, J.Atkins’ Physical Chemistry,7thed.Oxford University Press:Oxford, 2002; pp691−693.
19. Sze S. M. · 2007
20. Nicollian E. H. · 1982
21. Chen, C. H.Study on Amorphous Silicon Carbide Barrier Dielectric Materials. Master’s thesis, National Sun Yat-Sen Univeristy, Taiwan, 2002; p22.
22. Tian H. · Appl. Phys. Lett. · 2006 · 89 · 14290510.1063/1.2358934 ↗
23. Tomar M. S. · Appl. Phys. Lett. · 2003 · 83 · 34110.1063/1.1592308 ↗
24. Lisca M. · Appl. Surf. Sci. · 2006 · 252 · 454910.1016/j.apsusc.2005.07.149 ↗
25. PZT film preparation. The PZT precursor solution was obtained from INOSTEK Inc. (Korea). The solution was spin-coated at 4000 rpm and 30 s on the platinum bottom electrode. Then the film was dried at 80 °C on a hot plate for 5 min in an air atmosphere to remove the remaining solvents. This procedure was iterated three times, giving a thickness of about 1 μm. The film was annealed at 450 °C for 10 min in a quartz tube in an air atmosphere and finally annealed at 700 °C for 30 min in the same condition.
26. Lee E. C. · Phys. Rev. B · 2002 · 66 · 23320510.1103/PhysRevB.66.233205 ↗
27. Boero M. · Phys. Rev. Lett. · 1997 · 78 · 88710.1103/PhysRevLett.78.887 ↗
28. Miura Y. · Mater. Res. Soc. Symp. Proc. · 2000 · 592 · 26310.1557/PROC-592-263 ↗