Supercharging cell-level potential-induced degradation (PID) testing using a salt-enriched hybrid polymer layer
Source abstract
Abstract
Potential-induced degradation of the shunting type (PID-s) is a well-known problem for photovoltaic modules. However, standard PID testing at the cell or module level takes 96 h due to the time it takes for the Na ions to diffuse from the glass to the solar cell through the ethylene-vinyl acetate (EVA) encapsulant. This is too slow to monitor production quality in the fast-paced solar cell industry. Moreover, it results in the encapsulation of solar cells, significantly restricting characterization options after PID testing. In this work, we replace the EVA in the PID testing setup with a salt-enriched hybrid polymer, which provides the solar cell with direct access to sodium (Na) ions while at the same time avoiding encapsulation during the testing process. Solar cells that underwent PID-s testing with the salt-enriched hybrid polymer showed a maximum degradation after only 12 min, over two orders of magnitude faster than standard PID-s testing using EVA, which took 4,300 min (∼72 h) to reach maximum degradation. Hence, PID-s testing using the salt-enriched hybrid is significantly faster than conventional techniques and avoids encapsulation, thus allowing for more detailed post-PID cell analysis. This new test shows that some solar cells can recover from PID-s, which was corroborated by extending the standard test to 300 h. This important novel insight shines a new light on the PID-s mechanism and the impact of this failure mode in field operation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Photovoltaic System Optimization Techniques · Silicon and Solar Cell Technologies · solar cell performance optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Photovoltaic failure and degradation modes10.1002/pip.2866 ↗
2. Potential Induced Degradation of solar cells and panels
3. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
4. Potential-induced degradation in photovoltaic modules: a critical review10.1039/C6EE02271E ↗
5. On the mechanism of potential-induced degradation in crystalline silicon solar cells10.1002/pssr.201206276 ↗
6. Consideration on Na diffusion and recovery phenomena in potential-induced degradation for crystalline Si photovoltaic modules10.7567/JJAP.55.02BF10 ↗
7. Potential‐induced degradation in high‐efficiency n‐type crystalline‐silicon photovoltaic modules: a literature review10.1002/solr.202100708 ↗
8. Evaluation of potential-induced degradation in crystalline Si solar cells using Na fault injection10.1016/j.microrel.2016.07.059 ↗
9. Chemically strengthened cover glass for preventing potential induced degradation of crystalline silicon solar cells
10. Sodium decoration of PID-s crystal defects after corona induced degradation of bare silicon solar cells10.1016/j.egypro.2015.07.055 ↗
11. Diffusion processes for integrated waveguide fabrication in glasses: a solid-state electrochemical approach10.1016/0009-2509(95)00115-L ↗
12. Photovoltaic failure and degradation modes10.1002/pip.2866 ↗
13. Influence of sodium on the potential-induced degradation for n-type crystalline silicon photovoltaic modules
14. Degradation behavior of crystalline silicon solar cells in a cell-level potential-induced degradation test10.1016/j.solener.2017.07.009 ↗
15. Toward a PID test standard: understanding and modeling of laboratory tests and field progression10.1109/JPHOTOV.2015.2487828 ↗
16. Quick test for reversible and irreversible PID of bifacial PERC solar cells10.1016/j.solmat.2020.110755 ↗
17. Large-area material and junction damage in c–Si solar cells by potential-induced degradation
18. Potential-induced degradation (PID): incomplete recovery of shunt resistance and quantum efficiency losses10.1109/JPHOTOV.2015.2459919 ↗
19. Recover possibilities of potential induced degradation caused by the micro-cracked locations in p-type crystalline silicon solar cells10.1002/pip.3383 ↗
20. Comparison of potential-induced degradation (PID) of n-type and p-type silicon solar cells10.1016/j.energy.2018.07.118 ↗
21. Fault diagnosis of PID in crystalline silicon photovoltaic modules through I-V curve10.1016/j.microrel.2021.114236 ↗
22. Comparison of potential-induced degradation (PID) of n-type and p-type silicon solar cells10.1016/j.energy.2018.07.118 ↗