journal article·2022-06

Effective way to reduce rear-side potential-induced degradation of bifacial PERC solar cells

S. Ma, R. Tong, X.Y. Wu, Z.P. Li, X.Y. Kong, W.Z. Shen

Publisher page

Abstract

While bifacial p -type silicon ( p- Si) passivated emitter and rear cells (PERCs) have dominated the current photovoltaic industry, potential-induced degradation (PID), especially in the rear-side, has become a big issue in their practical applications. Here, we have investigated the impact of different rear passivation layers on the anti-PID and electrical property of bifacial p-Si PERCs. Both simulation and characterization showed that the introduction of SiN x films with a high refractive index and additive oxide films were in favor of reducing the rear PID effect. Finally, we proposed a combined structure of stack films as the rear passivation layer, yielding an absolute front-side and rear-side efficiency improvement of 0.09% and 0.18% with 800 pieces of 166 × 166 mm 2 Si wafers on the production line, and the rear PID related power loss dropped from the baseline of 5.46%–1.05% and 5.15%–0.56% by single-cell modules and commercial glass-glass modules, respectively. Together with the well-solved front-side anti-PID technique in industry, the presented novel rear passivation layer establishes a base for the efficient applications of the bifacial p-Si PERCs.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. The passivated emitter and rear cell (PERC): from conception to mass production10.1016/j.solmat.2015.06.055 ↗
2. Bifacial solar photovoltaics-A technology review10.1016/j.rser.2016.03.041 ↗
3. Outdoor performance test of bifacial n-type silicon photovoltaic modules10.3390/su11226234 ↗
4. Effect of humidity and temperature on the potential-induced degradation10.1002/pip.2238 ↗
5. Pingel · 2010 · 2817
6. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
7. Microstructural analysis of crystal defects leading to potential induced degradation (PID) of Si solar cells10.1016/j.egypro.2013.05.042 ↗
8. Micro structural root cause analysis of potential induced degradation in c-Si solar cells10.1016/j.egypro.2012.07.020 ↗
9. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
10. Irreversible damage at high levels of potential-induced degradation on photovoltaic modules: a test campaign
11. Voltage dependence of potential-induced degradation and recovery on photovoltaic one-cell laminates
12. Potential induced degradation effects on crystalline silicon cells with various antireflective coatings
13. Minimizing the polarization-type potential-induced degradation in PV modules by modification of the dielectric antireflection and passivation stack10.1109/JPHOTOV.2019.2896944 ↗
14. Green · 1987 · 681
15. Overcoming over-plating problems for PECVD SiNx passivated laser doped p-type multi-crystalline silicon solar cells10.1016/j.solmat.2011.12.003 ↗
16. Mitigating potential-induced degradation (PID) using SiO2 ARC layer10.3390/en13195139 ↗
17. Research on the effect of encapsulation material on anti-PID performance of 1500 V solar module10.1016/j.ijleo.2019.163540 ↗
18. Elucidating potential‐induced degradation in bifacial PERC silicon photovoltaic modules10.1002/pip.3028 ↗
19. Investigation of the impact of illumination on the polarization-type potential-induced degradation of crystalline silicon photovoltaic modules10.1109/JPHOTOV.2018.2843791 ↗
20. The surface polarization effect in high-efficiency silicon solar cells
21. Changes in the current density-voltage and external quantum efficiency characteristics of n‐type single‐crystalline silicon photovoltaic modules with a rear‐side emitter undergoing potential‐induced degradation10.1016/j.solmat.2016.03.003 ↗
22. Investigation of potential‐induced degradation in n‐PERT bifacial silicon photovoltaic modules with a glass/glass structure10.1109/JPHOTOV.2017.2762587 ↗
23. Microstructural analysis of local silicon corrosion of bifacial solar cells as root cause of potential-induced degradation at the rear-side10.1002/pssa.201900334 ↗
24. Root cause analysis on corrosive potential-induced degradation effects at the rear-side of bifacial silicon PERC solar cells10.1016/j.solmat.2019.110062 ↗
25. The role of stacking faults for the formation of shunts during potential-induced degradation of crystalline Si solar cells10.1002/pssr.201307090 ↗
26. Quick test for reversible and irreversible PID of bifacial PERC solar cells10.1016/j.solmat.2020.110755 ↗
27. Kambe · 2013 · 2861
28. Consideration on Na diffusion and recovery phenomena in potential-induced degradation for crystalline Si photovoltaic modules10.7567/JJAP.55.02BF10 ↗
29. Time-resolved investigation of transient field effect passivation states during potential-induced degradation and recovery of bifacial silicon solar cells10.1002/solr.202100140 ↗
30. Surface effects on p‐n junctions: characteristics of surface space‐charge regions under non‐equilibrium conditions10.1016/0038-1101(66)90118-3 ↗
31. Low temperature surface passivation of silicon for solar cells10.1149/1.2096673 ↗
32. Influence of the chemical composition in SiNx films on silver paste contact formation at silicon surface10.1016/j.solener.2016.01.001 ↗
33. Influence of hydrogenated passivation layers on the regeneration of boron-oxygen related defects10.1016/j.egypro.2013.07.328 ↗
34. Broad range refractive index engineering of SixNy and SiOxNy thin films and exploring their potential applications in crystalline silicon solar cells10.1016/j.matchemphys.2017.05.035 ↗
35. Application of SiOxNy films in industrial bifacial PERC solar cells10.1016/j.solmat.2021.111199 ↗
36. Detailed study of SiOxNy:H/Si interface properties for high quality surface passivation of crystalline silicon10.1016/j.spmi.2017.07.052 ↗