The effect of post deposition anneal temperature on the structure of BiFeO3–PbTiO3 thin films
Source abstract
Abstract
Abstract Pulsed laser deposition was used to produce 0.7BiFeO 3 –0.3PbTiO 3 bismuth ferrite–lead titanate thin films on polycrystalline platinised silicon substrates. The films were post deposition annealed at different temperatures ranging from 500 to 700 °C in an oxygen atmosphere for 30 min. The films annealed at 500–550 °C possess a single perovskite phase tetragonal structure, with (001) preferred orientation appearing in films annealed at 550 °C. Films annealed at 600 °C possess a mixed tetragonal–rhombohedral perovskite phase structure with {100} preferential orientation. At anneal temperatures between 650 and 700 °C, non-perovskite secondary phases are present with the film structure. The ability to tailor film crystallographic structure and texture using varying anneal temperatures is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Multiferroics and related materials · Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.