journal article·2026-04Open access

Accelerated corrosion performance of solar cells: A critical review

Zuraiz Rana, Douglas Olivares, Aitor Marzo, Víctor M. Jiménez-Arévalo, Edward Fuentealba, Jorge Rabanal-Arabach, Felipe M. Galleguillos Madrid

Abstract

This review examines accelerated corrosion in photovoltaic (PV) systems, focusing on the effects of moisture, salt exposure, and atmospheric conditions on material degradation. It connects ASTM-B117 salt spray testing with electrochemical and nanoscale characterization techniques (EIS, potentiodynamic polarization, SEM, AFM, XPS, FTIR) to identify defects such as delamination, snail trails, and metallization discoloration that reduce PV performance. The work highlights generational improvements in materials and designs, and proposes a multidimensional framework for real-time monitoring and failure prediction. These insights aim to guide the development of robust, durable PV technologies suitable for extreme environments.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Cdte-based thin film solar cells: past, present and future
2. A comprehensive review on life cycle assessment of commercial and emerging thin-film solar cell systems10.1016/j.rser.2023.113652 ↗
3. Design, fabrication, and testing of salt spray as an atmospheric corrosion test tool using MgCl2 and NaCl solutions10.14710/jksa.27.10.499-509 ↗
4. Atmospheric corrosion behavior of typical aluminum alloys in low-temperature environment10.3390/met15030277 ↗
5. Evaluation of degradation energy productivity of photovoltaic installations in long-term case study10.1016/j.apenergy.2023.121109 ↗
6. Beyond the horizon: exploration of perovskite solar cells in extreme environments10.1002/cptc.202400337 ↗
7. An investigation of the dust accumulation on photovoltaic panels10.1007/s11356-019-06742-2 ↗
8. A novel solution for addressing the problem of soiling and improving performance of PV solar systems10.1016/j.solener.2022.06.012 ↗
9. Air-Processed perovskite solar cells: challenges, progress, and industrial strategies
10. Assessing corrosion effects on the electrical performance of wearable photovoltaic cells: a comparative analysis of current consistency and resistance10.3390/ma18020267 ↗
11. Corrosion monitoring and mitigation techniques on advanced thermal energy storage materials for CSP plants10.1016/j.solmat.2018.12.028 ↗
12. Novel textured surfaces for superior corrosion mitigation in molten carbonate salts for concentrating solar power10.1016/j.rser.2022.112961 ↗
13. A comprehensive review of solar dish system: components, performance, and economy10.1016/j.rser.2025.115882 ↗
14. Advanced coatings and structures for enhancing concentrating solar power efficiency10.1016/j.rser.2024.115270 ↗
15. Wang Z, Zou S, Lu Z, Dai L, Peng C-W, Chen Z, Sun H, Zhang J, Liao B, Su X, author Jiangsu C. Solution-processed selective Ni seed layers enabling simplified copper electroplating for silicon heterojunction solar cells. n.d. https://doi.org/10.2139/ssrn.5217440.10.2139/ssrn.5217440 ↗
16. Influence of pulsed waveform parameters on the microstructure and electrochemical corrosion resistance of electrodeposited Ni–Sn alloy coatings10.1007/s40243-025-00317-7 ↗
17. Silver-doped zirconium copper oxide nanohybrid for electrochemical identification of dihydroxybenzene isomers10.1007/s11581-025-06633-2 ↗
18. A unique sustainable chemical method for the recovery of pure silicon from waste crystalline silicon solar panels
19. Output power enhancement of a bifacial solar photovoltaic with upside down installation during module defects10.1016/j.apenergy.2023.122070 ↗
20. Climate change impacts on global photovoltaic variability10.1016/j.apenergy.2024.124087 ↗
21. An experimental study on the effect of salt spray testing on the optical properties of solar selective absorber coatings produced with different manufacturing technologies10.1007/s40095-019-0299-7 ↗
22. An investigation on the reliability and degradation of polycrystalline silicon solar cells under accelerated corrosion test10.37358/MP.17.3.4872 ↗
23. Accelerated environmental chambers and testing of PV modules
24. Evaluating the impact of laundering on the electrical performance of wearable photovoltaic cells: a comparative study of current consistency and resistance10.3390/textiles4040028 ↗
25. Gonzalez-Pena V, Natarajan S, Xia Y, Klein D, Carter R, Pang Y, Shaner B, Annu K, Putnam D, Chen W, Connelly J, Pruett-Miller S, Chen X, Easton J, Gawad C, Zuckerberg Biohub C, Francisco S, by Christopher Walsh EA. Accurate genomic variant detection in single cells with primary template-directed amplification n.d. https://doi.org/10.1073/pnas.2024176118/-/DCSupplemental.
26. A review on life cycle environmental impacts of emerging solar cells10.1016/j.scitotenv.2023.168019 ↗
27. Insights into the recycling of discarded solar panels: challenges and future outlook
28. From lab to fab: bridging the quality divide of scalable perovskite solar cells thin-films
29. Yamaguchi T, Serikawa T, Henmi M, Oginuma H, Kondoh K. Mg 2 Si Coating Technology on Magnesium Alloys to Improve Corrosion and Wear Resistance *. n.d. https://doi.org/10.2320/matertrans.47.1026.10.2320/matertrans.47.1026 ↗
30. Correlation between the anticorrosive performance of protective coatings under neutral salt spray testing and outdoor atmospheric and immersion exposure10.3390/cmd5040023 ↗
31. Raymund Singleton Singleton Corp B. testing ACCELERATED CORROSION TESTING. n.d. https://doi.org/10.1016/S0026-0576(10)80256-80259.
32. Estimating the uncertainty of the result for tests of resistance to environmental conditions on the example of the method of resistance to neutral salt mist according to EN ISO 9227/ASTM B11710.36137/1982E ↗
33. Crystalline silicon photovoltaic module degradation: galvanic corrosion and its solution10.1016/j.engfailanal.2022.106329 ↗
34. Controlled growth of CdTe films by periodic voltammetry for solar cell applications10.1016/j.electacta.2009.04.046 ↗
35. Revisiting a minimally destructive analytic approach for determining electrochemical kinetic parameters: measuring aluminum corrosion across a wide pH range based on the Butler-Volmer equation10.1016/j.corsci.2025.112900 ↗
36. Suitability of existing photovoltaic degradation models for agrivoltaic systems10.3390/en18081937 ↗
37. Electrochemical mechanisms of leakage-current in photovoltaic modules10.1002/pip.3677 ↗
38. Solar panel corrosion: a review10.3390/ijms26135960 ↗
39. Potential-Induced electrochemical corrosion in crystalline silicon solar cells10.1002/solr.202300980 ↗
40. Berghold
41. Electrochemical mechanisms of leakage-current-enhanced delamination and corrosion in Si photovoltaic modules10.1016/j.solmat.2018.09.010 ↗
42. Recent progress in non-precious metal single atomic catalysts for solar and non-solar driven hydrogen evolution reaction10.1002/adsu.202000151 ↗
43. Two-dimensional materials as catalysts for solar fuels: hydrogen evolution reaction and CO 2 reduction10.1039/C8TA09496A ↗
44. Boosting electrocatalysis of oxygen reduction reaction through photovoltaic-driven potential manipulation strategy10.1016/j.mtener.2018.08.002 ↗
45. Photoinduced oxygen reduction reaction boosts the output voltage of a zinc–air battery10.1002/anie.201905954 ↗
46. De N, Filho M, Cardoso Diniz ASA, Vasconcelos CKB, Kazmerski LL. Snail trails on PV modules in Brazil's tropical climate: detection, Chemical Properties, Bubble Formation, and Performance Effects. n.d. https://doi.org/doi.org/10.1016/j.seta.2022.102808.
47. Encapsulant adhesion to surface metallization on photovoltaic cells10.1109/JPHOTOV.2017.2746572 ↗
48. Dhere NG, Raravikar NR. Adhesional shear strength and surface analysis of a PV module deployed in harsh coastal climate. n.d. https://doi.org/10.1016/S0927-0248(00)00304-4.10.1016/S0927-0248(00)00304-4 ↗
49. Heat generation in perovskite/CZTSSe tandem solar cells
50. High-humidity stable perovskite solar cells using dopant-free pyrrolo[3,4-c]pyrrole-1,4-dione-based polymeric hole transport material
51. Assessing power degradation and reliability of crystalline silicon solar modules with snail trails10.1016/j.solmat.2018.07.021 ↗
52. Failures of photo
53. Performance degradation and reliability evaluation of crystalline silicon photovoltaic modules without and with considering measurement reproducibility: a case study in desert area10.1016/j.renene.2023.119421 ↗
54. Inspection and condition monitoring of large-scale photovoltaic power plants: a review of imaging technologies10.1016/j.rser.2022.112353 ↗
55. Kettle · Prog. Photovoltaics Res. Appl. · 2022 · 30 · 136510.1002/pip.3577 ↗
56. The performance of solar PV modules with two glass types after 11 years of outdoor exposure under the mediterranean climatic conditions
57. A review on silicon photovoltaic module degradations and recent identification techniques10.1016/j.solener.2025.113288 ↗
58. Controlling TiO2 photocatalytic behaviour via perhydropolysilazane-derived SiO2 ultrathin shell10.1039/D4NR03566F ↗
59. Annealing-free fluoropolymer protective layer for mitigating snail trails in crystalline silicon photovoltaic modules10.1016/j.solmat.2025.113473 ↗
60. Synthesis and electrochemical investigations of ABPBI grafted montmorillonite based polymer electrolyte membranes for PEMFC applications10.1016/j.renene.2020.09.104 ↗
61. Solar PV potential in Africa for three generational time-scales: present, near future and far future10.1016/j.solener.2024.112638 ↗
62. Delamination-and electromigration-related failures in solar panels—a review
63. Corrosion effects in bifacial crystalline silicon PV modules; interactions between metallization and encapsulation10.1016/j.solmat.2023.112321 ↗
64. A comprehensive review on composite phase change materials for sustainable thermal energy solutions: advances and barriers
65. Corrosion behavior of crystalline silicon solar cells10.1016/j.microrel.2017.01.006 ↗
66. Automatic detection of photovoltaic module defects in infrared images with isolated and develop-model transfer deep learning10.1016/j.solener.2020.01.055 ↗
67. Review of degradation and failure phenomena in photovoltaic modules10.1016/j.rser.2022.112160 ↗
68. Li
69. Microstructural analysis of the PV module cementation process at the solar platform of the Atacama Desert10.1016/j.solmat.2021.111109 ↗
70. Soil characterization and soiling impact to facilitate photovoltaic installation10.3390/app122010582 ↗
71. Effect of soiling on photovoltaic modules10.1016/j.solener.2013.07.017 ↗
72. The effect of environmental factors and dust accumulation on photovoltaic modules and dust-accumulation mitigation strategies10.1016/j.rser.2017.09.042 ↗
73. An analytical indoor experimental study on the effect of soiling on PV, focusing on dust properties and PV surface material10.1016/j.solener.2020.03.089 ↗
74. Effect of dust and methods of cleaning on the performance of solar PV module for different climate regions: comprehensive review10.1016/j.scitotenv.2022.154050 ↗
75. Experimental analysis of dust composition impact on photovoltaic panel performance: a case study10.1016/j.solener.2023.112206 ↗
76. Recent progress of soiling impact on solar panels and its mitigation strategies: a review10.1016/j.apenergy.2024.124979 ↗
77. Progress in research and technological developments of phase change materials integrated photovoltaic thermal systems: the allied problems and their mitigation strategies
78. Electrolyte for quantum dot-sensitized solar cells assessed with cyclic voltammetry10.1007/s40843-015-0054-1 ↗
79. Enhanced photoelectrochemical activity of electro-synthesized CdS-Bi 2S3 composite films grown with self-designed cross-linked structure10.1016/j.electacta.2010.06.022 ↗
80. Electrochemical growth and characterization of size-quantized CdTe thin films grown by underpotential deposition10.1016/j.jelechem.2010.12.005 ↗
81. A simple synthesis, characterization, and properties of poly(methyl methacrylate) grafted CdTe nanocrystals10.1080/15421406.2015.1076305 ↗
82. Electrical impedance spectroscopy: a complementary approach differentiating PID mechanisms in photovoltaics
83. CdTe nanoparticles decorated titania for dye sensitized solar cell: a novel co-sensitizer approach towards highly efficient energy conversion10.1039/C7NJ00737J ↗
84. Cyclic voltammetric and chronoamperometric deposition of CdS10.2320/matertrans.M2013125 ↗
85. Cyclic voltammetry studies of copper, tin and zinc electrodeposition in a citrate complex system for CZTS solar cell application10.1016/j.cap.2015.11.017 ↗
86. High efficiency CdS/CdSe quantum dot sensitized solar cells with two ZnSe layers10.1021/acsami.6b12842 ↗
87. A review on electrical characterization techniques performed to study the device performance of quantum dot sensitized solar cells10.1016/j.solener.2017.11.037 ↗
88. From efficiency to eternity: a holistic review of photovoltaic panel degradation and end-of-life management10.1016/j.solener.2023.112135 ↗
89. Effect of modified titanium dioxide photoanode and agarose gel electrolyte on electrochemical studies of dye-sensitized solar cell10.1016/j.optmat.2024.115275 ↗
90. On voltage, photovoltage, and photocurrent in bulk heterojunction organic solar cells10.1021/jz2004864 ↗
91. Electrochemical impedance spectroscopic analysis of dye-sensitized solar cells10.1021/jp052768h ↗
92. Electrochemical impedance spectroscopic analysis of sensitization-based solar cells10.1002/ijch.201500007 ↗
93. Investigation of solar cell degradation using electrochemical impedance spectroscopy10.1002/er.5567 ↗
94. Theory for electrochemical impedance spectroscopy of heterogeneous electrode with distributed capacitance and charge transfer resistance10.1007/s12039-017-1335-x ↗
95. Degradation behavior of crystalline silicon solar cells in a cell-level potential-induced degradation test10.1016/j.solener.2017.07.009 ↗
96. Solid-state and flexible dye-sensitized TiO2 solar cells: a study by electrochemical impedance spectroscopy10.1021/jp014456u ↗
97. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
98. Online electrochemical impedance spectroscopy (EIS) estimation of a solar panel10.1016/j.vacuum.2017.01.011 ↗
99. Electrochromic device with hierarchical metal mesh electrodes: transmittance switching in the full spectral range of solar radiation10.1016/j.solmat.2023.112345 ↗
100. Gettering in silicon photovoltaics: a review10.1016/j.solmat.2021.111447 ↗