Annealing-free fluoropolymer protective layer for mitigating snail trails in crystalline silicon photovoltaic modules
Source abstract
Abstract
Snail trail faults, caused by the reaction between the silver electrodes of crystalline silicon (c-Si) photovoltaic (PV) cells and various chemicals, lead to electrode disconnection, performance degradation, and localized heating. This study aimed to develop stable c-Si PV modules by applying two different room-temperature processed protective layers: cyclic transparent optical polymer (CYTOP) and perhydropolysilazane (PHPS). Both coatings are designed to prevent acid-induced reactions at the cell`s electrodes. After 3 min of direct exposure to nitric acid, c-Si PV cells with protective coatings retained 75 % of their electrode height and performance, while 66 % of electrodes without protective layers were corroded. As a result, the series resistance of uncoated c-Si PV cells increased more than tenfold, whereas cells with PHPS and CYTOP coatings exhibited only a twofold increase. A 1000-h damp heat test of the encapsulated c-Si PV cells revealed that CYTOP effectively suppressed electrode degradation and preserved its shape, outperforming encapsulated uncoated cells. While the PHPS film demonstrated excellent protective properties at the cell level, its performance at the module level was hindered by poor adhesion between the encapsulant and the cell, leading to delamination. Therefore, a thin layer of CYTOP shows strong potential for protecting c-Si PV modules from acid-related degradation during operation. This work offers valuable insights for designing more reliable PV modules.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: solar cell performance optimization · Silicon and Solar Cell Technologies · Organic Electronics and Photovoltaics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Identifying methods to reduce emission intensity of centralised Photovoltaic deployment for net zero by 2050: Life cycle assessment case study of a 30 MW PV plant10.1002/pip.3747 ↗
2. Solar PV cell materials and technologies: analyzing the recent developments
3. Review of next generation photovoltaic solar cell technology and comparative materialistic development
4. Photovoltaic cell generations and current research directions for their development10.3390/ma15165542 ↗
5. Up-to-date literature review on Solar PV systems: technology progress, market status and R&D10.1016/j.jclepro.2022.132339 ↗
6. Analysis of the impact of power loss due to snail trails in a 95-kWp photovoltaic power system10.1016/j.microrel.2021.114230 ↗
7. Monitoring solar irradiance and PV module performance in mobile applications10.1016/j.solmat.2024.113101 ↗
8. Comprehensive analysis of aging mechanisms and design solutions for desert-resilient photovoltaic modules10.1016/j.solmat.2024.112707 ↗
9. Corrosion testing of solar cells: wear-out degradation behavior10.1016/j.solmat.2022.111974 ↗
10. Snail trails and cell microcrack impact on PV module maximum power and energy production10.1109/JPHOTOV.2016.2576682 ↗
11. Investigations of snail-trail and associated microcrack properities and behavior in Brazil's tropical climate
12. Encapsulation of PV modules using ethylene vinyl acetate copolymer as a pottant: a critical review10.1016/0927-0248(95)00150-6 ↗
13. Silver grid finger corrosion on snail track affected PV modules–investigation on degradation products and mechanisms10.1016/j.egypro.2016.10.083 ↗
14. Multi‐pronged degradation analysis of a photovoltaic power plant after 9.5 years of operation under hot desert climatic conditions10.1002/pip.3694 ↗
15. Long‐term degradation rate of crystalline silicon PV modules at commercial PV plants: an 82‐MWp assessment over 10 years10.1002/pip.3456 ↗
16. Quantifying the influence of encapsulant and backsheet composition on PV‐power and electrical degradation10.1002/pip.3679 ↗
17. Acetic acid permeation through photovoltaic backsheets: influence of the composition on the permeation rate10.1016/j.polymertesting.2017.04.025 ↗
18. Dependence of the optimization of the front grid design in passivated emitter and rear contact c-Si solar cells on the finger width and the aspect ratio10.3938/jkps.76.774 ↗
19. Screen pattern simulation for an improved front‐side Ag‐electrode metallization of Si‐solar cells10.1002/pip.3313 ↗
20. Corrosion of novel reactive silver ink and commercial silver-based metallizations in diluted acetic acid10.1016/j.solmat.2020.110900 ↗
21. Durable superhydrophobic surface with highly antireflective and self-cleaning properties for the glass covers of solar cells10.1016/j.apsusc.2018.05.139 ↗
22. Transparent alumina based superhydrophobic self–cleaning coatings for solar cell cover glass applications10.1016/j.solmat.2017.02.027 ↗
23. A review on emerging barrier materials and encapsulation strategies for flexible perovskite and organic photovoltaics10.1002/aenm.202101383 ↗
24. Recent advances in superhydrophobic polymers for antireflective self-cleaning solar panels10.1016/j.rser.2021.111538 ↗
25. Antireflective and anti-dust modified silica based thin film on solar cell cover glass10.1016/j.jallcom.2021.162228 ↗
26. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
27. Properties and degradation behaviour of polyolefin encapsulants for photovoltaic modules10.1002/pip.3323 ↗
28. Corrosion and tribocorrosion mitigation of perhydropolysilazane-derived coatings on low carbon steel10.1016/j.corsci.2020.108946 ↗
29. Superior properties of silica thin films prepared from perhydropolysilazane solutions at room temperature in comparison with conventional alkoxide-derived silica gel films10.1021/am400845y ↗
30. High temperature oxidation behaviors of SiON coated AISI 441 in Ar+ O2, Ar+ H2O, and Ar+ CO2 atmospheres10.1016/j.corsci.2020.108429 ↗
31. Inorganic encapsulation method using solution-processible polysilazane for flexible solar cells10.1021/acsaem.0c01593 ↗
32. Hydrophobic, transparent and hard silicon oxynitride coating from perhydropolysilazane10.1002/pi.4871 ↗
33. Room temperature processed protective layer for printed silver electrodes10.1039/D3RA02212A ↗
34. Study on the enhanced shelf lifetime of CYTOP-encapsulated organic solar cells10.3390/en14133993 ↗
35. Comparison of semiconductor growth and charge transport on hydrophobic polymer dielectrics of organic field-effect transistors: cytop vs. polystyrene10.1016/j.orgel.2019.105485 ↗
36. Room‐temperature printing of organic thin‐film transistors with π‐junction gold nanoparticles10.1002/adfm.201400169 ↗
37. The role of antireflective coating CYTOP, immersion oil, and sensitizer selection in fabricating a 2.3 V, 10% power conversion efficiency SSM‐DSC device10.1002/aenm.201900162 ↗
38. Acetic acid production and glass transition concerns with ethylene-vinyl acetate used in photovoltaic devices10.1016/j.solmat.2006.10.009 ↗
39. Polysilazane‐based coatings with anti‐adherent properties for easy release of plastics and composites from metal molds
40. Novel approach to anti‐fouling and fouling‐release marine coatings based on dual‐functional siloxanes
41. Design and preparation of durable anti‐icing polysilazane coatings with abrasion and UV resistance10.1002/app.53416 ↗
42. A universal stamping method of graphene transfer for conducting flexible and transparent polymers10.1038/s41598-019-40408-w ↗