article·2003-08-01

Crack alleviation processing of lead zirconate titanate thin films deposited by sol–gel method

Bing‐Huei Chen, Cheng‐Liang Huang, Long Wu

Publisher page

Abstract

Abstract This paper illustrates the preparation of polycrystalline Pb(Zr,Ti)O3 (PZT) thin film using sol–gel processing and spin coating method. Lead acetate, zirconium n-propoxide and titanium isopropoxide were used as raw precursors. The PZT thin films with lower gel concentration of 0.2 and 0.3 M were used and deposited on Al/Si3N4/Si (100) substrate. After drying at 150 °C, pre-baking at 350 °C and sintering at 600–700 °C, the amorphous PZT thin films have been changed to perovskite-type crystal structure. The influence of gel solutions concentration and heating conditions on the morphology of PZT thin films were discussed. The cracking problem was alleviated by employing lower gel concentration of 0.2 M with a drying at 150 °C for 5 min and a pre-baking at 350 °C for 10 min, and then sintering at 700 °C for 30 min with a heating rate 50 °C/min. The values of the remanent polarization (Pr) and coercive field (Ec) are 11.39 μc/cm2 and 84.52 KV/cm, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Acoustic Wave Resonator Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.