High-density polyethylene facial implants show surface oxidation in SEM and EDX examination: A pilot study

G.F. Draenert, M. Doeblinger, M. Draenert, M. Gosau

Acta Biomaterialia· Volume 5· Issue 4
Publisher page

Abstract

Previous histopathological studies on explanted Medpor high-density polyethylene (HDPE) facial implants indicated signs of material destruction and claimed to observe phagocytized HDPE particles within the tissue samples beside the usual type IV reaction with severe fibrosis. We examined new and explanted Medpor material with scanning electron microscopy (SEM) and energy-dispersive X-ray analysis (EDX). The implant surface of three patient-derived specimens showed significantly higher oxygenation in EDX analysis and morphological changes in SEM compared to the new unused material directly after opening of the package and after 1 year of exposure to air. Our preliminary findings indicate a possible oxidative biocorrosion in HDPE surgical implants. Further studies should confirm these pilot project results.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental Implant Techniques and Outcomes · Facial Nerve Paralysis Treatment and Research · Facial Rejuvenation and Surgery Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Nomenclature of regular single-strand organic polymers (IUPAC Recommendations 2002); pure and applied chemistry
2. Analysis of the postoperative outcome in 405 cases of orbital fracture using 2 synthetic orbital implants10.1097/01.sap.0000199173.73610.bc ↗
3. Clinical outcome of 285 Medpor grafts used for craniofacial reconstruction10.1097/01.scs.0000168761.46700.dc ↗
4. Facial augmentation with porous polyethylene (Medpor®)-histological evidence of intense foreign body reaction10.1002/jbm.b.31072 ↗
5. Characterisation of wear particles produced by metal on metal and ceramic on metal hip prostheses under standard and microseparation simulation10.1007/s10856-006-0015-z ↗
6. Corrosion behavior of copper/LDPE nanocomposites in simulated uterine solution10.1016/j.biomaterials.2004.08.003 ↗
7. Surface oxidation of polyethylene fiber reinforced polyolefin biomedical composites and its effect on cell attachment10.1023/A:1014789815441 ↗
8. Mechanism of polyethylene oxidation10.1002/app.1964.070080419 ↗
9. Biodegradation of low-density polyethylene, polystyrene, polyvinyl chloride, and urea formaldehyde resin buried under soil for over 32 years10.1002/app.1995.070561309 ↗
10. Biodegradation of polyethylene by the thermophilic bacterium Brevibacillus borstelensis10.1111/j.1365-2672.2005.02553.x ↗
11. Unacceptable biodegradation of polyethylene in vivo10.1016/0142-9612(96)83282-0 ↗
12. Biodegradation of polyethylene foils by bacterial and liver homogenates10.1016/0142-9612(90)90049-V ↗
13. Interaction of oxidation and crosslinking in gamma-irradiated ultrahigh molecular weight polyethylene10.1002/jbm.10203 ↗
14. Effect of lipid absorption on wear and compressive properties of unirradiated and highly crosslinked UHMWPE: an in vitro experimental model10.1016/j.biomaterials.2003.11.049 ↗
15. Wear behaviour of crosslinked polyethylene assessed in vitro under severe conditions10.1016/j.biomaterials.2004.07.070 ↗
16. Spinal implant debris-induced osteolysis10.1097/00007632-200310151-00006 ↗
17. Oxidation-resistant and wear-resistant polyethylenes for human joint replacement and methods for making them