journal article·2016-12Open access

Degradation of thermally-cured silicone encapsulant under terrestrial UV

Can Cai, David C. Miller, Ian A. Tappan, Reinhold H. Dauskardt

Abstract

Abstract Concentrator photovoltaic (CPV) modules operate in extreme conditions, including enhanced solar flux, elevated operating temperature, and frequent thermal cycling. Coupled with active environmental species such as oxygen and moisture, the operating conditions pose a unique materials challenge for guaranteeing operational lifetimes of greater than 25 years. Specifically, the encapsulants used in the optical elements are susceptible to environmental degradation during operation. For example, the interfaces must remain in contact to prevent optical attenuation and thermal runaway. We developed fracture mechanics based metrologies to characterize the adhesion of the silicone encapsulant and its adjacent surfaces, as well as the cohesion of the encapsulant. Further, we studied the effects of weathering on adhesion using an outdoor concentrator operating in excess of 1100 times the AM1.5 direct irradiance and in indoor environmental chambers with broadband ultraviolet (UV) irradiation combined with controlled temperature and humidity. We observed a sharp initial increase in adhesion energy followed by a gradual decrease in adhesion as a result of both outdoor concentrator exposure and indoor UV weathering. We characterized changes in mechanical properties and chemical structures using XPS, FTIR, and DMA to understand the fundamental connection between mechanical strength and the degradation of the silicone encapsulant. We developed physics based models to explain the change in adhesion and to predict operational lifetimes of the materials and their interfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · solar cell performance optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Durability of polymeric encapsulation materials for concentrating photovoltaic systems10.1002/pip.1241 ↗
2. Adhesion and debonding of multi-layer thin film structures10.1016/S0013-7944(98)00052-6 ↗
3. Moisture-assisted subcritical debonding of a polymer/metal interface10.1063/1.1427139 ↗
4. Adhesion and debonding kinetics of photovoltaic encapsulation in moist environments10.1002/pip.2657 ↗
5. Environmentally assisted debonding of copper/barrier interfaces10.1016/j.actamat.2012.01.007 ↗
6. Analysis of transmitted optical spectrum enabling accelerated testing of multijunction concentrating photovoltaic designs
7. Photo-oxidation of polydimethylsiloxane oils: Part I—effect of silicon hydride groups10.1016/0141-3910(92)90155-X ↗
8. Photo-oxidation of polydimethylsiloxane oils: II—effect of vinyl groups10.1016/0141-3910(92)90161-W ↗
9. Photo-oxidation of polydimethylsiloxane oils Part III—effect of dimethylene groups10.1016/0141-3910(93)90223-6 ↗
10. Surface modification of Sylgard-184 poly(dimethyl siloxane) networks by ultraviolet and ultraviolet/ozone treatment10.1006/jcis.2002.8594 ↗
11. Hydrophobic recovery of UV/ozone treated poly(dimethylsiloxane): adhesion studies by contact mechanics and mechanism of surface modification10.1016/j.apsusc.2004.06.005 ↗
12. Photosensitive poly(dimethylsiloxane) materials for microfluidic applications10.1016/j.mee.2007.01.011 ↗
13. Photodecomposition of polymethylsiloxane10.1002/pol.1969.150071210 ↗
14. Effects of chain pull-out on adhesion of elastomers10.1021/ma00059a027 ↗
15. Adhesion at the solid-elastomer interface: influence of the interfacial chains10.1021/ma00126a021 ↗
16. Effect of interfacial bonding on the strength of adhesion of elastomers. I. Self-Adhesion
17. Photoinduced transformation of polysiloxane layers to SiO210.1016/0169-4332(89)90229-8 ↗
18. Thermal analysis of polydimethylsiloxanes. I. Thermal degradation in controlled atmospheres10.1002/pol.1969.160070308 ↗
19. Polydimethylsiloxane thermal degradation Part 1. Kinetic aspects10.1016/S0032-3861(00)00652-2 ↗
20. Crack path selection in a brittle adhesive layer10.1016/0020-7683(91)90069-R ↗
21. The strength of highly elastic materials10.1098/rspa.1967.0160 ↗
22. Threshold fracture energies for elastomers
23. Effect of materials variables on the tear behaviour of a non-crystallising elastomer10.1023/A:1004860522186 ↗
24. Threshold tear strength of elastomers
25. Molecular origins of the mechanical behavior of hybrid glasses10.1002/adfm.201000558 ↗