Crystallization trend in STO-seeded sputtered PZT thin films: Effects of seed layer thickness and post-annealing temperature
Source abstract
Abstract
Abstract Based on the results of X-ray diffractometry (XRD) and analytical scanning/transmission electron microscopy (S/TEM), the crystallization trend and local chemistry of sputtered PZT films on SrTiO 3 (STO) coated corning glass substrates have been scrutinized as functions of STO layer thickness (∼20–150 nm) and post-annealing temperature (450 C–650 °C). It is shown that as a seed layer, STO thin films promote perovskite PZT nucleation at the PZT/STO interface at a temperature of ∼450 °C. Irrespective of STO seed layer thickness, PZT films evolve as a bi-layered structure comprising of tetragonal perovskite and disordered fcc fluorite upon post-annealing. The perovskite crystals are found to be enriched with Pb and lean in Zr and oxygen than fluorite structures. During the post-crystallization growth, Zr atoms get preferentially segregated from perovskite structures and accumulate in top fluorite zone resulting in Zr-enrichment in the latter. Thinner STO seed layers are observed to be more effective in realizing better perovskite growth while crystallographic orientation selection of perovskite is dependent on both seed layer thickness and post-annealing temperature. Transverse compositional homogeneity of the grown perovskite PZT and the level of Pb-diffusion from film to the seed layer and glass substrate are also observed to be seed layer thickness dependent.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Perovskite Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Jin · J Appl Phys · 2002 · 92 · 459410.1063/1.1506193 ↗
2. Kanno · J Appl Phys · 2003 · 93 · 409110.1063/1.1558951 ↗
3. Gong · Acta Mater · 2004 · 52 · 278710.1016/j.actamat.2004.02.025 ↗
4. Desfeux · Surf Sci · 2006 · 600 · 21910.1016/j.susc.2005.09.053 ↗
5. Brennecka · J Am Ceram Soc · 2004 · 87 · 145910.1111/j.1551-2916.2004.01459.x ↗
6. Tokita · Appl Phys Lett · 2003 · 82 · 412210.1063/1.1581975 ↗
7. Hiboux · J Euro Ceram Soc · 2004 · 24 · 159310.1016/S0955-2219(03)00404-7 ↗
8. Millon · Sensors Actuat A · 2004 · 113 · 37610.1016/j.sna.2004.01.055 ↗
9. Kalpat · J Appl Phys · 2001 · 90 · 270310.1063/1.1385580 ↗
10. Li · Sensors Actuat A · 2000 · 82 · 26510.1016/S0924-4247(99)00307-6 ↗
11. Li · Thin Solid Films · 2000 · 375 · 9110.1016/S0040-6090(00)01231-1 ↗
12. Jiang · Appl Surf Sci · 2006 · 252 · 875610.1016/j.apsusc.2005.12.112 ↗
13. Muralt · J Appl Phys · 2006 · 100 · 05160510.1063/1.2337362 ↗
14. Kwok · J Mater Res · 1993 · 8 · 33910.1557/JMR.1993.0339 ↗
15. Kao · Appl Phys Lett · 2003 · 83 · 391510.1063/1.1625428 ↗
16. Moon · Mater Sci Eng B · 2008 · 148 · 2210.1016/j.mseb.2007.09.051 ↗
17. Takahara · Thin Solid Films · 2008 · 516 · 839310.1016/j.tsf.2008.04.078 ↗
18. Talin · Appl Phys Lett · 2002 · 81 · 106210.1063/1.1498006 ↗
19. Shin · Thin Solid Films · 1999 · 354 · 25110.1016/S0040-6090(99)00429-0 ↗
20. Bose · J Am Ceram Soc · 2011 · 94 · 406610.1111/j.1551-2916.2011.04684.x ↗
21. Thomas · Thin Solid Films · 2002 · 413 · 6510.1016/S0040-6090(02)00354-1 ↗
22. Parish · J Am Ceram Soc · 2008 · 91 · 369010.1111/j.1551-2916.2008.02708.x ↗
23. Brennecka · Adv Mater · 2008 · 20 · 140710.1002/adma.200702442 ↗
24. Bose · Appl Surf Sci · 2013 · 282 · 20210.1016/j.apsusc.2013.05.103 ↗
25. Sreemany · Mater Chem Phys · 2009 · 115 · 45310.1016/j.matchemphys.2009.01.009 ↗
26. Goh · J Appl Phys · 2001 · 89 · 449710.1063/1.1356426 ↗
27. Holman · J Appl Phys · 1973 · 44 · 522710.1063/1.1662136 ↗