The impact of surface polarisation on the degradation of tunnel oxide passivating contacts in silicon solar cells
Source abstract
Abstract
Tunnelling oxide passivating contact (TOPCon) silicon solar cells have risen to the mainstream in photovoltaic energy deployment worldwide. Enhancing the reliability and longevity of TOPCon solar modules will ensure the continuous growth of solar power on a multi-terawatt scale. This work investigates the mechanisms involved in surface-related degradation (SRD) in TOPCon passivating schemes, specifically focusing on two aspects. Firstly, TOPCon contacts can exhibit firing-induced instabilities that correlate with increased recombination from degradation in surface passivation. Secondly, we explored the influence of surface polarisation, induced by corona charging, on SRD by subjecting samples to various light soaking and annealing conditions. The results demonstrate that the presence of an electric field at the surface accelerates SRD, particularly under positive corona charge conditions. Effective lifetimes on symmetrical TOPCon specimens were significantly reduced and correlated to surface passivation degradation under positive polarisation. The degradation observed supports previous findings where charged hydrogen ions, which respond readily to electric fields, play a critical role in the observed degradation. This study contributes to the body of evidence aimed at understanding hydrogen kinetics at the SiO x /c-Si interface, providing valuable insights into the mechanisms driving SRD in TOPCon solar cells, with implications for enhancing the stability and performance of silicon solar panels. • Surface polarisation accelerates degradation in TOPCon solar cells. • Positive surface charge significantly reduces TOPCon lifetime performance. • Hydrogen ions migrate under electric fields, causing Surface-Related-Degradation (SRD). • SRD impacts TOPCon solar cell stability and efficiency.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Passivated rear contacts for high-efficiency n-type Si solar cells providing high interface passivation quality and excellent transport characteristics10.1016/j.solmat.2013.09.017 ↗
2. Silicon-based passivating contacts: the TOPCon route
3. 24.58% total area efficiency of screen-printed, large area industrial silicon solar cells with the tunnel oxide passivated contacts (i-TOPCon) design10.1016/j.solmat.2019.110258 ↗
4. 24.58% efficient commercial n-type silicon solar cells with hydrogenation10.1002/pip.3464 ↗
5. 2021
6. 2022
7. Working principle of carrier selective poly-Si/c-Si junctions: is tunnelling the whole story?10.1016/j.solmat.2016.05.045 ↗
8. 26.1%-efficient POLO-IBC cells: quantification of electrical and optical loss mechanisms10.1002/pip.3098 ↗
9. Effect of carrier-induced hydrogenation on the passivation of the poly-Si/SiOx/c-Si interface10.1063/1.5049289 ↗
10. Degradation and regeneration of n+-doped poly-Si surface passivation on p-type and n-type Cz-Si under illumination and dark annealing10.1109/JPHOTOV.2020.2964987 ↗
11. Long-term stability study of the passivation quality of polysilicon-based passivation layers for silicon solar cells10.1016/j.solmat.2020.110691 ↗
12. Investigating the degradation behaviours of n+-doped Poly-Si passivation layers: an outlook on long-term stability and accelerated recovery10.1016/j.solmat.2021.111491 ↗
13. Firing stability of tube furnace-annealed n-type poly-Si on oxide junctions10.1002/pip.3459 ↗
14. Optimum hydrogen injection in phosphorus-doped polysilicon passivating contacts10.1021/acsami.1c17342 ↗
15. Firing stability of phosphorus-doped polysilicon passivating contacts: factors affecting the degradation behavior10.1016/j.solmat.2021.111407 ↗
16. Hydrogen induced contact resistance in PERC solar cells10.1016/j.solmat.2018.04.036 ↗
17. Observations of contact resistance in TOPCon and PERC solar cells10.1016/j.solmat.2022.111934 ↗
18. The influence of surface electric fields on the chemical passivation of Si-SiO2 interfaces after firing10.1063/5.0089930 ↗
19. Enhancing dielectric-silicon interfaces through surface electric fields during firing10.1016/j.solmat.2024.112799 ↗
20. Silicon-based passivating contacts: the TOPCon route10.1002/pip.3522 ↗
21. Measurement of the emitter saturation current by a contactless photoconductivity decay method
22. The path to 25% silicon solar cell efficiency: history of silicon cell evolution10.1002/pip.892 ↗
23. Effect of firing process on electrical properties and efficiency of n-TOPCon solar cells10.1016/j.solener.2023.112205 ↗
24. A critical review of the process and challenges of silicon crystal growth for photovoltaic applications10.1002/crat.202300131 ↗
25. Impact of firing temperature on fire-through metal contacts to P-doped (n+) and B-doped (p+) poly-Si10.1016/j.solmat.2021.111217 ↗
26. Enlarged firing window and efficiency boosting of PERC solar cells by ‘laser enhanced contact optimization’ (LECO)10.1063/5.0089264 ↗
27. Industrial silicon solar cells applying the passivated emitter and rear cell (PERC) concept—a review10.1109/JPHOTOV.2016.2571627 ↗
28. Review of advanced hydrogen passivation for high efficient crystalline silicon solar cells10.1016/j.mssp.2018.01.019 ↗
29. The role of hydrogenation and gettering in enhancing the efficiency of next-generation Si solar cells: an industrial perspective
30. Hydrogen-induced degradation
31. Hydrogen induced degradation: a possible mechanism for light- and elevated temperature- induced degradation in n-type silicon10.1016/j.solmat.2018.05.034 ↗
32. Hydrogen-induced degradation: explaining the mechanism behind light- and elevated temperature-induced degradation in n- and p-type silicon10.1016/j.solmat.2019.110353 ↗
33. On the defect physics behind light and elevated temperature-induced degradation (LeTID) of multicrystalline silicon solar cells10.1109/JPHOTOV.2019.2937223 ↗
34. Impact of hydrogen-rich silicon nitride material properties on light-induced lifetime degradation in multicrystalline silicon10.1002/pssr.201900201 ↗
35. Instability of dielectric surface passivation quality at elevated temperature and illumination10.1016/j.egypro.2016.07.061 ↗
36. Bulk and surface instabilities in boron doped float-zone samples during light induced degradation treatments10.1016/j.egypro.2017.09.349 ↗
37. Degradation of surface passivation on crystalline silicon and its impact on light-induced degradation experiments10.1109/JPHOTOV.2017.2755072 ↗
38. Degradation of surface passivation and bulk in p-type monocrystalline silicon wafers at elevated temperature10.1109/JPHOTOV.2018.2878791 ↗
39. Impact of surface doping profile and passivation layers on surface-related degradation in silicon PERC solar cells10.1016/j.solmat.2021.111497 ↗
40. Delay of regeneration by adding aluminum in boron-doped crystalline Si
41. Interpretation of recombination at c-Si/SiNx interfaces by surface damage10.1063/1.3437643 ↗
42. Surface passivation of crystalline silicon solar cells: a review10.1002/1099-159X(200009/10)8:5<473::AID-PIP337>3.0.CO;2-D ↗
43. Dielectric surface passivation for silicon solar cells: a review
44. Hydrogen induced passivation of Si interfaces by Al2O3 films and SiO2/Al2O3 stacks10.1063/1.3497014 ↗
45. Feldmann · 2020
46. Research progress of light and elevated temperature-induced degradation in silicon solar cells: a review10.1016/j.jallcom.2022.165120 ↗
47. Temperature dependent degradation and regeneration of differently doped mc-Si materials10.1016/j.egypro.2017.09.085 ↗
48. Stability of the regeneration of the boron–oxygen complex in silicon solar cells during module integration10.1016/j.solmat.2013.01.047 ↗
49. Degradation of crystalline silicon due to boron–oxygen defects10.1109/JPHOTOV.2016.2614119 ↗
50. www.synopsys.com/silicon/tcad.html, Device Simulation Tools - Sentaurus, Synopsys Inc - Sentaurus Device TCAD, (2017).
51. Changes in hydrogen concentration and defect state density at the poly-Si/SiOx/c-Si interface due to firing10.1016/j.solmat.2021.111297 ↗
52. Modelling of hydrogen transport in silicon solar cell structures under equilibrium conditions10.1063/1.5016854 ↗
53. Field drift of the hydrogen‐related, acceptor‐neutralizing defect in diodes from hydrogenated silicon10.1063/1.96204 ↗
54. Diffusion of negatively charged hydrogen in silicon10.1103/PhysRevB.46.15554 ↗
55. Huang · 2004
56. Hydrogen in silicon: a discussion of diffusion and passivation mechanisms10.1016/0927-0248(95)00098-4 ↗
57. Development of advanced hydrogenation processes for silicon solar cells via an improved understanding of the behaviour of hydrogen in silicon10.1002/pip.3240 ↗
58. Effect of carrier-induced hydrogenation on the passivation of the poly-Si/SiOx/c-Si interface10.1063/1.5049289 ↗
59. Investigating the degradation behaviours of n-doped Poly-Si passivation layers: an outlook on long-term stability and accelerated recovery
60. Thermal processes and their impact on surface-related degradation10.1002/pssr.202100464 ↗