Laser annealing of SrBi2Ta2O9 thin films

Zhigang Zhang, Jinsong Zhu, Dong Su, Jianshe Liu, Huiming Shen, Yening Wang, Ling Kang, Jun Zhou, Shengzhu Yang, Peihen Wu

Publisher page

Abstract

A laser annealing technique was used to fabricate SrBi 2 Ta 2 O 9 (SBT) thin films at a low temperature. Amorphous SBT thin films were prepared on Pt/Ti/SiO 2 /Si substrates by a metalorganic decomposition (MOD) technique. A two-step process was used to crystallize the amorphous thin films: the films were annealed at 550°C for 0.5 h to initiate the nucleation of the SBT phase, and then annealed with a KrF excimer laser. X-Ray diffraction (XRD) patterns showed that the laser-annealed thin films were transformed into a SBT perovskite structure without the presence of a second phase. The films irradiated by laser with a lower energy density and a greater pulse number had a better grain and a rougher surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Electronic and Structural Properties of Oxides · Photorefractive and Nonlinear Optics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.