Suppression of the shunting-type potential induced degradation (PID-s) through ion exchange on soda lime silicate glasses
Source abstract
Abstract
This study investigates the potential of chemically strengthened soda-lime-silicate (SLS) glass to mitigate Potential Induced Degradation (PID-s) caused by the shunting mechanism in photovoltaic (PV) modules, a key factor in efficiency losses in these systems. PID-s primarily results from the migration of sodium ions (Na+) from the SLS glass into the cell junctions, leading to reduced performance. In this study, we modified commercial SLS glass through an ion exchange process, substituting Na+ ions with potassium (K+) ions, which have a larger ionic radius, to improve resistance to PID-s. The modified glass was tested in a PIDcon Bifacial Device under accelerated test conditions, and the results were compared with untreated SLS glass. The findings showed that chemically strengthened SLS glass with K+ content significantly reduced Na+ migration compared to standard SLS glass. Given that cover glasses are the primary structural elements in PV modules, we also examined the mechanical properties and demonstrated that the ion exchange process improved the strength of the SLS glass by introducing a surface compressive stress state. Our results suggest that SLS glass, commonly used in the PV module industry, is a cost-effective solution for reducing PID-s degradation, and integrating this feature into modules does not necessitate the use of more expensive glass compositions, such as aluminosilicates, which are typically used for ion exchange treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Building materials and conservation · Glass properties and applications · Photonic Crystals and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Reduced real lifetime of PV panels – economic consequences10.1016/j.solener.2023.04.063 ↗
2. Investigation of potential-induced degradation (PID) of solar modules from different manufacturers
3. Physics of potential-induced degradation in bifacial p-PERC solar cells10.1016/j.solmat.2019.109950 ↗
4. Explanation of potential-induced degradation of the shunting type by Na decoration of stacking faults in Si solar cells10.1016/j.solmat.2013.06.015 ↗
5. The influence of sodium ions decorated micro-cracks on the evolution of potential-induced degradation in p-type crystalline silicon solar cells10.1016/j.solener.2018.08.082 ↗
6. Origin of Na causing potential-induced degradation for p-type crystalline Si photovoltaic modules10.1063/1.5040516 ↗
7. Elucidating the mechanism of potential-induced degradation delay effect by ultraviolet light irradiation for p-type crystalline silicon solar cells10.1016/j.solener.2020.02.034 ↗
8. Characterization of multicrystalline silicon modules with system bias voltage applied in damp heat
9. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
10. Accelerated stress testing of potential induced degradation susceptibility of PV modules under different climatic conditions10.1016/j.solener.2021.05.020 ↗
11. Quantum efficiency loss after PID stress: wavelength dependence on cell surface and cell edge
12. Optimization of cation-barrier film on solar panel glass
13. Na-free glass for elimination of potential-induced degradation
14. Crystalline Si photovoltaic modules based on TiO₂-coated cover glass against potential-induced degradation10.1039/C4RA06791F ↗
15. PID-free c-Si PV module using novel chemically-tempered glass
16. Ion exchange for glass strengthening10.1016/j.mseb.2007.11.029 ↗
17. Chemical strengthening of glass: lessons learned and yet to be learned10.1111/j.2041-1294.2010.00010.x ↗
18. Towards improved cover glasses for photovoltaic devices10.1002/pip.3334 ↗
19. Fischer · 2024
20. Surface stress meters utilizing the optical waveguide effect of chemically tempered glasses10.1016/0143-8166(83)90004-0 ↗
21. A study on ion-exchanged, soda-lime glass's residual stress relationship with K+/Na+ concentration10.1111/ijag.14077 ↗
22. Stress in ion-exchanged soda-lime silicate and sodium aluminosilicate glasses: experimental and theoretical comparison10.1111/ijag.15787 ↗
23. Electric field-assisted ion exchange strengthening of borosilicate and soda-lime silicate glass10.1111/ijag.12266 ↗