Abstract

Effects of alkali metal on the potential-induced degradation (PID) phenomena in wafer-based conventional p-type crystalline silicon technologies were studied. It is known that sodium rapidly and severely brings the shunting-type PID (PID-s) phenomenon; however, the impact of other alkali metal such as lithium and potassium on the PID-s phenomenon is unrevealed. We used solar cells that light-receiving surface was contaminated with lithium, sodium or potassium, and in order to control the sodium content, prepared were photovoltaic modules without cover glass and performed were PID tests and anneal tests. During the tests, the performance of each module was judged by the current-voltage measurements and the electroluminescence images. After a certain time of PID tests, the secondary ion mass spectrometry analysis was performed on the solar cells of some modules. Thus, the penetration status of alkali metal elements is judged. From the PID tests and anneal tests, we conclude that, the negative potential of the solar cell light-receiving surface is the basis of the PID-s phenomenon. Furthermore, in the PID tests, all elements penetrated into the solar cell, but only sodium rapidly causes severe PID-s phenomenon. The PID-s phenomenon appears to be moderated when both lithium and sodium are present on the solar cell light-receiving surface. Therefore, we believe that lithium and potassium do not cause PID-s phenomenon, and lithium seems to mitigate the sodium-induced PID-s phenomenon.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Potential induced degradation of solar cells and panels
2. Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat
3. System voltage potential-induced degradation mechanisms in PV modules and methods for test
4. Crystalline Si solar cells and modules featuring excellent stability against potential-induced degradation
5. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
6. Towards a kinetic model of potential-induced shunting
7. Potential-induced degradation (PID): introduction of a novel test approach and explanation of increased depletion region recombination10.1109/JPHOTOV.2014.2300238 ↗
8. Sodium decoration of PID-s crystal defects after corona induced degradation of bare silicon solar cells10.1016/j.egypro.2015.07.055 ↗
9. Origin of Na causing potential-induced degradation for P-type crystalline Si photovoltaic modules10.1063/1.5040516 ↗
10. 2015
11. Crystalline Si photovoltaic modules based on TiO2-coated cover glass against potential-induced degradation10.1039/C4RA06791F ↗
12. PID test round robins and outdoor correlation
13. Degradation behavior of crystalline silicon solar cells in a cell-level potential-induced degradation test10.1016/j.solener.2017.07.009 ↗
14. Comparison of potential-induced degradation (PID) of N-type and P-type silicon solar cells10.1016/j.energy.2018.07.118 ↗
15. Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules10.1002/pip.3028 ↗
16. Investigation of the impact of illumination on the polarization-type potential-induced degradation of crystalline silicon photovoltaic modules10.1109/JPHOTOV.2018.2843791 ↗
17. Physics of potential-induced degradation in bifacial p-PERC solar cells10.1016/j.solmat.2019.109950 ↗
18. Local corrosion of silicon as root cause for potential‐induced degradation at the rear side of bifacial PERC solar cells10.1002/pssr.201900163 ↗
19. Root cause analysis on corrosive potential-induced degradation effects at the rear side of bifacial silicon PERC solar cells10.1016/j.solmat.2019.110062 ↗
20. Microstructural analysis of local silicon corrosion of bifacial solar cells as root cause of potential-induced degradation at the rear side
21. Potential-induced degradation of bifacial PERC solar cells under illumination10.1109/JPHOTOV.2019.2937231 ↗
22. Influence of refining agent in soda lime glass for ultraviolet ray transmittance10.2320/matertrans.MRA2007172 ↗
23. Roles of SiNx in potential-induced degradation for P-type crystalline Si photovoltaic modules
24. Potential-free sodium-induced degradation of silicon heterojunction solar cells10.1002/pip.3698 ↗
25. Sodium accumulation at potential-induced degradation shunted areas in polycrystalline silicon modules10.1109/JPHOTOV.2016.2601950 ↗
26. Multistage performance deterioration in N-type crystalline silicon photovoltaic modules undergoing potential-induced degradation10.1016/j.microrel.2018.03.018 ↗
27. Explanation of commonly observed shunt currents in c-Si solar cells by means of recombination statistics beyond the shockley-read-Hall approximation10.1063/1.3607310 ↗
28. Investigations on the formation of stacking fault-like PID-shunts10.1016/j.egypro.2016.07.021 ↗
29. Ionic radius scale of establishing synthesis factor of ionic mass and electricity10.1016/S1872-1508(07)60043-6 ↗
30. S. M. Sze, K.K. Ng, “Physics of Semiconductor Devices” third ed. (Wiley) p. 2S3.