Abstract The growth of epitaxial (001) CeO 2 on a (001) Ge surface using a reactive sputter deposition method is reported. Hydrogen gas (4%H 2 /Ar sputtering gas) is introduced during film growth in order to reduce or eliminate the presence of the GeO 2 from the semiconductor surface during the initial nucleation of the metal oxide film. A metal cerium target was used as the cation source, with water vapor serving as the oxidizing species. Epitaxial films were sputter deposited at a substrate temperature of 550 °C in a H 2 O vapor pressure of approximately 10 −3 Torr. The hydrogen partial pressure and substrate temperature were selected to be sufficiently high such that the germanium native oxides are thermodynamically unstable. The Gibbs free energy of CeO 2 is larger in magnitude than that of the Ge native oxides, making it more favorable for the metal oxide to reside at the interface in comparison to the native Ge oxides.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Catalytic Processes in Materials Science · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.