Role of post-metallization anneal sequence and forming gas anneal to mitigate light and elevated temperature induced degradation of multicrystalline silicon solar cells
Source abstract
Abstract
Abstract The mystery surrounding the role of hydrogen in light and elevated temperature induced degradation (LeTID) of multicrystalline silicon (mc-Si) solar cells is attracting a lot of interest in the photovoltaic community. It is still unclear whether hydrogen plays a role in the degradation or the regeneration phase, with convincing evidence reported for both. In this paper, we base our work on the hypothesis that hydrogen plays a role in both phases depending on its charge state. Hydrogen in at least one charge state can passivate the LeTID defect. Thus, it is possible to mitigate LeTID in mc-Si by controlling the charge state of hydrogen. We observe in our experiments that the sequence of different thermal anneals impacts the degree of degradation. We also explore the possibility of mitigating LeTID by annealing the samples in a forming gas atmosphere. P-type mc-Si samples that received a forming gas anneal (FGA) show an improvement of the effective carrier lifetime when subjected to 1-Sun light soaking at 80 °C. Mc-Si PERC solar cells fabricated by incorporating a FGA anneal step show about 1.5% (relative) maximum drop in efficiency during 300 h of light soaking, as compared to about 3.2% (relative) maximum drop for cells fabricated by annealing in atmospheric air (without FGA), and 5.3% (relative) maximum drop for non-annealed cells. It thus seems that, after optimization, FGA is an easy to implement solution to minimise LeTID in industrial mc-Si solar cells.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Light induced degradation of rear passivated mc-Si solar cells
2. Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperature10.1016/j.solmat.2015.06.015 ↗
3. Dependence of LeTID on brick height for different wafer suppliers with several resistivities and dopants
4. Seasonal variations in the operating temperature of silicon solar panels in southern Ghana10.1080/20421338.2015.1038006 ↗
5. Multi-physics modeling and simulation of heat and electrical yield generation in photovoltaics10.1016/j.solmat.2017.07.039 ↗
6. Development of a real-scale cooling module for a PV power plant10.1049/iet-rpg.2016.0192 ↗
7. Simulation of large photovoltaic arrays10.1016/j.solener.2017.12.034 ↗
8. System performance loss due to LeTID10.1016/j.egypro.2017.09.260 ↗
9. Engineering solutions and root-cause analysis for light-induced degradation in p-type multicrystalline silicon PERC modules10.1109/JPHOTOV.2016.2556981 ↗
10. Lifetime degradation and regeneration in multicrystalline silicon under illumination at elevated temperature10.1063/1.4944839 ↗
11. Impact of the firing temperature profile on light induced degradation of multicrystalline silicon10.1002/pssr.201600272 ↗
12. Evolution of LeTID defects in p-type multicrystalline silicon during degradation solar and regeneration10.1109/JPHOTOV.2017.2695496 ↗
13. Kinetics of carrier-induced degradation at elevated temperature in multicrystalline silicon solar cells10.1016/j.solmat.2017.05.066 ↗
14. Influence of Al2O3 and SiNx passivation layers on LeTID10.1016/j.egypro.2016.07.079 ↗
15. Carrier-induced degradation in multicrystalline silicon: dependence on the silicon nitride passivation layer and hydrogen released during firing10.1109/JPHOTOV.2017.2783851 ↗
16. Rapid stabilization of high-performance multicrystalline p-type silicon PERC cells10.1109/JPHOTOV.2016.2606704 ↗
17. Influence of hydrogen effusion from hydrogenated silicon nitride layers on the regeneration of boron-oxygen related defects in crystalline silicon10.1063/1.4833243 ↗
18. Energy levels of isolated interstitial hydrogen in silicon10.1103/PhysRevB.64.125209 ↗
19. Modelling of hydrogen transport in silicon solar cell structures under equilibrium conditions10.1063/1.5016854 ↗
20. Optimization of belt furnace anneal to reduce light and elevated temperature induced degradation of effective carrier lifetime of p-type multicrystalline silicon wafers10.1002/solr.201800070 ↗
21. Modulation of carrier-induced defect kinetics in multi-crystalline silicon PERC cells through dark Annealing
22. Impact of annealing on the formation and mitigation of carrier-induced defects in multi-crystalline silicon10.1016/j.egypro.2017.09.087 ↗
23. Understanding the light-induced lifetime degradation and regeneration in multicrystalline silicon10.1016/j.egypro.2016.07.060 ↗
24. Rapid mitigation of carrier-induced degradation in commercial silicon solar cells10.7567/JJAP.56.08MB13 ↗
25. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
26. Temperature and light-induced changes in bulk and passivation quality of boron-doped float-zone silicon coated with SiNx:H10.1109/JPHOTOV.2017.2649601 ↗
27. Light and elevated temperature induced degradation in p-type and n-type cast-grown multicrystalline and mono-like silicon10.1016/j.solmat.2018.03.002 ↗
28. A unified approach to modelling the charge state of monatomic hydrogen and other defects in crystalline silicon10.1063/1.4906465 ↗
29. Advanced bulk defect passivation for silicon solar cells10.1109/JPHOTOV.2013.2281732 ↗
30. Erratum: evidence for the existence of a negatively charged hydrogen species in plasma-treated n-type Si (Applied Physics Letters (1990) 56 (94910.1063/1.104293 ↗
31. Efficiency improved by H2 forming gas treatment for Si-based solar cell applications
32. Mechanism underlying the beneficial effect of forming gas annealing on screen-printed Ag contacts of crystalline Si solar cells10.1016/j.actamat.2014.02.023 ↗
33. Gettering and hydrogen passivation of edge-defined film-fed grown multicrystalline silicon solar cells by Al diffusion and forming gas anneal10.1063/1.110880 ↗
34. Mechanism (s) of hydrogen diffusion in silicon solar cells during forming gas anneal
35. Manipulation of hydrogen charge states for passivation of P-type wafers in photovoltaics10.1109/JPHOTOV.2014.2339494 ↗